Fluxless Bonding of Large Silicon Chips to Ceramic Packages Using Electroplated Eutectic Au/Sn/Au Structures
Source abstract
Abstract
A fluxless process of bonding large silicon chips to ceramic packages has been developed using a Au-Sn eutectic solder. The solder was initially electroplated in the form of a Au/Sn/Au multilayer structure on a ceramic package and reflowed at 430°C for 10 min to achieve a uniform eutectic 80Au-20Sn composition. A 9 mm × 9 mm silicon chip deposited with Cr/Au dual layers was then bonded to the ceramic package at 320°C for 3 min. The reflow and bonding processes were performed in a 50-mTorr vacuum to suppress oxidation. Therefore, no flux was used. Even without any flux, high-quality joints were produced. Microstructure and composition of the joints were studied using scanning electron microscopy with energy-dispersive x-ray spectro- scopy. Scanning acoustic microscopy was used to verify the joint quality over the entire bonding area. To employ the x-ray diffraction method, samples were made by reflowing the Au/Sn/Au structure plated on a package. This was followed by a bonding process, without a Si chip, so that x-rays could scan the solder surface. Joints exhibited a typical eutectic structure and consisted of (Au,Ni)Sn and (Au,Ni)5Sn phases. This novel fluxless bonding method can be applied to packaging of a variety of devices on ceramic packages. Its fluxless nature is particularly valuable for packaging devices that cannot be exposed to flux such as sensors, optical devices, medical devices, and laser diodes.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Electronic Packaging and Soldering Technologies · 3D IC and TSV technologies · Advanced Welding Techniques Analysis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (17)
Show source-provided references
1. E. Jung, MRS Bull. 28, 51 (2003).10.1557/mrs2003.17 ↗
2. R. Therrien, S. Singhal, A. Chaudhari, W. Nagy, J. Marquart, J.W. Johnson, A.W. Hanson, J. Riddle, P. Rajagopal, B. Preskenis, O. Zhitova, J. Willamson, I.C. Kizilyalli, and K.J. Linthicum, IEEE MTT-S International Microwave Symposium Digest (2006), p. 710.10.1109/MWSYM.2006.249732 ↗
3. S.B. Park1, R. Joshi, and B. Sammakia, IEEE Twenty-First Annual Semiconductor Thermal Measurement Management Symposium (2005), p. 214.
4. J.Z. Shi, X.M. Xie, F. Stubhan, and J. Freytag, Trans. ASME 122, 168 (2000).
5. S.K. Kang, R.S. Rai, and S. Purushothaman, IEEE Trans. Compon. Packag. Manuf. Technol. A 21, 18 (1998).10.1109/95.679027 ↗
6. K. Mizuishi, M. Tokuda, and Y. Fujita, IEEE Electronic Components Conference (1988), p. 330.
7. S. Bonafede, A. Huffman, and W.D. Palmer, IEEE Trans. Compon. Packag. Technol. 30, 604 (2006).10.1109/TCAPT.2006.880506 ↗
8. R. Venkatramna, J.R. Wilcox, and S.R. Cain, Metall. Mater. Trans. A 28A, 699 (1997).10.1007/s11661-997-0056-z ↗
9. D. Kim, J. Kim, G.L. Wang, and C.C. Lee, Mater. Sci. Eng. A 393, 315 (2005).10.1016/j.msea.2004.11.022 ↗
10. C.C. Lee, C.Y. Wang, and G. Matijasevic, IEEE Trans. Compon. Hybr. Manuf. Technol. 14, 407 (1991).10.1109/33.87322 ↗
11. G.S. Matijasevic, C.C. Lee, and C.Y. Wang, Thin Solid Films 223, 276 (1993).10.1016/0040-6090(93)90533-U ↗
12. C.C. Lee and J. Kim, Proceedings of the 10th IEEE International Symposium on Advanced Packaging Materials (Irvine, CA, March 16–18, 2005).
13. C.C. Lee, D.T. Wang, and W.S. Choi, Rev. Sci. Instrum. 77, 125104 (2006).10.1063/1.2402910 ↗
14. S. Anhöck, H. Oppermann, C. Kallmayer, R. Aschenbrenner, L. Thomas, and H. Reichl, Proceedings of IEEE/CPMT Berlin International Manufacturing Technology Symposium (1998), pp. 156–165.
15. J.Y. Tsai, C.W. Chang, Y.C. Shieh, Y.C. Hu, and C.R. Kao, J. Electron. Mater. 34, 182 (2005).10.1007/s11664-005-0231-1 ↗
16. J.Y. Tsai, C.W. Chang, C.E. Ho, Y.L. Lin, and C.R. Kao, J. Electron. Mater. 35, 65 (2006).10.1007/s11664-006-0185-y ↗
17. H. Okamoto and T.B. Massalski, eds., Phase Diagram of Binary Gold Alloys (Metals Park, OH: ASM International, 1987), pp. 278–289.