journal article·2017-01

Effect of bulk heat treatment and plasma surface hardening on the microstructure and erosion wear resistance of complex-alloyed cast irons with spheroidal vanadium carbides

V. G. Efremenko, K. Shimizu, T. V. Pastukhova, Yu. G. Chabak, K. Kusumoto, A. V. Efremenko

Journal of Friction and Wear· Volume 38· Issue 1
Publisher page

Abstract

The results of an investigation of the effect of bulk quenching from temperature in the range of 760–1050°C, cryogenic treatment (–196°C) and surface plasma hardening on the abrasive-erosion wear of frugally alloyed V–Cr–Mn–Ni cast irons with spheroidal vanadium carbides have been presented in this article. It has been found that cast irons containing 5.0–7.5% V, 4.5–9.0% Cr, and 5.5–5.7% (total) of Mn and Ni after heat treatment have a 2–3-fold advantage in wear resistance compared to the prototype high-vanadium cast iron (11.9% V, 12.9% Mn). The maximum wear resistance of cast irons studied is achieved by quenching at 760°C followed by plasma surface hardening, as well as quenching at 840°C, followed by cryogenic treatment. These treatments result in the formation of an optimum microstructure that consists of spheroidal vanadium carbides, eutectic carbides M7C3, and a martensite-austenite matrix reinforced by secondary carbides. The increase in quenching temperature leads to an increase in the amount of residual austenite and decrease in the erosive wear resistance of cast irons.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Metal Alloys Wear and Properties · Advanced materials and composites · High Entropy Alloys Studies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (10)

Show source-provided references
1. Kawano, Y., Shigenori, N., Sugawara, K., and Yamamoto, S., Corrosion and wear resistance of high V–Cr–Ni cast iron with spheroidal carbides, J. Jpn. Foundry Eng. Soc., 1999, vol. 1, pp. 727–732.
2. Shigenori, N., Kitsudo, T., and Matsumoto, H., Influence of Mg-treatment condition on morphology of vanadium-carbide in stainless spheroidal carbide cast iron, J. Jpn. Foundry Eng. Soc., 2008, vol. 80, pp. 3–7.
3. Xinba, Y., Shimizu, K., Matsumoto, H., Kitsudo, T., and Momono, T., Erosive wear characteristics of spheroidal carbides cast iron, Wear, 2008, vol. 264, pp. 247–257.
4. Shigenori, N., Satoru, Y., and Teruo, T., Composition and structure of vanadium carbides in high V–Cr–Ni cast iron, J. Jpn. Foundry Eng. Soc., 2002, vol. 74, pp. 279–284.
5. Kawano, Y., Nishiuchi, S., Yamamoto, S., Sugahara, S., and Kikuchi, T., US Patent 6406563, 2002.
6. Filipovic, M., Romhanji, E., Kamberovic, Z., and Korac, M., Matrix microstructure and its micro-analysis of constituent phases in As-cast Fe–Cr–C–V alloys, Mater. Trans., 2009, vol. 50, pp. 2488–2492.10.2320/matertrans.M2009002 ↗
7. Koval, A.D., Efremenko, V.G., Brykov, M.N., Andrushchenko, M.I., Kulikovskii, R.A., and Efremenko, V.G., Principles of development of grinding media with increased wear resistance. Part 2. Optimization of steel composition to suit conditions of operation of grinding media, J. Frict. Wear, 2012, vol. 33, no. 2, pp. 153–159.10.3103/S1068366612020079 ↗
8. Efremenko, V.G., Chabak, Yu.G., and Brykov, M.N., Kinetic parameters of secondary carbide precipitation in high–Cr white iron alloyed by Mn–Ni–Mo–V complex, J. Mater. Eng. Perform., 2013, vol. 22, pp. 1378–1385.10.1007/s11665-012-0434-6 ↗
9. Efremenko, V.G., Shimizu, K., Cheiliakh, A.P., Kozarevskaya, T.V., Kusumoto, K., and Yamamoto, K., Effect of vanadium and chromium on the microstructural features of V–Cr–Mn–Ni spheroidal carbide cast irons, Int. J. Miner., Metall. Mater., 2014, vol. 21, pp. 1096–1108.10.1007/s12613-014-1014-6 ↗
10. Leshchinskii, L.K., Samotugin, S.S., Pirch, I.I., and Komar, V.I., Plazmennoe poverkhnostnoe uprochnenie (Plasma Surface Hardening), Kiev: Tekhnika, 1990.