Mechanisms of structural thermal adaptability of silicate coatings
Source abstract
Abstract
The present work describes the results of experimental research of surface layers of fine silicate coatings appearing due to the minerals, such as lubricating coatings as fillers. It is shown that the structure of protective films degrades primarily due to accumulation of impurities in the boundary layer and at the inter-phase boundary with the metallic substrate, particularly carbon promoting the formation of a larger amount of crystalline structure defects. The effect of sliding velocity on the wear resistance of the silicate coating is weighed. The compatibility of friction materials and minerals is advised in order to achieve the maximum efficiency of protective coatings.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Tribology and Wear Analysis · Lubricants and Their Additives · Metal Alloys Wear and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (20)
Show source-provided references
1. Okhlopkova, A.A., Vinogradov, A.V., and Pinchuk, L.S., Plastiki, napolnennye ul’tradispersnymi neorganicheskimi soedineniyami (Plastics Filled by Ultra-Dispersed Inorganic Compounds), Gomel’: IMMS NANB, 1999.
2. Vislovich, A.N., Danilov, V.D., Dudarev, V.V., and Suloeva, L.V., Magnetic and tribotechnic properties of magnetic lubricating liquids, Trenie Iznos, 1992, vol. 13, pp. 271–279.
3. Broshcheva, P.N., Okhlopkova, A.A., and Yuchyugyaeva, T.S., Effect of natural zeolite rock on tribological characteristics of polytetrafluoroethylene, J. Frict. Wear, 2001, vol. 22, pp. 50–53.
4. Mikhailova, L.V., Vorontsov, A.S., and Liopo, V.A., Peculiarities of energetic state of components of metalpolymer systems, Vestn. Grodnensk. Gos. Univ., 2012, vol. 141, no. 4, pp. 6–19.
5. Lyubimov, D.N., Dolgopolov, K.N., Ponomarenko, A.G., Chigarenko, G.G., and Boiko, M.V., The structure of lubricating layers appearing during friction in the presence of additives of mineral friction modifiers, J. Frict. Wear, 2009, vol. 30, pp. 377–379.10.3103/S1068366609050134 ↗
6. Lyubimov, D.N., Dolgopolov, K.N., Kozakov, A.T., and Nikol’skii, A.V., Improvement of performance of lubricating materials with additives of clayey minerals, J. Frict. Wear, 2011, vol. 32, pp. 442–451.10.3103/S1068366611060092 ↗
7. Dolgopolov, K.N., Lyubimov, D.N., Kozakov, A.T., Nikol’skii, A.V., and Glazunova, E.A., Tribochemical aspects of interactions between high-dispersed serpentine particles and metal friction surface, J. Frict. Wear, 2012, vol. 33, pp. 108–114.10.3103/S1068366612020031 ↗
8. Wright, M.S., Jain, V.K., and Saba, C.S., Wear rate calculation in the four-ball wear test, Wear, 1989, no. 2, pp. 321–334.
9. Czichos, H., Tribology: a Systems Approach to the Science and Technology of Friction, Lubrication, and Wear (Tribology series), Elsevier Sci., Amsterdam, 1978.
10. Lozovoi, Yu.A., Maier, K., Kuz’mina, G.N., and Bokhinek, G., Kinetic modification of friction surfaces. Surface layers formed during boundary friction, Trenie Iznos, 1990, vol. 11, pp. 270–277.
11. Ingason, A.S., Eriksson, A.K., Lewin, E., Jensen, J., and Olafsson, S., Growth and structural properties of MgC thin films prepared by magnetron sputtering, Thin Solid Films, 2010, vol. 518, pp. 4225–4230.10.1016/j.tsf.2009.12.082 ↗
12. Kobyakov, V.A., Gritsyna, V.T., Kazarinov, Yu.G., and Volokitin, V.N., Termoluminescence of stoichiometric magnium-aluminum spinel defects, Vopr. At. Nauki Tekhn. Ser. “Fiz. Radiat. Povrezhd. Radiats. Materialoved”, 2005, no. 5, pp. 37–43.
13. Vereshchak, A.V., Gripachevskii, A.N., and Gorskii, V.V., Effect of sliding rate on structure and composition of copper contact zone in copper-steel 45 friction couple, Trenie Iznos, 1992, vol. 13, pp. 295–299.
14. Titov, V.V., Role of mechanical stresses at material alloying with the help of ionic beams, Preprint IAE, No. 3774, Moscow: Inst. At. Ener., 1983.
15. Pyatiletov, Yu.S., Effect of vacation loops on radiation “swelling” of metals, Fiz. Metal. Metallov., 1980, vol. 50, pp. 1246–1250.
16. Aseev, A.L., Bolotov, V.V., Smirnov, L.S., and Stenin, S.I., On nature and conditions of formation of rod-like defects in silicon, Fiz. Tekhn. Poluprovod., 1979, vol. 13, pp. 1302–1308.
17. Lambert, J.A. and Dobson, P.S., The structure and formation of radiation defects in ion implanted Si, Philos. Mag., 1981, no. 5, pp. 1043–1053.
18. Buckley, D.H., Surface Effects in Adhesion, Friction, Wear and Lubrication, Elsevier, 1981.
19. Markov, D.P. and Kelly, D., Adhesion-initiated types of catastrophic wear, J. Frict. Wear, 2002, vol. 23, pp. 483–493.
20. Markov, D.P. and Markova, T.F., Electrical monitoring of friction couples, J. Frict. Wear, 2001, vol. 22, pp. 92–98.