Thermoelectric Properties of In Situ Formed Bi0.85Sb0.15/Bi-Rich Particles Composite
Source abstract
Abstract
A Bi-15 at.%Sb alloy, homogenized by equal channel angular extrusion (ECAE) at T = 523 K, has been treated just above its solidus temperature, causing segregation of a secondary Bi-rich phase at the grain boundaries. This process results in an in situ composite. The thermoelectric properties of the composite have been measured in the range of 5 K < T < 300 K. The results are compared with those of the homogeneous alloy. The presence of a Bi-rich phase improves the Seebeck coefficient at T < 50 K, and enhances the electrical conductivity by a factor of 1.4 at T = 300 K up to a factor of 3.4 at T = 50 K; unfortunately, the thermal conductivity also increases by about 50% in the same temperature range. As a result, the figure of merit, Z, is slightly suppressed above T = 110 K, but increases at lower temperatures, reaching a peak value of 4.2 x 10(-3) K(-1) at T = 90 K. The power factor considerably increases over the whole temperature range, rendering this material suitable as the n-type leg of a cryogenic thermoelectric generator for cold energy recovery in a liquefied natural gas plant.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced Thermoelectric Materials and Devices · Advanced Thermodynamics and Statistical Mechanics · Physics of Superconductivity and Magnetism
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (8)
Show source-provided references
1. G.E. Smith and R.J. Wolfe, J. Appl. Phys. 33, 831 (1962).
2. W.M. Yim and A. Amith, Solid-State Electron. 15, 1141 (1972).10.1016/0038-1101(72)90173-6 ↗
3. S. Ceresara, G. Giunchi, P. Bassani, T. Cavallin, and C. Fanciulli, Proc 5th European Thermoelectric Conference, Odessa (2007), p. 72.
4. H. Okamoto, Binary Alloy Phase Diagrams, ed B. Massalski, Vol. 1 (1991), p. 787.
5. F. Weinberg and E. Teghtsoonian, Acta Met. 8, 455 (1957).10.1016/0001-6160(57)90064-0 ↗
6. B. Lenoir, A. Dausher, M. Cassart, Yu.I. Ravich, and H. Sherrer, J. Phys. Chem. Solids 59, 129 (1998).10.1016/S0022-3697(97)00187-X ↗
7. B. Lenoir, M. Cassart, J.P. Michenaud, H. Sherrer, and S. Sherrer, J. Phys. Chem. Solids 57, 89 (1996).10.1016/0022-3697(95)00148-4 ↗
8. V.D. Kagan and N.A. Red’ko, Proc 14th International Conference on Thermoelectrics, St Petersburg (1995), p. 78.