journal article·2022-08

Tribotechnical and Corrosion Characteristics of Electrospark Fe–Al Aluminide Coatings on AISI 304 Stainless Steel

A. A. Burkov

Journal of Friction and Wear· Volume 43· Issue 4
Publisher page

Abstract

The effect of a ratio between Al and Fe in the electrode mixture exerted on the phase composition, tribotechnical properties, corrosion behavior, and oxidation resistance of electrospark Fe–Al coatings on AISI 304 stainless steel have been studied. Five mixtures of granules with an aluminum concentration ranging from 20 to 100 mol % have been prepared. The structure of the coatings has been studied by means of XRD analysis, scanning electron microscopy, and energy dispersion spectroscopy. The wear resistance of the coatings has been studied according to the ASTM G99-17 standard in the course of dry sliding friction using disk-shaped riders made of R6M5 grade high-speed steel at a velocity of 0.47 m/s under a load of 10 N. The oxidation resistance test was performed at a temperature of 900°C for 100 h. It has been found that with increasing aluminum content in the mixture of granules, the aluminum concentration in the coatings exhibits a monotonic increase, and the phase composition of the intermetallic compounds changes from FeAl to Fe14Al86. The microhardness of the coatings ranges from 5.8 to 7.1 GPa. The average friction coefficient of the coatings is in the range from 0.71 to 0.87. The wear rate of Fe–Al coatings ranges from 2.3 × 10–5 to 7.9 × 10–5 mm3/(N m). The coating with the lowest aluminum concentration exhibits the best wear resistance, whereas its wear rate is 4 times lower than that of AISI 304 grade steel. The oxidation resistance of coated stainless steel increases with increasing iron concentration in the mixture of granules. The results of testing have shown that the coatings obtained in the anode mixture with 20 at % of aluminum can provide a 13-fold increase in the oxidation resistance of AISI 304 grade stainless steel. Testing the samples by means of potentiodynamic polarization and impedance spectroscopy in 3.5% NaCl solution have shown an increase in the corrosion resistance with increasing aluminum concentration in the coatings.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Surface Treatment and Coatings · Material Properties and Applications · Intermetallics and Advanced Alloy Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (15)

Show source-provided references
1. Riffard, F. et al., The influence of implanted yttrium on the cyclic oxidation behaviour of 304 stainless steel, Appl. Surf. Sci., 2006, vol. 252, no. 10, pp. 3697–3706.10.1016/j.apsusc.2005.05.054 ↗
2. Yürektürk, Y. and Baydoğan, M., Effect of aluminizing and austempering processes on structural, mechanical and wear properties of a SSF ductile iron, Mater. Res. Express, 2018, vol. 6, no. 1, p. 016550. https://doi.org/10.1088/2053-1591/aae80410.1088/2053-1591/aae804 ↗
3. Palm, M., Stein, F., and Dehm, G., Iron aluminides, Ann. Rev. Mater. Res., 2019, vol. 49, pp. 297–326.10.1146/annurev-matsci-070218-125911 ↗
4. Deevi, S.C., Advanced intermetallic iron aluminide coatings for high temperature applications, Prog. Mater. Sci., 2021, vol. 118, p. 100769.10.1016/j.pmatsci.2020.100769 ↗
5. Canakci, A. et al., Microstructure and properties of Fe-Al intermetallic coatings on the low carbon steel synthesized by mechanical alloying, Int. J. Adv. Manuf. Technol., 2014, vol. 73, no. 5, pp. 849–858.10.1007/s00170-014-5851-2 ↗
6. Frangini, S. and Masci, A., Intermetallic FeAl based coatings deposited by the electrospark technique: Corrosion behavior in molten (Li+ K) carbonate, Surf. Coat. Technol., 2004, vol. 184, no. 1, pp. 31–39.10.1016/j.surfcoat.2003.10.050 ↗
7. Burkov, A.A. and Chigrin, P.G., Effect of tungsten, molybdenum, nickel and cobalt on the corrosion and wear performance of Fe-based metallic glass coatings, Surf. Coat. Technol., 2018, vol. 351, pp. 68–77.10.1016/j.surfcoat.2018.07.078 ↗
8. Jamnapara, N.I. et al., Microstructural studies of electrospark deposited aluminide coatings on 9Cr steels, Surf. Eng., 2012, vol. 28, no. 9, pp. 700–704.10.1179/1743294412Y.0000000043 ↗
9. Pyachin, S.A. and Burkov, A.A., Formation of intermetallic coatings by electrospark deposition of titanium and aluminum on a steel substrate, Surf. Eng. Appl. Electrochem., 2015, vol. 51, no. 2, pp. 118–124.10.3103/S1068375515020131 ↗
10. Burkov, A.A. et al., Wear resistance of Fe33Ni8Cr8W8Mo8Co8C16B11 metallic glass-based electrospark coatings, J. Frict. Wear, 2018, vol. 39, no. 5, pp. 381–387.10.3103/S1068366618050045 ↗
11. Wang, Y. et al., Effect of bionic hydrophobic structures on the corrosion performance of Fe-based amorphous metallic coatings, Surf. Coat. Technol., 2021, vol. 416, p. 127176.10.1016/j.surfcoat.2021.127176 ↗
12. Nikolenko, S.V. and Syui, N.A., Investigation of coatings produced by the electrospark machining method of steel 45 with electrodes based on carbides of tungsten and titanium, Prot. Met. Phys. Chem. Surf., 2017, vol. 53, no. 5, pp. 889–894.10.1134/S207020511705015X ↗
13. PalDey, S. and Deevi, S.C., Cathodic arc deposited FeAl coatings: Properties and oxidation characteristics, Mater. Sci. Eng. A, 2003, vol. 355, nos. 1–2, pp. 208–21510.1016/S0921-5093(03)00076-5 ↗
14. Alman, D.E. et al., Wear of iron-aluminide intermetallic-based alloys and composites by hard particles, Wear, 2001, vol. 251, nos. 1–12, pp. 875–884.10.1016/S0043-1648(01)00745-1 ↗
15. Song, B. et al., Microstructure and wear resistance of FeAl/Al2O3 intermetallic composite coating prepared by atmospheric plasma spraying, Surf. Coat. Technol., 2015, vol. 268, pp. 24–29.10.1016/j.surfcoat.2014.06.055 ↗