High-Temperature Gas-Abrasive Wear Resistance Tests of Deposited Alloys
Source abstract
Abstract
Abstract A method and a device for testing materials for resistance to gas-abrasive wear at normal temperatures and temperatures elevated to 1000°C is developed. The test results provide a substantiated choice of surfacing materials for restoring working surfaces of parts of exhaust fans, industrial fans, top-charging gear, gas turbine units, and other equipment. The dependences of the wear of some surfacing alloys on the test temperature, gas-abrasive flow velocity, and the angle of its attack on the sample surface is determined. It is shown that under conditions of high-temperature gas-abrasive wear at small attack angles and increased speed of abrasive particles, it is advisable to use eutectic alloys with a reduced content of expensive carbide-forming elements and carbon, and at high attack angles and low-speed abrasive, heat-resistant and refractory austenitic steels. It is found that the foreign deposited C6.0Cr23Nb7Mo7W2Si2VT alloy, characterized by the highest alloying level and volume fraction of strengthening phases, has the highest resistance to gas-abrasive wear at normal temperatures among those tested. When the test temperature increases to 600°C, its wear resistance decreases by 2.5 times, yielding to the indicator of the experimental C2.8Cr14Ni6Mn6Mo3Ti2Nb2 alloy. The processes of destruction of thin surface layers of alloys are studied using the electron-ion microscopy method, which makes it possible to evaluate the influence of their structural and phase composition on the high-temperature wear mechanism. The study of the wear pattern of the C2.8Cr14Ni6Mn6Mo3Ti2Nb2 alloy showed that under the impact action of the abrasive, cracks are formed in lamellar carbides Me3C2 and Me7C3, but the high plasticity of nickel-alloyed austenite reduces the likelihood of breakdown of the resulting fragments. At the same time, small carbides (Ti,Nb,Mo)xCy and Mo2C of a compact form restrain the plastic deformation of the austenite-carbide eutectic without destruction.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Metal Alloys Wear and Properties · High-Temperature Coating Behaviors · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (15)
Show source-provided references
1. Shumilov, A.A., Shtanko, P.K., and Gordienko, V.N., Development of overlaying welding materials for increase of wear resistance of details of power blast machins of thermal powerstations, Vestnik SevNTU, 2010, no. 110, pp. 216–218.
2. Yuzvenko, Yu.A. et al., Arc cladding of blast furnace backfill parts, Avtom. Svarka, 1972, no. 2, pp. 59–63.
3. Kleis, I.R., Fundamentals of the choice of materials for operation in the gas abrasion wear, Trenie Iznos, 1980, no. 2, pp. 263–271.
4. Polyarus, E.N., Umanskyi, A.P., Stelmah, A.U., Evdokimenko, Yu.I., Kysil, V.M., and Subbotin, V.I., Influence of materials composition on their high temperature erosion gas-abrasive mechanism of wear, Vestnik Dvigatelestroeniya, 2017, no. 2, pp. 149–152.
5. Gee, M.G. and Hutchings, I.M., General Approach and Procedures for Erosive Wear Testing, Measurement Good Practice Guide, vol. 51, Teddington, United Kingdom: National Physical Laboratory, 2002.
6. Zhudra, A.P., Study of wear resistance of composite alloys under conditions of gas-abrasive wear at elevated temperatures, Avtom. Svarka, 2014, no. 11, pp. 31–34.10.15407/tpwj2014.11.05 ↗
7. Kleis, I. and Kulu, P., Solid Particle Erosion: Occurrence, Prediction and Control, London: Springer, 2008. https://doi.org/10.1007/978-1-84800-029-210.1007/978-1-84800-029-2 ↗
8. Badisch, E., Katsich, C., Winkelmann, H., Franek, F., and Roy, M., Wear behaviour of hardfaced Fe–Cr–C alloy and austenitic steel under 2-body and 3-body conditions at elevated temperature, Tribol. Int., 2010, vol. 43, no. 7, pp. 1234–1244. https://doi.org/10.1016/j.triboint.2010.01.00810.1016/j.triboint.2010.01.008 ↗
9. Higuera Hidalgo, V., Belzunce Varela, J., Carriles Menéndez, A., and Poveda Martínez, S., High temperature erosion wear of flame and plasma-sprayed nickel–chromium coatings under simulated coal-fired boiler atmospheres, Wear, 2001, vol. 247, no. 2, pp. 214–222. https://doi.org/10.1016/s0043-1648(00)00540-810.1016/s0043-1648(00)00540-8 ↗
10. Shimizu, K., Naruse, T., Xinba, Y., Kimura, K., Minami, K., and Matsumoto, H., Erosive wear properties of high V–Cr–Ni stainless spheroidal carbides cast iron at high temperature, Wear, 2009, vol. 267, nos. 1–4, pp. 104–109. https://doi.org/10.1016/j.wear.2008.12.08610.1016/j.wear.2008.12.086 ↗
11. Zhang, Ya., Shimizu, K., Kusumoto, K., Tamura, K., Hara, H., and Ito, J., Effect of Co addition on high temperature erosive wear characteristics of Fe–C–Cr–Mo–W–V multi-component white cast iron, Mater. Trans., 2017, vol. 58, no. 6, pp. 927–931. https://doi.org/10.2320/matertrans.f-m201781010.2320/matertrans.f-m2017810 ↗
12. Tkhabisimov, A.B., Kachalin, G.V., Mednikov, A.F., and Sidorov, S.V., Experimental rig for research of structural materials and protective coatings abrasive resistance, Estestv. Tekh. Nauki, 2013, no. 5, pp. 234–238.
13. Artem’ev, A.A., Antonov, A.A., Sokolov, G.N., and Lysak, V.I., Test procedure of cladded alloys for resistance against high temperature abrasive wear, J. Frict. Wear, 2017, vol. 38, no. 3, pp. 225–230. https://doi.org/10.3103/s106836661703003510.3103/s1068366617030035 ↗
14. Priyatkin, D.V., Artemyev, A.A., and Lysak, V.I., Investigation of the surfaced metal of the Fe–Cr–Ni–Mn–Mo–Ti–Nb–C system for operation under high-temperature gas-abrasive wear, Vopr. Materialoved., 2022, no. 3, pp. 17–28. https://doi.org/10.22349/1994-6716-2022-111-3-17-2810.22349/1994-6716-2022-111-3-17-28 ↗
15. Tereshchenko, A.F., Shimanovskii, V.P., and Yuzvenko, Yu.A., Investigation of jet wear of clad metal, Avtom. Svarka, 1966, no. 11, pp. 32–35.