journal article·2003-10

Formation of nickel disilicide using nickel implantation and rapid thermal annealing

Chel-Jong Choi, Sung-Young Chang, Young-Woo Ok, Tae-Yeon Seong, H. Gan, G. Z. Pan, K. N. Tu

Journal of Electronic Materials· Volume 32· Issue 10
Publisher page

Abstract

Transmission electron microscopy (TEM), secondary ion mass spectroscopy (SIMS), and x-ray photoemission spectroscopy (XPS) have been used to investigate the nucleation, growth, and ripening behavior of nickel-disilicide precipitates formed by Ni implantation in an amorphous-Si layer on (100) Si and followed by a two-step annealing treatment. The TEM and XPS results show that amorphous-disilicide precipitates are formed in a depth of ∼21 nm in the amorphous-Si layer when pre-annealed at 380°C for 30 sec. It is also shown that the second-step annealing at temperatures in the range of 450–600°C causes the amorphous precipitates to transform to randomly oriented crystalline ones embedded in the amorphous-Si layer. Annealing above 550°C is shown to induce the crystallization of amorphous Si by solid-phase epitaxial growth (SPEG). It is further shown that, in a prolonged annealing at high temperatures, the disilicide has dissolved and reprecipitated on the Si surface. Based on the roles of the silicide-mediated crystallization (SMC), the dissolution and reprecipitation of silicides, and SPEG, possible mechanisms are given to explain how the surface-disilicide islands are formed during annealing at temperatures of 550–950°C.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Semiconductor materials and interfaces · Silicon Nanostructures and Photoluminescence · Thin-Film Transistor Technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (14)

Show source-provided references
1. K. Maex, Mater. Sci. Eng. R11, 53 (1993).
2. E.G. Colang, J.P. Gambino, and Q.Z. Hong, Mater. Sci. Eng. R16, 43 (1996).
3. I. Kunishima, K. Suguro, T. Aoyama, and J. Matsunaga, Jpn. J. Appl. Phys. 29, 2329 (1990).10.1143/JJAP.29.L2329 ↗
4. H. Ishiwara, S. Saitoh, and K. Hikosaka, Jpn. J. Appl. Phys. 20, 843 (1981).10.1143/JJAP.20.843 ↗
5. J.P. Sullivan, R.T. Tung, and F. Schrey, J. Appl. Phys. 72, 478 (1992).10.1063/1.351878 ↗
6. W.J. Chen and L.J. Chen, J. Appl. Phys. 70, 2628 (1991).10.1063/1.349375 ↗
7. J. Vanhellemont, H. Bender, M.F. Wu, J. De Wachter, P. Hendrickx, H. Pattyn, A.M. Van Bavel, G. Langouche, M. Maenhoudt, and Y. Bruynseraede, Appl. Phys. Lett. 62, 2795 (1993).10.1063/1.109212 ↗
8. K.Y. Gao and B.X. Liu, Appl. Phys. A 68, 333 (1999).10.1007/s003390050898 ↗
9. R.C. Cammarata, C.V. Thompson, and K.N. Tu, Appl. Phys. Lett. 51, 1108 (1987).10.1063/1.99003 ↗
10. R.C. Cammarata, C.V. Thomposon, C. Hayzelden, and K.N. Tu, J. Mater. Res. 5, 2133 (1990).10.1557/JMR.1990.2133 ↗
11. C. Hayzelden and J.L. Batstone, J. Appl. Phys. 73, 8279 (1993).10.1063/1.353446 ↗
12. S. Rey, J. Hommet, G. Schmerber, and F. Le Normand, J. Cryst. Growth 216, 225 (2000).10.1016/S0022-0248(00)00365-1 ↗
13. K.N. Tu, Advances in Electronic Materials, ed. B. Wessels and G.V. Chin (Metals Park, OH: American Society for Metals, 1986), p. 147.
14. M.F. Wu, J. De Wachter, P. Hendrickx, A.M. Van Bavel, H. Pattyn, G. Langouche, J. Vanhellemont, H. Bender, M. Maenhoudt, and Y. Bruynseraede, Appl. Phys. Lett. 63, 542 (1993).10.1063/1.109999 ↗