Intermetallic reactions in a Sn-20In-2.8Ag solder ball-grid-array package with Au/Ni/Cu pads
Source abstract
Abstract
The intermetallic compounds formed during the reflow and aging of Sn-20In-2.8Ag ball-grid-array (BGA) packages are investigated. After reflow, a large number of cubic-shaped AuIn2 intermetallics accompanied by Ag2In precipitates appear in the solder matrix, while a Ni(Sn0.72Ni0.28)2 intermetallic layer is formed at the solder/pad interface. With further aging at 100°C, many voids can be observed in the solder matrix and at the solder/pad interface. The continuous distribution of voids at the interface of specimens after prolonged aging at 100°C causes their bonding strength to decrease from 5.03 N (as reflowed) to about 3.50 N. Aging at 150°C induces many column-shaped (Cu0.74Ni0.26)6(Sn0.92In0.08)5 intermetallic compounds to grow rapidly and expand from the solder/pad interface into the solder matrix. The high microhardness of these intermetallic columns causes the bonding strength of the Sn-20In-2.8Ag BGA solder joints to increase to 5.68 N after aging at 150°C for 500 h.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Electronic Packaging and Soldering Technologies · 3D IC and TSV technologies · Advanced Welding Techniques Analysis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (18)
Show source-provided references
1. J. Glazer, Int. Mater. Rev. 40, 65 (1995).10.1179/imr.1995.40.2.65 ↗
2. W.K. Choi and H.M. Lee, J. Electron. Mater. 29, 1207 (2000).10.1007/s11664-000-0014-7 ↗
3. S. Kang and A. Sarkhel, J. Electron. Mater. 23, 701 (1994).10.1007/BF02651362 ↗
4. O. Hiroshi, M. Masamitsu, and I. Kiyohito, J. Jpn. Inst. Met. 63, 685 (1999).10.2320/jinstmet1952.63.6_685 ↗
5. U.R. Kattner and W.J. Boettinger, J. Electron. Mater. 23, 603 (1994).10.1007/BF02653345 ↗
6. Y. Kariya and M. Otsuka, J. Electron. Mater. 27, 1229 (1998).10.1007/s11664-998-0074-7 ↗
7. J. Glazer, Int. Mater. Rev. 40, 65 (1995).10.1179/095066095790151115 ↗
8. N.C. Lee, Soldering Surf. Mount Technol. 26, 25 (1997).
9. D.M. Jacobson and G. Humpston, Gold Bull. 22, 9 (1989).10.1007/BF03214704 ↗
10. P.G. Kim and K.N. Tu, Mater. Chem. Phys. 53, 165 (1998).10.1016/S0254-0584(97)02076-2 ↗
11. K.W. Huang and T.H. Chuang, J. Mater. Eng. Performance, in press (2005).
12. T.H. Chuang, K.W. Huang, and W.H. Lin, J. Electron. Mater. 33, 374 (2004).10.1007/s11664-004-0146-2 ↗
13. M.J. Chiang and T.H. Chuang, Z. Metallkd. 93, 1194 (2002).10.3139/146.021194 ↗
14. T.H. Chuang, S.Y. Chang, L.C. Tsao, W.P. Weng, and H.M. Wu, J. Electron. Mater. 32, 195 (2003).10.1007/s11664-003-0193-0 ↗
15. Y. H. Tseng (Ph.D. Thesis, National Taiwan University, 2000).
16. T.H. Chuang, K.H. Huang, and W.H. Lin, J. Electron. Mater. 33, 4 (2004).
17. C.Y. Huang and S.W. Chen, J. Electron. Mater. 31, 2 (2002).10.1007/s11664-002-0165-9 ↗
18. T.L. Yu (Ph. D. Thesis, National Taiwan University, 2003).