journal article·2015-10Open access

A Novel Electronic Packaging Method to Replace High-Temperature Sn-Pb Solders

Yee-wen Yen, Hsien-Ming Hsiao, Pei-Sheng Shao, Yen Wei Chang

Journal of Electronic Materials· Volume 44· Issue 10

Abstract

The In/Ni/Cu/Ni/In multilayer was prepared by an electroplating method to replace high-temperature Sn-Pb solders that are conventionally used but are very harmful to the environment. This study shows all the sandwich couples that formed the (Cu,Ni)6(Sn,In)5 and Cu2In3Sn phases at the interface. When the solder joint was reflowed at 200°C, a planar layer (Ni,Cu)3(Sn,In)4 formed near the Ni layer. When the reflowing temperature was increased to 300°C, another planar layer Cu3(Sn,In) formed near the Cu substrate. The greater part of the intermetallic compounds in this case were the (Cu,Ni)6(Sn,In)5 and Cu3(Sn,In) phases. The Cu3(Sn,In) phase thickness was increased with increasing aging time. The thicker formation of Cu3(Sn,In) phase improved the solder-joint strength. The samples reflowed at 300°C exhibited the best mechanical strength, which was 57.6 kg/cm2 as reflowed. This In/Ni/Cu/Ni/In multilayer structure is a suitable candidate for high-temperature Pb-free solders.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Electronic Packaging and Soldering Technologies · 3D IC and TSV technologies · Advanced Welding Techniques Analysis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (18)

Show source-provided references
1. K. Suganuma, S.J. Kim, and K.S. Kim, JOM 61, 64 (2009).10.1007/s11837-009-0013-y ↗
2. V. Chidambaram, J. Hattel, and J. Hald, Microelectron. Eng. 88, 981 (2011).10.1016/j.mee.2010.12.072 ↗
3. M. Nahavandi, M.A. Azmah Hanim, Z.N. Ismarrubie, A. Hajalilou, R. Rohaizuan, and M.Z.S. Fadzli, J. Electron. Mater. 43, 579 (2014).10.1007/s11664-013-2873-8 ↗
4. Y. Du, C. Li, B. Huang, M. Tang, and C. Du, Solder. Surf. Mt. Technol. 27, 7 (2015).10.1108/SSMT-07-2014-0015 ↗
5. S.W. Chen, S.K. Lin and C.F Yang. J. Electron. Mater. 35, 72 (2006).10.1007/s11664-006-0186-x ↗
6. L. Yan, C. Lee, D. Yu, W.K. Choi, A. Yu, S.U. Yoon, and J.H. Lao, Proceeding 58th Electronic Components and Technology Conference, p. 1844 (2008).
7. Y.W. Yen, W.K. Liou, H.Y. Wei, and C. Lee, J. Electron. Mater. 38, 93 (2009).10.1007/s11664-008-0575-4 ↗
8. S. Bader, W. Gust, and H. Hieber, Acta Metall. Mater. 43, 329 (1995).
9. W. Hume-Rothery, J. Inst. Met. 35, 295 (1926).
10. T.B. Massalski, Binary Alloy Phase Diagrams-CD-ROM, Materials Park (OH: ASM International, 1996).
11. T.H. Chuang, C.L. Yu, S.Y. Chang, and S.S. Wang, J.␣Electron. Mater. 31, 640 (2002).10.1007/s11664-002-0136-1 ↗
12. S.K. Lin, T.Y. Chung, S.W. Chen, and C.H. Chang, J. Mater. Res. 24, 2628 (2009).10.1557/jmr.2009.0317 ↗
13. A.D. Roming, F.G. Yost, and P.F. Hiava, Proc. Microbeam Anal. 1984, ed. A.D. Romig, Jr. and J.I. Goldstein (San Francisco Press, San Francisco, 1984), p. 87.
14. J.L. Freer and J.W. Morris, J. Electron. Mater. 21, 647 (1992).10.1007/BF02655434 ↗
15. J.M. Koo and S.B. Jung, J. Electron. Mater. 34, 1565 (2005).10.1007/s11664-005-0166-6 ↗
16. S.S. Wang, Y.H. Tseng, and T.H. Chuang, J. Electron. Mater. 35, 165 (2006).10.1007/s11664-006-0199-5 ↗
17. W.T. Chen, C.E. Ho, and C.R. Kao, J. Mater. Res. 17, 263 (2002).10.1557/JMR.2002.0036 ↗
18. C.H. Ho, Y.W. Lin, S.C. Yang, C.R. Kao, and D.S. Jian, J. Electron. Mater. 35, 1017 (2006).10.1007/BF02692562 ↗