Electrical Characteristics of the Three-Dimensional Interconnection Structure for the Chip Stack Package with Cu through Vias
Source abstract
Abstract
A chip stack specimen of a three-dimensional (3-D) interconnection structure with Cu vias of 75-μm diameter, 90-μm height, and 150-μm pitch was successfully fabricated using via hole formation with deep reactive ion etching (RIE), Cu via filling with pulse-reverse pulse electroplating, Si thinning, Cu/Sn bump formation, and flip-chip bonding. The contact resistance of a Cu/Sn bump joint and Cu via resistance could be determined from the slope of the daisy chain resistance versus the number of bump joints of the flip-chip specimen containing Cu vias. When the flip chip was bonded at 270°C for 2 min, the contact resistance of a Cu/Sn bump joint of 100-μm diameter was 6.74 mΩ, and the resistance of a Cu via of 75-μm diameter and 90-μm height was 2.31 mΩ. As the power transmission characteristics of the Cu through via, the S21 parameter was measured up to 20 GHz.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Electronic Packaging and Soldering Technologies · 3D IC and TSV technologies · Electromagnetic Compatibility and Noise Suppression
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (16)
Show source-provided references
1. Al-Sarawi S.F., Abbott D., Franzon P.D. (1988) IEEE Trans. CPMT 21B:2
2. Sheng S., Chandrakasan A., Brodersen R.W. (1992) IEEE Commun. Mag. 30:6410.1109/35.210358 ↗
3. R.E. Terrill, Proc. 1995 Int. Conf. Multichip Modules (1995), pp. 7–11
4. R. Crowley, Technical Report (Austin, TX: Techsearch Int. Inc., 1993), pp. 159–161
5. O. Ehrmann, K. Buschick, G. Chmiel, and A. Pareds (Paper presented at Proc. 1995 Int. Conf. Multichip Modules, Denver, CO, 1995)
6. Kanbach H., Wilde J., Kriebel F., and Meusel E., Int. Conf. on High Density Packaging and MCMs (1999), pp. 248–53
7. M. Karnezos, F. Carson, and R. Pendse, Chip Scale Rev. (2005)
8. Takahashi K., Terao H., Tomita Y., Yamaji Y., Hoshino M., Sato T., Morifuji T., Sunohara M., Bonkohara M. (2001) Jpn. J. Appl. Phys. 40:303210.1143/JJAP.40.3032 ↗
9. T. Matsumoto, Extracts and Abstracts, 1995 Int. Conf. Solid State Devices Materials (1995), pp. 1073–1073
10. Ramm P. (1997) Microelectron. Eng. 37:3910.1016/S0167-9317(97)00092-0 ↗
11. Seah C.H., Mridha S., Chan L.H. (2001) J. Mater. Process Technol. 114:23310.1016/S0924-0136(01)00614-8 ↗
12. Tanida K., Umemoto M., Kojima K., Takahashi K. (2005) Electron. Jisso Gakkai Shi 40:308
13. P.V. Zant, Microchip Fabrication, 3rd ed. (New York: McGraw-Hill, 1997), p. 39
14. Lee K.Y., Lee Y.H., Kim Y.H., Oh T.S. (2005) J. Kor. Inst. Met. Mater. 43:248
15. D.K. Schroder, Semiconductor Material and Device Characterization, 2nd ed. (New York: John Wiley & Sons, Inc., 1998), p. 10
16. J. Cutnell and K. Johnson, Physics, 4th ed. (New York: Wiley, 1998), p. 755