Adhesion strength of the Sn-9Zn-xAg/Cu interface

Tao-Chih Chang, Min-Hsiung Hon, Moo-Chin Wang

Journal of Electronic Materials· Volume 32· Issue 6
Publisher page

Abstract

The adhesion strength of the Sn-9Zn-xAg/Cu interface was studied. The strength increased from 3.34±0.68 MPa to 7.79±0.57 MPa and from 4.75±1.04 MPa to 10.70±0.75 MPa for the Sn-9Zn-1.5Ag/Cu and Sn-9Zn-2.5Ag/Cu interfaces, respectively, as soldered at 250°C for the soldering time from 10 sec to 30 sec. However, the strength decreased from 8.11±0.72 MPa to 5.61±0.36 MPa for the Sn-9Zn-3.5Ag/Cu interface at 250°C for 10–30 sec. Both prolonging soldering time and raising temperature are beneficial for the adhesionstrength enhancement of the Sn-9Zn-1.5Ag/Cu and Sn-9Zn-2.5Ag/Cu interfaces because of the increment of wettability, but it is detrimental to the Sn-9Zn-3.5Ag/Cu interface because of microvoid formation.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Electronic Packaging and Soldering Technologies · Advanced Welding Techniques Analysis · 3D IC and TSV technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (25)

Show source-provided references
1. R.E. Pratt, E.I. Stromswold, and D.J. Quesnel, J. Electron. Mater. 23, 375 (1994).10.1007/BF02671217 ↗
2. “IPC Adopts Lead-free Position,” Surf. Mount Technol. 13, 64 (1999).
3. D. Napp, Proc. of the 27th Inl. SAMPE Technical Conf. (Albuquerque, NM, 9–12 October 1995), pp. 334–337.
4. M. Abtew and G. Selvaduray, Mater. Sci. Eng. 27, 95 (2000).10.1016/S0927-796X(00)00010-3 ↗
5. J. Glazer, J. Electron. Mater. 23, 693 (1994).10.1007/BF02651361 ↗
6. S.K. Kang and A.K. Sarkhel, J. Electron. Mater. 23, 701 (1994).10.1007/BF02651362 ↗
7. E.P. Wood and K.L. Nimmo, J. Electron. Mater. 23, 709 (1994).10.1007/BF02651363 ↗
8. S.P. Yu, H.J. Lin, M.H. Hon, and M.C. Wang, J. Electron. Mater. 29, 237 (2000).10.1007/s11664-000-0149-6 ↗
9. K. Suganuma and Y. Nakamura, J. Jpn. Inst. Met. 59, 1299 (1995).10.2320/jinstmet1952.59.12_1299 ↗
10. K.S. Bae and S.J. Kim, J. Mater. Res. 17, 743 (2002).10.1557/JMR.2002.0108 ↗
11. M. McCormack and S. Jin, JOM 45, 36 (1993).10.1007/BF03222379 ↗
12. T.C. Chang, M.C. Wang, and M.H. Hon, J. Alloys Compounds 352, 168 (2003).10.1016/S0925-8388(02)01122-2 ↗
13. T.C. Chang, M.C. Wang, and M.H. Hon, J. Cryst. Growth 252, 391 (2003).10.1016/S0022-0248(02)02479-X ↗
14. H.T. Lee and M.H. Chen, Mater. Sci. Eng. A333, 24 (2002).
15. D.R. Frear, S.N. Burchett, H.S. Morgan, and J.H. Lau, The Mechanics of Solder Alloy Interconnects (New York: Van Nostrand Reinhold, 1994), p. 62.
16. S.P. Yu, M.C. Wang, and M.H. Hon, J. Mater. Res. 16, 76 (2001).10.1557/JMR.2001.0015 ↗
17. Y. Wu, J.A. Sees, C. Pouraghabagher, L.A. Foster, J.L. Marshall, E.G. Jacobs, and R.F. Pinizzotto, J. Electron. Mater. 22, 769 (1993).10.1007/BF02817353 ↗
18. S.C. Cheng and K.L. Lin, J. Electron. Mater. 31, 940 (2002).10.1007/s11664-002-0187-3 ↗
19. I. Shohji, T. Nakamura, F. Mori, and S. Fujiuchi, Mater. Trans. 43, 1797 (2002).10.2320/matertrans.43.1797 ↗
20. K. Suganuma, K. Niihara, T. Shoutoku, and Y. Nakamura, J. Mater. Res. 13, 2859 (1998).10.1557/JMR.1998.0391 ↗
21. T.C. Chang, M.C. Wang, and M.H. Hon, J. Cryst. Growth 252, 401 (2003).10.1016/S0022-0248(02)02480-6 ↗
22. R. Hultgren, P.D. Desai, D.T. Hawkins, M. Gleiser, and K.K. Kelley, Selected Values of the Thermodynamic Properties of Binary Alloys (Metals Park, OH: ASM, 1973), p. 795.
23. P. Shewmon, Diffusion in Solids (Warrendale, PA: TMS, 1989), p. 183.
24. R.J.K. Wassink, Soldering in Electronics, 2nd ed. (Scotland: Electrochemical Publications Limited, 1989), p. 357.
25. H.B. Aaron, J. Mater. Sci. 2, 192 (1968).