Abstract
Wear characteristics of silicate glass and sapphire at abrasive machining have been studied. The data obtained and the analysis of images of worn surfaces have allowed the authors to conclude that two modes of material damage run simultaneously; these are the local melting of the glass followed by its squeezing towards the contact exit and periodical fatigue fracture (growth of microcracks). Under a short-term effect of high thermal stresses the glass was found to undergo thermal cracking even outside the contact site. The crystalline material (sapphire) demonstrated anisotropy of fatigue strength under abrasive wear, when its wear rate in two perpendicular directions differed almost by an order of magnitude. The possibility of sapphire damage outside the contact site is explained by the position of the maximal surface temperature region being some distance ahead of the zone of the abrasive tool-blank contact.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Advanced Surface Polishing Techniques · Advanced machining processes and optimization · Tunneling and Rock Mechanics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (11)
Show source-provided references
1. Sulim, A.V., Proizvodstvo opticheskikh detalei (Manufacture of Optical Components), Moscow, Vysshaya Shkola, 1969.
2. Rogov, V.V., Filatov, Yu.D., Karapuzov, V.R., Ruban, F.G., and Bondarev, E.K., Temperature on a diamond disc grain during grinding, Syntet. Almazy, 1978, no. 3, pp. 49–53.
3. Malyarenko, A.D. and Filonov, I.P., Tekhnologicheskie osnovy upravlyaemogo formoobrazovaniya opticheskikh poverkhnostei (Technological Bases of Regulated Shaping of Optical Surfaces), Minsk, VUZ-YUNITI BGPA, 1999.
4. Loladze, T.N. and Bokuchava, G.V., Iznos almazov i almaznykh krugov (Wear of Diamonds and Diamond Wheels), Moscow, Mashinostroenie, 1967.
5. Couto, M.S., van Enckvort, W.J.P., and Seal, M., On the Mechanism of Diamond Polishing in the Soft Directions, J. Hard Mater., 1994, no. 5, pp. 31–47.
6. Feng, Z., Field, J.E., The Friction and Wear of Diamond Sliding on Diamond, J. Phys. D: Appl. Phys, 1992, vol. 25, no. A33–A37.10.1088/0022-3727/25/1A/007 ↗
7. Gogotsi, Y.G., Kailer, A., and Nickel, K.G., Transformation of Diamond to Graphite, Nature, 1999 no. 401, pp. 663–664.10.1038/44323 ↗
8. Van Bouwelen, F.M., Field, J.E., and Brown L.M., Electron Microscopy Analysis of Debris Produced during Diamond Polishing, Phil. Magn., 2003, no. 83, pp. 839–856.10.1080/0141861021000055673 ↗
9. Hird, J.R. and Field, J.E., A Wear Mechanism Map for the Diamond Polishing Process, Wear, 2004, no. 256, pp. 345–353.
10. Bogdanovich, P.N., Belov, V.M., and Tkachuk, D.V., An Experimental Setup for Studying Heat Processes in Solid Body Contracts, Mater., Technol., Tools, 2006, vol. 11, no. 4, pp. 89–97.
11. Bogdanovich, P.N., Belov, V.M., and Tkachuk, D.V., Determination of Temperature Field in Zone of Cutting of Diamond Crystals by Thermography, J. Fric. and Wear, 2007, vol. 28, no. 1, pp. 44–50.10.3103/S1068366607010060 ↗