Abstract

The thermal fatigue endurance of completely lead-free 95.5Sn4Ag0.7Cu/plastic core solder ball (PCSB) composite joint structures in low-temperature Co-fired ceramic/printed wiring board (LTCC/PWB) assemblies was investigated using thermal cycling tests over the temperature ranges of −40°C–125°C and 0°C–100°C. Two separate creep/fatigue failures initiated and propagated in the joints during the tests: (1) a crack along the intermetallic compound (IMC)/solder interface on the LTCC side of the joint, which formed at the high-temperature extremes; and (2) a crack in the solder near the LTCC solder land, which formed at the low-temperature extremes. Moreover, localized recrystallization was detected at the outer edge of the joints that were tested in the harsh (−40°C–125°C) test conditions. The failure mechanism was creep/fatigue-induced mixed intergranular and transgranular cracking in the recrystallized zone, but it was dominated by transgranular thermal fatigue failure beyond the recrystallized zone. The change in the failure mechanism increased the rate of crack growth. When the lower temperature extreme was raised from −40°C to 0°C, no recrystallized zone was detected and the failure was due to intergranular cracks.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Electronic Packaging and Soldering Technologies · 3D IC and TSV technologies · Advanced Welding Techniques Analysis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (18)

Show source-provided references
1. Prabhu A., Schaefer W.J., Patil S. (2000) Proc. 26th IEEE/CPMT International Electronics Manufacturing Technology Symp. Piscataway, NJ: IEEE, pp. 311–323
2. Nousiainen O., Rautioaho R., Kautio K., Jääskeläinen J., Leppävuori S. (2005) Solder Surf. Mt. Technol. 17:3210.1108/09540910510613538 ↗
3. T. Kangasvieri, O. Nousiainen, J. Putaala, R. Rautioaho, and J. Vähäkangas, Microelectron. Reliab. (in press)
4. O. Nousiainen, J. Putaala, T. Kangasvieri, R. Rautioaho, and J. Vähäkangas, J. Electron. Mater. (accepted for publication)
5. M. Klein, H. Oppermann, S. Behnke, K. Halser, R. Aschenbrenner, and H. Reichl, Proc. IMAPS Nordic Conf. (IMAPS, 2002) pp. 157–162
6. D. Schwanke, T. Haas, C. Zeilmann, K. Halser, and M. Klein, Proc. 14th European Microelectronics and Packaging Conf. (IMAPS, 2003), pp. 213–218
7. Movva S., Aguirre G. (2004) Proc. 2004 Electronic Components and Technology Conf. Piscataway, NJ: IEEE, pp. 1443–1448
8. J. Bartelo et␣al., Proc. IPC SMEMA Council APEX 2001 (IPC, 2001), pp. LF2-2 1–LF2-2 12
9. J.-P. Clech, Proc. IPC Printed Circuits Expo (IPC, 2004) p.␣S28-3-1–S28-3-14
10. O. Salmela, K. Andersson, J. Särkkä, and M. Tammenmaa, Proc. Pan Pacific Microelectronics Symp. Conf. (SMTA, 2005), pp. 161–169
11. Qi Y., Lam R., Ghorbani H.R., Snugovsky P., Spelt J.K. (2006) Microelectron. Reliab. 46:57410.1016/j.microrel.2005.01.008 ↗
12. JEDEC Standard No. 22-A104C (JEDEC, 2005)
13. Semmens J.E., Kessler L.W. (1997) Proc. 5th Annual IEEE International Reliability Physics Symp. Piscataway, NJ: IEEE, pp. 141–148
14. O. Nousiainen, R. Rautioaho, S. Leppävuori, A. Uusimäki, and D. Tian, Proc. 13th European Microelectronic and Packaging Conf. (IMAPS, 2001), pp. 172–177
15. Terashima S., Takahama K., Nozaki M., Tanaka M. (2004) Mater. Trans. 45:138310.2320/matertrans.45.1383 ↗
16. Hendersson D.W., et␣al. (2004) J. Mater. Res. 19:160810.1557/JMR.2004.0222 ↗
17. Mattila T.T., Vuorinen V., Kivilahti J.K. (2004) J. Mater. Res. 19:321410.1557/JMR.2004.0436 ↗
18. Terashima S., Kariya Y., Hosoi T., Tanaka M. (2003) J. Electron. Mater. 32:152710.1007/s11664-003-0125-z ↗