journal article·2009-09

Study of Solidification Cracks in Sn-Ag-Cu Lead-Free Solder Joints

Wenxing Dong, Yaowu Shi, Yongping Lei, Zhidong Xia, Fu Guo

Journal of Electronic Materials· Volume 38· Issue 9
Publisher page

Abstract

In the present work, solidification cracks in Sn-Ag-Cu solder joints were investigated. Experimental results indicate that solidification cracks existed in significant numbers in the miniature Sn-Ag-Cu solder joints. In order to create solidification cracks in the miniature solder joints during solidification and evaluate the susceptibility of Sn-Ag-Cu alloys to solidification cracking, a copper self-restraint specimen was designed, which can simulate the process of solidification crack formation. The solidification crack susceptibility of the Sn-Ag-Cu solder alloy was evaluated using the total crack length of the solder joint. In addition, the effect of trace amounts of elemental additions on solidification cracking of Sn-Ag-Cu solder joints was studied. It was found that adding trace amounts of Ni or Ce could depress the solidification cracks in Sn-3.0Ag-0.5Cu solder joints. However, P additions aggravated the formation of solidification cracks.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Electronic Packaging and Soldering Technologies · Aluminum Alloy Microstructure Properties · Metallurgy and Material Forming

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (15)

Show source-provided references
1. Bo Li, Yaowu Shi, Yongping Lei, Fu Guo, Zhidong Xia, and Bin Zong. J.Electron. Mater., 34(2005)217. doi: 10.1007/s11664-005-0207-1 .10.1007/s11664-005-0207-1 ↗
2. Wenxing Dong, Yaowu Shi, Yongping Lei, Zhidong Xia, Fu Guo. J.Electron. Mater. 37, 982(2008). doi: 10.1007/s11664-008-0458-8 .10.1007/s11664-008-0458-8 ↗
3. M.A. Matin, W.P. Vellinga, M.G.D. Geers. Mater. Sci. Eng. A.73, 445(2007).
4. D.-S. Jiang, Y.-P. Wang, and C.S. Hsiao, Electronics Packaging Technology Conference (2006), p. 385.
5. C.M.L, Wu Y and W Wong, J Mater Sci. Mater Electron. 18, 77(2007). doi: 10.1007/s10854-006-9022-6 .
6. Zhong Chen, Aditya Kumar, and M. Mona. J.Electron. Mater. 35, 2126(2006). doi: 10.1007/s11664-006-0322-7 .10.1007/s11664-006-0322-7 ↗
7. Feng Gao, Tadashi Takemoto And Hiroshi Nishikawa. J.Electron. Mater. 35,2081(2006). doi: 10.1007/s11664-006-0317-4 .10.1007/s11664-006-0317-4 ↗
8. Hui Zou. J.Civil aviation Univ. China, 25, 49(2007).
9. Peter Biocca. Global SMT & Packag. 11/12, 23(2006).
10. N. Blattau and C. Hillman, IPC/APEX, Anaheim, CA, Vol. 2 (2006), p. 7.
11. S. Lin, C. Aliravci, and M.O. Pekguleryuz. Metall. Mater. Trans. A. 38,1056(2007), doi: 10.1007/s11661-007-9132-7 .10.1007/s11661-007-9132-7 ↗
12. V. M. Goritskii. Met. Sci. Heat Treat. 43,120(2001). doi: 10.1023/A:1010597317523 .10.1023/A:1010597317523 ↗
13. A.V. Nikolaeva, Yu.A. Nikolaev and Yu.R. Kevorkyan. Atomic Energy. 91, 534 (2001). doi: 10.1023/A:1012482419952 .10.1023/A:1012482419952 ↗
14. W.R. SUN, S.R. GUO, D.Z. LU, and Z.Q. HU. Metall. Mater. Trans. A, 28,649(1997). doi: 10.1007/s11661-997-0050-5 .10.1007/s11661-997-0050-5 ↗
15. ASM/NIST Date program for alloy phase diagrams, second edition plus updates.