Wear-Resistant Cr–Fe–Al2O3 Coating Deposition on Steel 35 Using Aluminum Oxide Powder
Source abstract
Abstract
Abstract Using electrospark alloying, Cr–Fe–Al2O3 coatings are obtained on steel 35 in a mixture of steel granules with chromium and aluminum oxide powders. The structure of the coatings is studied using X-ray diffraction analysis, scanning electron microscopy, and X-ray spectral microanalysis. The heat resistance of the coatings was studied for 100 h at a temperature of 700°C in air. The study of the mechanical properties of the coatings includes testing for microhardness under a load of 0.5 N and wear in the dry friction mode under a load of 25 N. According to X-ray diffraction analysis, the coating composition is dominated by ferrochrome and a small amount of aluminum oxide. According to EDS analysis, the element distribution in the coating is uniform throughout the coating thickness with a chromium concentration of about 60 at %, iron, 30 at %, and aluminum, 3.4 at %. The results indicate a uniform distribution of fine particles of aluminum oxide in the volume of the deposited layer. It has been shown that the metal powder participates four times more actively in the formation of the coating compared to the granules. The heat resistance test shows that with addition of Cr–Fe–Al2O3 powder in the anode mixture, the average rate of high-temperature weight gain of the samples increases. In general, the use of Cr–Fe–Al2O3 coatings increases the heat resistance of steel 35 from 2.4 to 4 times. The average values of the friction coefficient of coatings range from 0.76 to 0.83, with a minimum for the sample deposited using a minimal addition of Al2O3. The wear of the samples decreases monotonically from 3.3 × 10–6 to 1.8 × 10–6 mm3/(N m) with a decrease in the concentration of aluminum oxide in the anode mixture. In general, the application of Cr–Fe–Al2O3 coatings using the proposed method makes it possible to increase the wear resistance of the steel 35 surface from 11 to 20 times.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Surface Treatment and Coatings · Tribology and Wear Analysis · Material Properties and Applications
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (19)
Show source-provided references
1. Sherman, D., The mechanical behavior of layered brazed metal/ceramic composites, Mater. Lett., 1998, vol. 33, nos. 5–6, pp. 255–260. https://doi.org/10.1016/s0167-577x(97)00116-x10.1016/s0167-577x(97)00116-x ↗
2. Abyzov, A.M., Aluminum oxide and alumina ceramics (review). Part 1. Properties of Al2O3 and commercial production of dispersed Al2O3, Refract. Ind. Ceram., 2019, vol. 60, no. 1, pp. 24–32. https://doi.org/10.1007/s11148-019-00304-210.1007/s11148-019-00304-2 ↗
3. Yazdi, M.S., Rezayat, M., Zandi, M.D., and Azami, A., Tribological and corrosion behavior of St37 steel by electrochemically deposited Ni–Fe/Al2O3 coating, Res. Square Preprint, 2022. https://doi.org/10.21203/rs.3.rs-1811021/v110.21203/rs.3.rs-1811021/v1 ↗
4. Sun, K.-N., Hu, X.-N., Zhang, J.-H., and Wang, J.-R., Electrodeposited Cr–Al2O3 composite coating for wear resistance, Wear, 1996, vol. 196, nos. 1–2, pp. 295–297. https://doi.org/10.1016/0043-1648(95)06860-010.1016/0043-1648(95)06860-0 ↗
5. Baghani, M., Aliofkhazraei, M., and Poursalehi, R., Microwave-assisted sintering of Fe–Al2O3 nanocomposites: Study of corrosion and wear properties, Procedia Mater. Sci., 2015, vol. 11, pp. 689–694. https://doi.org/10.1016/j.mspro.2015.11.03310.1016/j.mspro.2015.11.033 ↗
6. Gerashchenkov, D.A., Sobolev, M.Y., Markov, M.A., Gerashchenkova, E.Y., Bykova, A.D., Krasikov, A.V., and Makarov, A.M., Tribolical study of cermet coatings Al–Sn–Zn–Al2O3 for friction couples, J. Frict. Wear, 2018, vol. 39, no. 6, pp. 522–527. https://doi.org/10.3103/s106836661806003x10.3103/s106836661806003x ↗
7. Huang, J., Xie, H., Luo, L., Zan, X., Liu, D., and Wu, Yu., Preparation and properties of FeAl/Al2O3 composite tritium permeation barrier coating on surface of 316L stainless steel, Surf. Coat. Technol., 2020, vol. 383, p. 125282. https://doi.org/10.1016/j.surfcoat.2019.12528210.1016/j.surfcoat.2019.125282 ↗
8. Burkov, A.A., Improving oxidation resistance of titanium alloy VT20 by forming composite electrospark Ti3Al + Al/Al2O3 coatings, Lett. Mater., 2015, vol. 5, no. 4, pp. 371–375. https://doi.org/10.22226/2410-3535-2015-4-371-37510.22226/2410-3535-2015-4-371-375 ↗
9. Nikolenko, S.V., Pyachin, S.A., and Burkov, A.A., Formation of electrospark coatings of the VK8 hard alloy with the Al2O3 additive, Russ. J. Non-Ferrous Met., 2011, vol. 52, no. 1, pp. 56–61. https://doi.org/10.3103/s106782121101018410.3103/s1067821211010184 ↗
10. Burkov, A.A., Wear resistance of electrospark WC–Co coatings with different iron contents, J. Frict. Wear, 2016, vol. 37, no. 4, pp. 385–388. https://doi.org/10.3103/s106836661604004810.3103/s1068366616040048 ↗
11. Burkov, A.A., Krutikova, V.O., Bytsura, A.Yu., and Khe, V.K., Ti–Cr–Cu electrospark coatings on steel St3, Probl. Chern. Metall. Materialoved., 2023, no. 1, pp. 93–104. https://doi.org/10.54826/19979258_2023_1_9310.54826/19979258_2023_1_93 ↗
12. Burkov, A.A. and Kulik, M.A., Electrospark deposition of metalloceramic Fe–Al/HfC coating on steel 1035, Izv. Vyssh. Uchebn. Zaved., Chern. Metall., 2023, vol. 66, no. 3, pp. 302–310. https://doi.org/10.17073/0368-0797-2023-3-302-31010.17073/0368-0797-2023-3-302-310 ↗
13. Cao, G., Zhang, X., Tang, G., and Ma, X., Microstructure and corrosion behavior of Cr coating on M50 steel fabricated by electrospark deposition, J. Mater. Eng. Perform., 2019, vol. 28, no. 7, pp. 4086–4094. https://doi.org/10.1007/s11665-019-04148-210.1007/s11665-019-04148-2 ↗
14. De Arellano-López, A.R. and Faber, K.T., Microstructural characterization of small-particle plasma spray coatings, J. Am. Ceram. Soc., 1999, vol. 82, no. 8, pp. 2204–2208. https://doi.org/10.1111/j.1151-2916.1999.tb02063.x10.1111/j.1151-2916.1999.tb02063.x ↗
15. Saowanee, S., Rachpech, V., and Sutham, N., Effect of substrate conditions on Fe–Al2O3 composite coating, Adv. Mater. Res., 2012, vol. 488, pp. 447–451. https://doi.org/10.4028/www.scientific.net/AMR.488-489.44710.4028/www.scientific.net/AMR.488-489.447 ↗
16. Darbeïda, A., Von Stebut, J., Barthole, M., Belliard, P., Lelait, L., and Zacharie, G., Comparative tribological study of chromium coatings with different specific hardness, Surf. Coat. Technol., 1994, vols. 68–69, pp. 582–590. https://doi.org/10.1016/0257-8972(94)90221-610.1016/0257-8972(94)90221-6 ↗
17. Guangxiong, C., Zhongrong, Z., Kapsa, P., and Vincent, L., Effect of surface topography on formation of squeal under reciprocating sliding, Wear, 2002, vol. 253, nos. 3–4, pp. 411–423. https://doi.org/10.1016/s0043-1648(02)00161-810.1016/s0043-1648(02)00161-8 ↗
18. Torabinejad, V., Aliofkhazraei, M., Rouhaghdam, A.S., Allahyarzadeh, M.H., Kasama, T., and Alimadadi, H., Mechanical properties of multilayer Ni–Fe and Ni–Fe–Al2O3 nanocomposite coating, Mater. Sci. Eng., A, 2017, vol. 700, no. 3, pp. 448–456. https://doi.org/10.1016/j.msea.2017.06.00910.1016/j.msea.2017.06.009 ↗
19. Burkov, A.A., Krutikova, V.O., Bytsura, A.Yu., and Khe, V.K., Ti–Cr–Cu electrospark coatings on steel St3, Probl. Chern. Metall. Materialoved., 2023, no. 1, pp. 93–104. https://doi.org/10.54826/19979258_2023_1_9310.54826/19979258_2023_1_93 ↗