The reactions between electroless Ni-Cu-P Deposit and 63Sn-37Pb flip chip solder bumps during reflow
Source abstract
Abstract
This study investigates the interfacial reactions between electroless Ni-Cu-P deposit and 63Sn-37Pb solder bumps under various reflow conditions. The morphology of the intermetallic compounds formed at the Ni-Cu-P/Sn-Pb interface changes with respect to reflow cycle, reflow temperature, and reflow time. The (Ni,Cu)3Sn4 compounds with three different morphologies of fine grain, whisker, and polygonal grain form at the Ni-Cu-P/Sn-Pb interface after reflow at 220°C for 15 s. The whisker-shape and polygonal grains detach from the Ni-Cu-P deposit into the Sn-Pb solder during multiple reflows. The (Ni,Cu)3Sn4 compound grows rapidly when the reflow temperature is above the Ni-Sn eutectic temperature, 231°C. A continuous (Ni,Cu)3Sn4 layer forms after reflow at 220°C for 10 min. A 4.5 µm Ni-Cu-P deposit prevents the interdiffusion of Sn and Al atoms across the Ni-Cu-P deposit after 10 reflow cycles at 220°C for 15 s and after reflow at 220°C for 10 min.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Electronic Packaging and Soldering Technologies · 3D IC and TSV technologies · Metallurgical and Alloy Processes
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (29)
Show source-provided references
1. D.S. Patterson, P. Elenius, and J.A. Leal, Adv. Electron. Pkg. 1, 337 (1997).
2. J.H. Lau, Flip Chip Technologies (New York: McGraw-Hill, 1996).
3. J.H. Lau, Chip on Board Technologies for Multichip Modules (New York: Van Nostrand Reinhold, 1994).
4. M. Pecht, Integrated Circuit, Hybrid, and Multichip Module Package Design Guidelines (New York: John Wiley & Sons, 1994).
5. J.H. Lau, Handbook of Fine Pitch Surface Mount Technology (New York: Van Nostrand Reinhold, 1994).10.1007/978-1-4684-1437-0 ↗
6. R.J. Klein Wassink, Soldering in Electronics, 2nd edition (Ayr, Scotland: Electrochemical Publications Ltd., 1989).
7. S. Bader, W. Gust, and H. Hieber, Acta Metall. Mater. 43, 329 (1995).
8. S.K. Kang, R.S. Rai, and S. Purushothaman, J. Electron. Mater. 25, 1113 (1996).10.1007/BF02659912 ↗
9. C.H. Zhong and S. Yi, Soldering & Surf. Mount Technol. 11, 44 (1999).10.1108/09540919910254930 ↗
10. R.H. Esser, A. Dimoulas, N. Strifas, A. Christou, and N. Papanicolau, Microelectron. Reliab. 38, 1307 (1998).10.1016/S0026-2714(98)00131-0 ↗
11. S.Y. Jang and K.W. Paik, Soldering & Surf. Mount Technol. 10, 29 (1998).10.1108/09540919810237093 ↗
12. C.Y. Lee and K.L. Lin, Thin Solid Films 249, 201 (1994).10.1016/0040-6090(94)90761-7 ↗
13. K.L. Lin and C.J. Chen, J. Mater. Sci.-Mater. Electron. 7, 397 (1996).
14. K.L. Lin and C.J. Chen, Int. J. Microcircuits & Electron. Pkg. 20, 46 (1997).
15. K.H. Hur, J.H. Jeong, and D.N. Lee, J. Mater. Sci. 26, 2037 (1991).10.1007/BF00549164 ↗
16. N. Krasteva, V. Fotty, and S. Armyanov, J. Electrochem. Soc. 141, 2864 (1994).10.1149/1.2059246 ↗
17. C.J. Chen and K.L. Lin, J. Electrochem. Soc. 146, 137 (1999).10.1149/1.1391576 ↗
18. C.Y. Lee and K.L. Lin, Jpn. J. Appl. Phys. 33, 4708 (1994).10.1143/JJAP.33.4708 ↗
19. C.J. Chen and K.L. Lin, Thin Solid Films, accepted for publication.
20. J.I. Han and S.J. Hong, Jpn. J. Appl. Phys. 1, 36, 2091 (1997).
21. O. Kubaschewski and C.B. Alcock, Metallurgical ThermoChemistry, 5th edition (New York: Pergamon, 1979), p. 300.
22. T.B. Massalski, Binary Alloy Phase Diagrams, Vol. 1 (Metals Park, OH: ASM, 1987), p. 942.
23. D.A. Porter and K.E. Easterling, Phase Transformations in Metals and Alloys, 2nd edition (London: Chapman & Hall, 1992).10.1007/978-1-4899-3051-4 ↗
24. J.W. Jang, P.G. Kim, K.N. Tu, D.R. Frear, and P. Thompson, J. Appl. Phys. 85, 8456 (1999).10.1063/1.370627 ↗
25. H.P.R. Frederikse, R.J. Fields, and A. Feldman, J. Appl. Phys. 72, 2879 (1992).10.1063/1.351487 ↗
26. A. Rahn, The Basics of Soldering (New York: John Wiley & Sons, 1993).
27. N. Jiang, J.A. Clum, R.R. Chromik, and E.J. Cotts, Scripta Mater. 37, 1851 (1997).10.1016/S1359-6462(97)00355-2 ↗
28. G.O. Mallory and J.B. Hajdu, Electroless Plating: Fundamentals and Applications (Orlando, FL: AESF, 1990).
29. P. Nash and A. Nash, Bulletin of Alloy Phase Diagrams 6, 350 (1985).10.1007/BF02880521 ↗