Process windows for low-temperature Au wire bonding
Source abstract
Abstract
The process windows are presented for low-temperature Au wire bonding on Au/Ni/Cu bond pads of varying Au-layer thicknesses metallized on an organic FR-4 printed circuit board (PCB). Three different plating techniques were used to deposit the Au layers: electrolytic plating, immersion plating, and immersion plating followed by electrolytic plating. Wide ranges of wire bond force, bond power, and bond-pad temperature were used to identify the combination of these processing parameters that can produce good wire bonds, allowing the construction of process windows. The criterion for successful bonds is no peel off for all 20 wires tested. The wire pull strengths and wire deformation ratios are measured to evaluate the bond quality after a successful wire bond. Elemental and surface characterization techniques were used to evaluate the bond-pad surfaces and are correlated to wire bondability and wire pull strength. Based on the process windows along with the pull strength data, the bond-pad metallization and bonding conditions can be further optimized for improved wire bondability and product yields. The wire bondability of the electrolytic bond pad increased with Au-layer thickness. The bond pad with an Au-layer thickness of 0.7 μm displayed the highest bondability for all bonding conditions used. The bondability of immersion bond pads was comparable to electrolytic bond pads with a similar Au thickness. Although a high temperature was beneficial to wire bondability with a wide process window, it did not improve the bond quality as measured by wire pull strength.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Electronic Packaging and Soldering Technologies · 3D IC and TSV technologies · Adhesion, Friction, and Surface Interactions
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (17)
Show source-provided references
1. J.K. Kim and B.P.L. Au, J. Electron. Mater. 30, 1001 (2001).10.1007/BF02657725 ↗
2. H.M. Ho, C.K. Yeo, S.L. Chan, N. Wong, C.C. Ng, C.S. Ramanujan, and K. Li, Proc. 2nd Electronic Packaging Technology Conf. (Piscataway, NJ: IEEE, 1998), pp. 190–195.
3. G.G. Harman, Wire Bonding in Microelectronics: Materials, Processes, Reliability and Yield, 2nd ed. (New York: McGraw Hill, 1997), pp. 171, 173, 267.
4. C. Dunn, R.W. Johnson, and M. Bozack, 1997 Int. Conf. on Multichip Modules (New York: IEEE, 1997), pp. 170–176.10.1109/ICMCM.1997.581168 ↗
5. D.W. Bushmire and P.H. Holloway, Proc. 1975 Int. Symp. on Microelectronics (Orlando, FL: ISHM, 1975), pp. 402–407.
6. J. Cai, S.W.R. Lee, D. Lau, and E. Leuenberger, Proc. 3rd Intl Symp. Electron. Packag. Technol. (Beijing, China: Tsinghua Univ. Press, 1998), pp. 176–181.
7. C. Lee, R. Gopalakrishnan, K. Nyunt, A. Wong, R.C.E. Tan, and J.W.L. Ong, Microelectron. Reliab. 39, 97 (1999).10.1016/S0026-2714(98)00184-X ↗
8. L. Yang, J.B. Bernstein, and K.C. Leong, IEEE Trans. Electron. Packag. Manuf. 25 (2002), pp. 91–99.10.1109/TEPM.2002.1021633 ↗
9. R.D. Rust and D.A. Doane, IEEE Trans. CHMT 14, 573 (1991).
10. H. Haji, T. Morita, K. Arita, H. Nakashima, and H. Yoshinaga, Mater. Trans. JIM 34, 960 (1993).10.2320/matertrans1989.34.960 ↗
11. L.J. Durney, Electroplating Engineering Handbook, 4th ed. (New York: Van Nostrand Reinhold, 1984), p. 421.10.1007/978-1-4757-0854-7 ↗
12. Y. Shirai, K. Otsuka, T. Araki, I. Seki, K. Kikuchi, N. Fujita, and T. Miwa, Proc. 1993 ICEMM, 366 (1993).
13. Y.M. Cheung, S.W. Or, and S. Ching, Int. Electronic Manufacturing Technology Symp. (Piscataway, NJ: IEEE, 1999), pp. 196–202.
14. J.K. Nesheim, Proc. 1984 Int. Symp. on Microelectronics (Montgomery, AL: ISHM, 1984), p. 70.
15. J.L. Jellison, Proc. Electronic Components Conf. (New York: IEEE, 1976), pp. 92–97.
16. C.M. Tan, E.E.Y. Hua, and V. Chai, IEEE Trans. CHMT 21, 585 (1998).
17. Y.H. Chan, J.K. Kim, D. Liu, P.C.K. Liu, Y.M. Cheung, and M.W. Ng, submitted to IEEE Trans. Adv. Packag. (2003).