journal article·2009-11

Fundamental Study of the Intermixing of 95Pb-5Sn High-Lead Solder Bumps and 37Pb-63Sn Pre-Solder on Chip-Carrier Substrates

C. C. Chang, Y. W. Lin, Y. S. Lai, C. R. Kao

Journal of Electronic Materials· Volume 38· Issue 11
Publisher page

Abstract

This study investigated the intermixing of 95Pb-5Sn solder bumps and 37Pb-63Sn pre-solder in flip-chip solder joints. The reaction conditions included multiple reflows (up to ten) at 240°C, whereby previously solder-coated parts are joined by heating without using additional solder. We found that the molten pre-solder had an irregular shape similar to a calyx (i.e., a cup-like structure) wrapped around a high-lead solder bump. The height to which the molten pre-solder ascended along the solid high-lead solder bump increased with the number of reflows. The molten pre-solder was able to reach the under bump metallurgy (UBM)/95Pb-5Sn interface after three to five reflows. The molten pre-solder at the UBM/95Pb-5Sn interface generated two important phenomena: (1) the molten solder dewetted (i.e., flowed away from the soldered surface) along the UBM/95Pb-5Sn interface, particularly when the number of reflows was high, and (2) the molten pre-solder transported Cu␣atoms to the UBM/95Pb-5Sn interface, which in turn caused the Ni-Sn compounds at the chip-side interface to change into (Cu0.6Ni0.4)6Sn5.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Electronic Packaging and Soldering Technologies · 3D IC and TSV technologies · VLSI and Analog Circuit Testing

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (16)

Show source-provided references
1. E.M. Davis, W.E. Harding, R.S. Schwartz, and J.J. Corning, IBM J. Res. Develop. 44, 56 (2000).10.1147/rd.441.0056 ↗
2. L.F. Miller, IBM J. Res. Develop. 13, 239 (1969).10.1147/rd.133.0239 ↗
3. P.A. Totta and R.P. Sopher, IBM J. Res. Develop. 13, 226 (1969).10.1147/rd.133.0226 ↗
4. K.N. Tu and K. Zeng, Mater. Sci. Eng. R 34, 1 (2001). doi: 10.1016/S0927-796X(01)00029-8 .10.1016/S0927-796X(01)00029-8 ↗
5. C.E. Ho, Y.L. Lin, and C.R. Kao, Chem. Mater. 14, 949 (2002). doi: 10.1021/cm010639h .10.1021/cm010639h ↗
6. W.T. Chen, C.E. Ho, and C.R. Kao, J. Mater. Res. 17, 263 (2002). doi: 10.1557/JMR.2002.0036 .10.1557/JMR.2002.0036 ↗
7. C.E. Ho, R.Y. Tsai, Y.L. Lin, and C.R. Kao, J. Electron. Mater. 31, 584 (2002). doi: 10.1007/s11664-002-0129-0 .10.1007/s11664-002-0129-0 ↗
8. C.M. Tsai, W.C. Luo, C.W. Chang, Y.C. Shieh, and C.R. Kao, J. Electron. Mater. 33, 1424 (2004). doi: 10.1007/s11664-004-0082-1 .10.1007/s11664-004-0082-1 ↗
9. C.E. Ho, S.C. Yang, and C.R. Kao, J. Mater. Sci. Mater. Electron. 18, 155 (2007). doi: 10.1007/s10854-006-9031-5 .10.1007/s10856-006-0675-8 ↗
10. A.J. Sunwoo, J.W. Morris, and G.K. Lucey, Metall. Trans. A 23, 1323 (1992). doi: 10.1007/BF02665064 .10.1007/BF02665064 ↗
11. W. Yang, L.E. Felton, and R.W. Messler, J. Electron. Mater. 24, 1465 (1995). doi: 10.1007/BF02655465 .10.1007/BF02655465 ↗
12. S. Choi, T.R. Bieler, J.P. Lucas, and K.N. Subramanian, J.␣Electron. Mater. 28, 1209 (1999). doi: 10.1007/s11664-999-0159-y .10.1007/s11664-999-0159-y ↗
13. Y.W. Wang, Y.W. Lin, C.T. Tu, and C.R. Kao, J. Alloys Compd. 478, 121 (2009). doi: 10.1016/j.jallcom.2008.11.052 .10.1016/j.jallcom.2008.11.052 ↗
14. Y.W. Wang, C.C. Chang, and C.R. Kao, J. Alloys Compd. 478, L1 (2009). doi: 10.1016/j.jallcom.2008.11.027 .10.1016/j.jallcom.2008.11.027 ↗
15. Y.W. Wang, Y.W. Lin, and C.R. Kao, Microelectron. Reliab. 49, 248 (2009). doi: 10.1016/j.microrel.2008.09.010 .10.1016/j.microrel.2008.09.010 ↗
16. M.L. Huang, T. Loeher, A. Ostmann, and H. Reichl, Appl. Phys. Lett. 86, 181908 (2005). doi: 10.1063/1.1925317 .10.1063/1.1925317 ↗