Intermetallic reactions in reflowed and aged Sn-9Zn solder ball grid array packages with Au/Ni/Cu and Ag/Cu pads
Source abstract
Abstract
During the reflowing of Sn-9Zn solder ball grid array (BGA) packages with Au/Ni/Cu and Ag/Cu pads, the surface-finished Au and Ag film dissolved rapidly and reacted with the Sn-9Zn solder to form a γ3-AuZn4/γ-Au7Zn18 intermetallic double layer and e-AgZn6 intermetallic scallops, respectively. The growth of γ3-AuZn4 is prompted by further aging at 100°C through the reaction of γ-Au7Zn18 with the Zn atoms dissolved from the Zn-rich precipitates embedded in the β-Sn matrix of Sn-9Zn solder BGA with Au/Ni/Cu pads. No intermetallic compounds can be observed at the solder/pad interface of the Sn-9Zn BGA specimens aged at 100°C. However, after aging at 150°C, a Ni4Zn21 intermetallic layer is formed at the interface between Sn-9Zn solder and Ni/Cu pads. Aging the immersion Ag packages at 100°C and 150°C caused a γ-Cu5Zn8 intermetallic layer to appear between e-AgZn6 intermetallics and the Cu pad. The scallop-shaped e-AgZn6 intermetallics were found to detach from the γ-Cu5Zn8 layer and float into the solder ball. Accompanied with the intermetallic reactions during the aging process of reflowed Sn-9Zn solder BGA packages with Au/Ni/Cu and Ag/Cu pads, their ball shear strengths degrade from 8.6 N and 4.8 N to about 7.2 N and 2.9 N, respectively.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Electronic Packaging and Soldering Technologies · Advanced Welding Techniques Analysis · Intermetallics and Advanced Alloy Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (17)
Show source-provided references
1. N.C. Lee, Adv. Microelectron. 26, 29 (1999).
2. H.J. Lau, C.P. Wong, N.C. Lee, and S.W. Ricky Lee, Electronics Manufacturing with Lead-Free, Halogen-Free & Conductive-Adhesive Materials (New York: McGraw-Hill Handbooks, 2003).
3. Z. Chen, M. He, and G. Qi, J. Electron. Mater. 33, 1465 (2004).10.1007/s11664-004-0088-8 ↗
4. J.W. Yoon, S.W. Kim, and S.B. Jung, J. Alloys Compounds 391, 82 (2005).10.1016/j.jallcom.2004.09.001 ↗
5. M.Y. Chiu, S.Y. Chang, Y.H. Tseng, Y.C. Chan, and T.H. Chuang, Z. Metallkd. 93, 248 (2002).10.3139/146.020248 ↗
6. Y.C. Chan, M.Y. Chiu, and T.H. Chuang, Z. Metallkd. 93, 95 (2002).10.3139/146.020095 ↗
7. M.Y. Chiu, S.S. Wang, and T.H. Chuang, J. Electron. Mater. 31, 494 (2002).10.1007/s11664-002-0105-8 ↗
8. P. Harris, Soldering Surf. Mount Technol. 11, 46 (1999).10.1108/09540919910293874 ↗
9. R.K. Shiue, L.W. Tsay, C.L. Lin, and J.L. On, Microelectron. Reliab. 43, 453 (2003).10.1016/S0026-2714(02)00259-7 ↗
10. T.H. Chuang, H.M. Wu, M.D. Cheng, S.Y. Chang, and S.F. Yen, J. Electron. Mater. 33, 22 (2004).10.1007/s11664-004-0289-1 ↗
11. Y.C. Chan, M.Y. Chiu, and T.H. Chuang, Z. Metallkd. 93, 95 (2002).10.3139/146.020095 ↗
12. K. Suganuma and K. Niihara, J. Mater. Res. 13, 2859 (1998).10.1557/JMR.1998.0391 ↗
13. W.H. Lin and T.H. Chuang, Mater. Eng. Performance 12, 452 (2003).10.1361/105994903770343015 ↗
14. H.M. Lee, S.W. Yoon, and B.J. Lee, J. Electron. Mater. 27, 1161 (1998).10.1007/s11664-998-0065-8 ↗
15. S.W. Yoon, J.R. Soh, H.M. Lee, and B.J. Lee, Acta Mater. 45, 951 (1997).10.1016/S1359-6454(96)00253-4 ↗
16. S.W. Yoon, W.K. Choi, and H.M. Lee, Scripta Mater. 40, 327 (1999).10.1016/S1359-6462(98)00414-X ↗
17. F.H. Huang and H.B. Huntington, Phys. Rev. B9 1479 (1974).10.1103/PhysRevB.9.1479 ↗