Wear Resistance of Eutectic Welding Coatings of Iron-Based Fe–Mn–C–B–Si–Ni–Cr at Increased Temperature
Source abstract
Abstract
This paper investigates the wear of iron-based Fe–Mn–C–B–Si–Ni–Cr hard-faced welding coatings. A tribological test of wear was performed at ambient and elevated (250°C) temperatures. The Anton Parr THT 1000 ball-on-disk tribometer was used for friction and wear tests. The surface after friction was evaluated using a scanning electron microscope (SEM). For the tested samples at ambient temperature the wear rate amounted to 6.23 × 10–6 mm3/(N m), whereas that of the samples tested at 250°C increased to 7.89 × 10–6 mm3/(N m). Eutectic coatings are used to increase the service life of the working bodies of machine parts and mechanisms subject to abrasive wear.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Metal Alloys Wear and Properties · Microstructure and Mechanical Properties of Steels · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (14)
Show source-provided references
1. Pashechko, M.I., Golubets, V.M., and Chernets, M.V., Formirovanie i friktsionnaya stoikost’ evtekticheskikh pokrytii (Formation and Friction Strength of Eutectic Coatings), Kyiv: Naukova Dumka, 1993.
2. Kragel’skii, I.V., Dobychin, M.N., and Kombalov, V.S., Osnovy raschetov na trenie i iznos (Fundamental Calculations of Friction and Wear), Moscow: Mashinostroenie, 1977.
3. Kostetskii, B.I., Trenie, smazka i iznos v mahsinakh (Friction, Lubrication, and Wear in Machines), Kiev: Tekhnika, 1970.
4. Garkunov, D.I., Tribotekhnika (Triboengineering), Moscow: Mashinostroenie, 1985.
5. Pashechko, M., Dziedzic, K., and Józwik, J., Analysis of wear resistance of borided steel C45, Materials, 2020, vol. 13, no. 23, p. 5529.10.3390/ma13235529 ↗
6. Lu, L., Soda, H., and McLean, A., Microstructure and mechanical properties of Fe–Cr–C eutectic composites, Mater. Sci. Eng., A, 2003, vol. 347, pp. 214–222.10.1016/S0921-5093(02)00588-9 ↗
7. Yüksel, N. and Şahin, S., Wear behavior–hardness–microstructure relation of Fe–Cr–C and Fe–Cr–C–B based hardfacing alloys, Mater. Des., 2014, vol. 58, pp. 491–498.10.1016/j.matdes.2014.02.032 ↗
8. Katsich, C., Badisch, E., Manish, R., Heath, G.R., and Franek, F., Erosive wear of hardfaced Fe–Cr–C alloys at elevated temperature, Wear, 2009, vol. 267, no. 11, pp. 1856–1864.10.1016/j.wear.2009.03.004 ↗
9. Pashechko, M., Dziedzic, K., Mendyk, E., and Jozwik, J., Chemical and phase composition of the friction surfaces Fe–Mn–C–B–Si–Ni–Cr hardfacing coatings, J. Tribol., 2018, vol. 140, art. ID 021302.10.1115/1.4037953 ↗
10. Abouei, V., Saghafian, H., and Kheirandish, S., Effect of microstructure on the oxidative wear behavior of plain carbon steel, Wear, 2007, vol. 262, pp. 1225–1231.10.1016/j.wear.2006.11.009 ↗
11. So, H., The mechanism of oxidational wear, Wear, 1995, vol. 184, pp. 161–167.10.1016/0043-1648(94)06569-1 ↗
12. Torres, H., Varga, M., Adam, K., and Rodríguez Ripoll, M., The role of load on wear mechanisms in high temperature sliding contacts, Wear, 2016, vols. 364–365, pp. 73–83.10.1016/j.wear.2016.06.025 ↗
13. Blau, P.J., Elevated-temperature tribology of metallic materials, Tribol. Int., 2010, vol. 43, pp. 1203–1208.10.1016/j.triboint.2010.01.003 ↗
14. Cihak-Bayr, U., Mozdzen, G., Badisch, E., Merstallinger, A., and Winkelmann, H., High plastically deformed sub-surface tribozones in sliding experiments, Wear, 2014, vol. 309, nos. 1–2, pp. 11–20.10.1016/j.wear.2013.10.008 ↗