Preparation and Characterization of Ultralow-Dielectric-Constant Porous SiCOH Thin Films Using 1,2-Bis(triethoxysilyl)ethane, Triethoxymethylsilane, and a Copolymer Template
Source abstract
Abstract
Ultralow-dielectric-constant (k) porous SiCOH films have been prepared using 1,2-bis(triethoxysilyl)ethane, triethoxymethylsilane, and a poly(ethylene oxide)–poly(propylene oxide)–poly(ethylene oxide) triblock copolymer template by means of spin-coating. The resulting films were characterized by cross-section scanning electron microscopy, small-angle x-ray diffraction, atomic force microscopy, Fourier-transform infrared spectroscopy, nanomechanical testing, and electrical measurements. Thermal treatment at 350°C for 2 h resulted in the formation of ultralow-k films with k of ∼2.0, leakage current density of 3 × 10−8 A/cm2 at 1 MV/cm, reduced modulus (E r) of ∼4.05 GPa, and hardness (H) of ∼0.32 GPa. After annealing between 400°C and 500°C for 30 min, the resulting films showed fluctuant k values of 1.85 to 2.22 and leakage current densities of 3.7 × 10−7 A/cm2 to 3 × 10−8 A/cm2 at 0.8 MV/cm, likely due to the change of the film microstructure. Compared with 350°C annealing, higher-temperature annealing can improve the mechanical strength of the ultralow-k film, i.e., E r ≈ 5 GPa and H ≈ 0.56 GPa after 500°C annealing.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Mesoporous Materials and Catalysis · Copper Interconnects and Reliability · Silicone and Siloxane Chemistry
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (25)
Show source-provided references
1. M. Tata, Y. Harada, and T. Tamura, IEDM Tech. Dig. 845 (2003).
2. D.D. Burkey and K.K. Gleason, J. Appl. Phys. 93, 5147 (2003).10.1063/1.1562744 ↗
3. S. Yang, P.A. Mirau, C.S. Pai, and O. Nalamasu, Chem. Mater. 14, 372 (2002).
4. N. Tajima, T. Ohno, T. Hamada, K. Yoneda, N. Kobayashi, S. Hasaka, and M. Inoue, Appl. Phys. Lett. 89, 061907 (2006).10.1063/1.2336273 ↗
5. A. Grill and V. Patel, Appl. Phys. Lett. 79, 803 (2001).10.1063/1.1392976 ↗
6. A. Grill, J. Appl. Phys. 93, 1785 (2003).10.1063/1.1534628 ↗
7. J. Lubguban, T. Rajagopalan, N. Mehta, B. Lahlouh, S.L. Simon, and S. Gagopadhyay, J. Appl. Phys. 92, 1033 (2002).10.1063/1.1483916 ↗
8. L.L. Chapelon, V. Arnal, and M. Broekaart, Microelectron. Eng. 76, 1 (2004).10.1016/j.mee.2004.07.012 ↗
9. V. Jousseaume, L. Favennec, A. Zenasni, and O. Gourhant, Surf. Coat. Technol. 201, 9249 (2007).10.1016/j.surfcoat.2007.04.105 ↗
10. A. Majumdar, G. Das, and N. Patel, J. Electrochem. Soc. 155, D22 (2008).10.1149/1.2801345 ↗
11. K. Maex, M.R. Baklanov, and D. Shamiryan, J. Appl. Phys. 93, 8800 (2003).10.1063/1.1567460 ↗
12. B.D. Hatton, K. Landsdron, and W.J. Hunks, Mater. Today 9, 24 (2006).10.1016/S1369-7021(06)71387-6 ↗
13. T.B. Casserly and K.K. Gleason, Plasma Process. Polym. 2, 680 (2005).
14. B.J. Cham, B. Kim, and B. Jung, J. Non Cryst. Solids 352, 5681 (2006).
15. B. Toury and F. Babonneau, J. Eur. Ceram. Soc. 25, 265 (2005).10.1016/j.jeurceramsoc.2004.08.013 ↗
16. F. Hoffmann, M. Cornelius, J. Morell, and M. Fröba, Angew. Chem. Int. Ed. 45, 3216 (2006).10.1002/anie.200503075 ↗
17. W.Y. Leong, C.F. Tsang, and H.Y. Li, Thin Solid Films 496, 403 (2006).10.1016/j.tsf.2005.08.283 ↗
18. H.W. Su and W.C. Chen, Mater. Chem. Phys. 114, 738 (2009).
19. B. Bharatiya, C. Guo, and J.H. Ma, Eur. Polym. J. 43, 1886 (2007).10.1016/j.eurpolymj.2007.02.010 ↗
20. T.K.S. Wong, B. Liu, and B. Narayanan, Thin Solid Films 462–463, 158 (2004).
21. Y. Shioya, T. Ohdaira, and R. Suzuki, J. Non Cryst. Solids 354, 2978 (2008).10.1016/j.jnoncrysol.2007.12.011 ↗
22. C.S. Yang, Y.H. Yu, and K.M. Lee, Thin Solid Films 506–507, 52 (2006).
23. J.C. Phillips, J. Non Cryst. Solids 34, 153 (1979).10.1016/0022-3093(79)90033-4 ↗
24. M.F. Thorpe, J. Non Cryst. Solids 57, 355 (1983).10.1016/0022-3093(83)90424-6 ↗
25. A.R. Balkenende, F.K. de Theije, and J.C.K. Kriege, Adv. Mater. 15, 139 (2003).10.1002/adma.200390028 ↗