Substructural Changes in the Surface Layers of Composite Gas-Thermal Cu–(Al–Si) Coatings during Friction under Various Conditions
Source abstract
Abstract
Abstract The structure, phase composition, hardness, and tribological properties of composite gas-thermal 50% Cu–50% (Al–Si) coatings under various friction conditions were studied. It has been shown that during the process of high-speed metallization, active interaction of molten aluminum and copper particles occurs, leading to the formation of solid solutions and intermetallic compounds in sprayed coatings. In particular, in 50% Cu–50% (Al–Si) coatings, in addition to the matrix phases of Cu and Al, intermetallic compounds Cu9Al4, CuAl2, and Cu3Al are recorded. The hardness and microhardness of the composite are 180 HV 1 and 180–190 HV 0.025, respectively. It has been established that a composite coating of 50% Cu–50% (Al–Si) has higher wear resistance under various friction conditions than the widely used coating of CuSn11P-C antifriction bronze, obtained by centrifugal induction surfacing. In particular, in the environment of I-20A lubricant, the wear resistance of the composite coating exceeds the wear resistance of bronze by ≈1.2 times, in the environment of Litol-24 plastic lubricant, by ≈1.4 times, and with dry friction up to ≈2.8 times. It has been shown that during boundary friction, dislocations accumulate in aluminum particles of the composite, while in copper particles at elevated test pressures, a predominant formation of a subgrain structure occurs. Based on the studies conducted, it was concluded that the increased wear resistance of the composite is due to the presence of solid intermetallic compounds in it, solid solution strengthening, the presence of silicon in aluminum interlayers, as well as dislocation strengthening of aluminum interlayers and the formation of a subgrain structure in copper interlayers.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Material Properties and Applications · Metal Alloys Wear and Properties · Powder Metallurgy Techniques and Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (15)
Show source-provided references
1. Kordikova, E.I., Tribotekhnika: konspekt lektsii (Triboengineering: Lecture Notes), Minsk: Belorusskii Gos. Tekhnol. Univ., 2013.
2. Belotserkovskii, M.A., Tekhnologii aktivirovannogo gazoplamennogo napyleniya antifriktsionnykh pokrytii (Technologies of Activated Gas Flame Spraying of Antifriction Coatings), Minsk: Tekhnoprint, 2004.
3. Kukareko, V.A., Belotserkovsky, M.A., Grigorchik, A.N., and Sosnovskiy, A.V., Structure and tribological properties of a Ti–TiN coating obtained by hypersonic metallization, J. Frict. Wear, 2022, vol. 43, no. 5, pp. 300–304. https://doi.org/10.3103/s106836662205007510.3103/s1068366622050075 ↗
4. Seliverstov, I.A., Trotsan, G.N., Smirnov, I.V., and Seliverstrova, S.R., Researches of structure and properties of plasma spray coatings on the basis of Fe–Al, Nauchn. Vestn. Khersonskoi Gos. Morskoi Akad., 2014, no. 1, pp. 249–254.
5. Filippov, M.A. and Sheshukov, O.Yu., Trenie i antifriktsionnye materialy. Uchebnoe posobie (Friction and Antifriction Materials: Training Manual), Yekaterinburg: Izd-vo Ural. Univ., 2021.
6. Astrashab, E.V., Grigorchik, A.N., Kukareko, V.A., and Belotserkovskii, M.A., Effect of heat treatment on the structure, phase composition, and wear resistance of thermal spray coatings of the pseudoalloy 08G2S + AK12, J. Frict. Wear, 2020, vol. 41, no. 1, pp. 6–11. https://doi.org/10.3103/s106836662001003110.3103/s1068366620010031 ↗
7. Umanskii, Y.S., Skakov, Yu.A., Ivanov, A.N., and Rastorguev, L.N., Kristallografiya, rentgenografiya i elektronnaya mikroskopiya (Crystallography, Radiography, and Electron Microscopy), Moscow: Metallurgiya, 1982.
8. Kononov, A.G., Kukareko, V.A., Beli, A.V., and Sharkeev, Yu.P., Ion-modified nanostructured titanium and zirconium alloys for medicine and industry, Mekh. Mash., Mekh. Mater., 2013, no. 1, pp. 47–53. https://www.elibrary.ru/qzpxov.
9. Koneva, N.A., Trishkina, L.I., Cherkasova, T.V., Solov’ev, A.N., and Cherkasov, N.V., Evolution of microstructure and its parameters after deformation of polycrystalline Cu–Al alloys with different stacking fault energy, Russ. Phys. J., 2021, vol. 64, no. 7, pp. 1219–1224. https://doi.org/10.1007/s11182-021-02447-710.1007/s11182-021-02447-7 ↗
10. Trishkina, L.I., Cherkasova, T.V., Solov’ev, A.N., and Cherkasov, N.V., Phase transitions of the dislocation structure in polycrystalline copper-based alloys, Vestn. Permsk. Nats. Issled. Politekh. Universiteta. Mashinostr., Materialoved., 2021, vol. 23, no. 3, pp. 59–65. https://doi.org/10.15593/2224-9877/2021.3.0710.15593/2224-9877/2021.3.07 ↗
11. Didenko, A.N., Sharkeev, Yu.P., Kozlov, E.V., and Ryabchikov, A.I., Effekty dal’nodeistviya v ionno-implantirovannykh metallicheskikh materialakh (Long-Range Effects in Ion-Implanted Metallic Materials), Tomsk: NTL, 2004.
12. Kim, A.V., Influence of thermomechanical treatments on microstructure and mechanical properties of austenitic steel EK-164, Bachelor’s Thesis, Tomsk, 2022.
13. Novikov, I.I., Defekty kristallicheskogo stroeniya metallov. Ucheb. posobie (Defects of Crystal Structure of Metals: Textbook), Moscow: Metallurgiya, 1983.
14. Markov, D.P. and Kelly, D., Adhesion-initiated types of catastrophic wear, Trenie Iznos, 2002, vol. 23, no. 5, pp. 483–493. https://www.elibrary.ru/mpldhv.
15. Kukareko, V.A., Submicroscopic structure of Ni–Cr precipitation-hardened alloys and their tribological behavior in adhesive wear, J. Frict. Wear, 2003, vol. 24, no. 2, pp. 70–79.