Interface properties of ZnO nanotips grown on Si substrates
Source abstract
Abstract
ZnO nanotips have been grown on Si (100) using metalorganic chemical vapor deposition (MOCVD). The growth temperature is optimized for good crystallinity, morphology, and optical properties. ZnO nanotips exhibit a strong near band edge emission of ∼376 nm at room temperature with negligible green band emission. Pregrowth substrate treatment using diluted hydrofluoric acid (HF) and minimized oxygen exposure before the initial growth significantly reduces the interfacial SiO2 thickness, while maintaining good morphology. An n-ZnO nanotips/p-Si diode is fabricated and its I–V characteristic is measured. The threshold voltage of the diode is found to be below 2.0 V with small reverse leakage current. The ZnO/p-Si diodes provide the possibility of integrating the ZnO nanotips with Si-based electronic devices.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: ZnO doping and properties · Gas Sensing Nanomaterials and Sensors · Ga2O3 and related materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (15)
Show source-provided references
1. M.H. Huang, S. Mao, H. Feick, H.Q. Yan, Y.Y. Wu, H. Kind, E. Weber, R. Russo, and P.D. Yang, Science 292, 1897 (2001).10.1126/science.1060367 ↗
2. M. Lorenz, J. Lenzner, E.M. Kaidashev, H. Hochmuth, and M. Grundmann, Ann. Phys. Leipzig 13, 39 (2004).10.1002/andp.200310040 ↗
3. C.J. Lee, T.J. Lee, S.C. Lyu, Y. Zhang, H. Ruh, and H.J. Lee, Appl. Phys. Lett. 81, 3648 (2002).10.1063/1.1518810 ↗
4. Q. Zhao, H.Z. Zhang, Y.W. Zhu, S.Q. Feng, X.C. Sun, J. Xu, and D.P. Yu, Appl. Phys. Lett. 86, 203115 (2005).10.1063/1.1931831 ↗
5. Y. Wu, H. Yan, M. Huang, B. Messer, J. Song, and P. Yang, Chem. Eur. J. 8, 1260 (2002).10.1002/1521-3765(20020315)8:6<1260::AID-CHEM1260>3.0.CO;2-Q ↗
6. X. Wang, C.J. Summers, and Z.L. Wang, Nano Lett. 4, 423 (2004).10.1021/nl035102c ↗
7. W.I. Park, D.H. Kim, S.W. Jung, and G.C. Yi, Appl. Phys. Lett. 80, 4232 (2002).10.1063/1.1482800 ↗
8. S. Muthukumar, H. Sheng, J. Zhong, Z. Zhang, N.W. Emanaetoglu, and Y. Lu, IEEE Trans. Nanotechnol. 2, 50 (2003).10.1109/TNANO.2003.809120 ↗
9. J. Wu and S. Liu, Adv. Mater. 14, 215 (2002).10.1002/1521-4095(20020205)14:3<215::AID-ADMA215>3.0.CO;2-J ↗
10. S.C. Liou, Chi-Sheng Hsiao, and San-Yuan Chen. J. Cryst. Growth 274, 438 (2005).10.1016/j.jcrysgro.2004.10.025 ↗
11. L. Guo, Y. Ji, H. Xu, P. Simon, and Z. Wu, J. Am. Chem. Soc. 124, 14864 (2002).10.1021/ja027947g ↗
12. J. Zhong, S. Muthukumar, Y. Chen, Y. Lu, H.M. Ng, W. Jiang, and E.L. Garfunkel, Appl. Phys. Lett. 83, 16 (2003).
13. K. Vanheusden, C.H. Seager, W.L. Warren, D.R. Tallant, and J.A. Voigt, Appl. Phys. Lett. 68, 403 (1996).10.1063/1.116699 ↗
14. M. Quirk and J. Serda, Semiconductor Manufacturing Technology (Upper Saddle River, NJ: Prentice-Hall, Inc., 2001), pp. 135–137.
15. A. Guillén-Santiago, M. de la L. Olvera, A. Maldonado, R. Asomoza, and D.R. Acosta, Phys. Status Solidi. 201, 952 (2004).10.1002/pssa.200306727 ↗