Thermoelectric Properties of Bi0.5Sb1.5Te3 Prepared by Liquid-Phase Growth Using a Sliding Boat
Source abstract
Abstract
A liquid-phase growth process using a graphite sliding boat was applied for synthesis of p-type Bi0.5Sb1.5Te3. The process lasted only 60 min, including rapid heating for melting, boat-sliding, and cooling. Thick sheets and bars of 1 mm and 2 mm in thickness having preferable crystal orientation for thermoelectric conversion were successfully prepared by the process. Control of carrier concentration was attempted through addition of excess tellurium (1 mass% to 10 mass%) to optimize the thermoelectric properties of the material. The Hall carrier concentration was found to be decreased by addition of excess tellurium. The electrical resistivity and Seebeck coefficient varied depending on the carrier concentration. As a result, the maximum observed power factor near 300 K was 4.4 × 10−3 W/K2m, with corresponding Hall carrier concentration of 4.6 × 1025 m−3. Thus, thermoelectric properties were controllable by addition of excess tellurium, and a large power factor was thus obtained through a simple and short process.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced Thermoelectric Materials and Devices · Advanced Thermodynamics and Statistical Mechanics · Advanced Semiconductor Detectors and Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (17)
Show source-provided references
1. W.M. Yim and F.D. Rosi, Solid-State Electron. 15, 1121 (1972).10.1016/0038-1101(72)90172-4 ↗
2. H. Kaibe, Y. Tanaka, M. Sakata, and I. Nishida, J. Phys. Chem. Solids 50, 945 (1989).10.1016/0022-3697(89)90045-0 ↗
3. T. Caillat, M. Carle, P. Pierrat, H. Scherrer, and S. Scherrer, J. Phys. Chem. Solids 53, 1121 (1992).10.1016/0022-3697(92)90087-T ↗
4. T. Caillat, L. Gailliard, H. Scherrer, and S. Scherrer, J. Phys. Chem. Solids 54, 575 (1993).10.1016/0022-3697(93)90235-J ↗
5. I.J. Ohsugi, T. Kojima, and I.A. Nishida, J. Appl. Phys. 68, 5692 (1990).10.1063/1.346985 ↗
6. D.B. Hyun, J.S. Hwang, T.S. Oh, J.D. Shim, and N.V. Kolomoets, J. Phys. Chem. Solids 59, 1039 (1998).10.1016/S0022-3697(97)00242-4 ↗
7. Y. Kinemuchi, T. Aoki, H. Kaga, K. Okanoue, H. Ishiguro, and K. Watari, J. Electron. Mater. 38, 1089 (2009).10.1007/s11664-008-0640-z ↗
8. T. Hayashi, Y. Horio, and H. Takizawa, Mater. Trans. 51, 1914 (2010).10.2320/matertrans.M2010065 ↗
9. T. Hayashi, M. Sekine, J. Suzuki, Y. Horio, and H. Takizawa, Mater. Trans. 48, 2724 (2007).10.2320/matertrans.MRA2007114 ↗
10. S.S. Kim, S. Yamamoto, and T. Aizawa, J. Alloys Compd. 375, 107 (2004).10.1016/j.jallcom.2003.11.141 ↗
11. J.T. Im, K.T. Hartwig, and J. Sharp, Acta Mater. 52, 49 (2004).10.1016/j.actamat.2003.08.025 ↗
12. S. Miura, Y. Sato, K. Fukuda, K. Nishimura, and K. Ikeda, Mater. Sci. Eng. A 277, 244 (2000).10.1016/S0921-5093(99)00539-0 ↗
13. J. Seo, D. Cho, K. Park, and C. Lee, Mater. Res. Bull. 35, 2157 (2000).10.1016/S0025-5408(00)00425-6 ↗
14. H. Kitagawa, T. Nagamori, T. Tatsuta, T. Kitamura, Y. Shinohara, and Y. Noda, Scripta Mater. 49, 309 (2003).10.1016/S1359-6462(03)00278-1 ↗
15. P. Pecheur and G. Toussaint, J. Phys. Chem. Solids 55, 327 (1994).10.1016/0022-3697(94)90229-1 ↗
16. Z. Starý, J. Horák, M. Stordeur, and M. Stölzer, J. Phys. Chem. Solids 49, 29 (1988).10.1016/0022-3697(88)90130-8 ↗
17. H. Kitagawa, A. Kurata, H. Araki, S. Morito, and S. Tanabe, Phys. Status Solidi A 207, 401 (2010).10.1002/pssa.200925133 ↗