Suppressing Sn-Patch Growth in Ti/Ni(V)/Cu Under Bump Metallization with Sn-Ag-Cu Solder After Reflow and Aging

Kai-Jheng Wang, Jenq-Gong Duh

Journal of Electronic Materials· Volume 41· Issue 4
Publisher page

Abstract

Sputtered Ti/Ni(V)/Cu under bump metallization (UBM) is widely used in flip chip technology because the metals are nonmagnetic and the consumption of the Ni(V) layer is low. It is noted that V does not react with solders and intermetallic compounds (IMC) during reflow and aging; however, a Sn-patch forms in the Ni(V) layer, and the Sn-patch growth may cause the IMCs to detach from the interface of solder joints. In this study, Sn-3.0Ag-0.5Cu solder was reflowed on Ti/Ni(V)/Cu UBM with different Cu thicknesses at 250°C for 60 s, and then aged at 150°C for various periods of time. It was revealed that the Sn-patch growth could be controlled by increasing the Cu thickness in the Ti/Ni(V)/Cu UBM. A feasible approach to suppress Sn-patch formation after reflow and aging is discussed.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Electronic Packaging and Soldering Technologies · 3D IC and TSV technologies · Advanced Welding Techniques Analysis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (18)

Show source-provided references
1. P.A. Totta and R.P. Sopher, IBM J. Res. Dev. 13, 226 (1969).10.1147/rd.133.0226 ↗
2. J.H. Lau, Flip Chip Technologies (New York: McGraw-Hill, 1996), p. 123.
3. D.R. Frear, J.W. Wang, J.K. Lin, and C. Zheng, JOM 53, 38 (2001).10.1007/s11837-001-0099-3 ↗
4. C.Y. Liu, K.N. Tu, T.T. Sheng, C.H. Tung, D.R. Frear, and P. Elenius, J. Appl. Phys. 87, 750 (2000).10.1063/1.371967 ↗
5. C.H. Tung, P.S. Teo, and C. Lee, IEEE Trans. Dev. Mater. Reliab. 5, 212 (2005).10.1109/TDMR.2005.846978 ↗
6. F. Zhang, M. Li, C.C. Chum, and K.N. Tu, J. Mater. Res. 17, 2757 (2002).10.1557/JMR.2002.0397 ↗
7. A.T. Wu and F. Hua, J. Mater. Res. 22, 735 (2007).10.1557/jmr.2007.0083 ↗
8. G.Y. Jang, J.G. Duh, H. Takahashi, S.W. Lu, and J.C. Chen, J. Electron. Mater. 35, 1745 (2006).10.1007/s11664-006-0229-3 ↗
9. G.Y. Jang and J.G. Duh, J. Electron. Mater. 35, 2061 (2006).10.1007/s11664-006-0314-7 ↗
10. K.J. Wang and J.G. Duh, J. Electron. Mater. 38, 2534 (2009).10.1007/s11664-009-0933-x ↗
11. K.J. Wang, Y.Z. Tsai, J.G. Duh, and T.Y. Shih, J. Mater. Res. 24, 2638 (2009).10.1557/jmr.2009.0315 ↗
12. S.W. Chen and C.C. Chen, J. Electron. Mater. 36, 1121 (2007).10.1007/s11664-007-0200-y ↗
13. K.J. Wang, J.G. Duh, B. Sykes, and D. Schade, J. Electron. Mater. 39, 2558 (2010).10.1007/s11664-010-1370-6 ↗
14. K.N. Tu and K. Zeng, Mater. Sci. Eng. R Rep. 34, 1 (2001).10.1016/S0927-796X(01)00029-8 ↗
15. K. Zeng, V. Vuorinen, and J.K. Kivilahti, IEEE Trans. Electron. Packag. Manuf. 25, 162 (2002).10.1109/TEPM.2002.801648 ↗
16. C.E. Ho, S.C. Yang, and C.R. Kao, J. Mater. Sci. Mater. Electron. 18, 155 (2007).10.1007/s10854-006-9031-5 ↗
17. J.W. Yoon, B.I. Noh, B.K. Kim, C.C. Shur, and S.B. Jung, J. Alloys Compd. 486, 142 (2009).10.1016/j.jallcom.2009.06.159 ↗
18. C.Y. Li and J.G. Duh, J. Mater. Res. 20, 3118 (2005).10.1557/JMR.2005.0391 ↗