Galvanomagnetic properties of CdTe below and above the melting point
Source abstract
Abstract
Temperature dependence of conductivity and Hall coefficient RH is measured by DC and AC methods at temperatures between 600–1180°C. Two experimental approaches are used.1 Galvanomagnetic measurements at defined temperature and Cd or Te pressure are performed in solid samples in the whole field of stability of solid in the pressure-temperature (P-T) diagram.2 Galvanomagnetic measurements define temperature both in solid and in liquid phase. The typical semiconducting character of and 1/|eRH|, when both parameters increase with temperature, is observed also in the liquid. The negative sign of RH is observed above 600°C within the whole region of stability of solid, both at Cd and at Te saturation, and RH<0 both in solid and liquid. 1/|eRH| reaches 5 1019 cm−3 at 1180°C and the corresponding Hall mobility is 20 cm2/Vs. Three slopes characterize the temperature dependence of a 0.7 eV in the solid CdTe below the melting point 1092°C and 4.6 eV in the liquid phase at 1092°C<T<1160°C. Above 1160°C, conductivity increases moderately with the slope 0.8 eV. The experimental data for solid CdTe are evaluated by a theoretical model, including electrons from both the central minimum (-point) and four satellite minima (L-point) of the Brillouin zone. Theab initio results fit our experimental data after small modifications very well.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced Semiconductor Detectors and Materials · Quantum and electron transport phenomena · Surface and Thin Film Phenomena
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (33)
Show source-provided references
1. D. Nobel,Philips Res. Rep. 14, 361, 430 (1959).
2. M.R. Lorenz,J. Phys. Chem. Sol. 23, 939 (1962).10.1016/0022-3697(62)90151-8 ↗
3. R.F. Brebrick,J. Electrochem. Soc. 118, 2014 (1971).10.1149/1.2407898 ↗
4. J.H. Greenberg, V.N. Guskov, V.B. Lazarev, and O.V. Shebershneva,J. Solid State Chem. 102, 382 (1993).10.1006/jssc.1993.1049 ↗
5. R. Fang and R.F. Brebrick,J. Phys. Chem. Sol. 57, 443 (1996).10.1016/0022-3697(95)00251-0 ↗
6. M.A. Berding,Appl. Phys. Lett. 74, 553 (1999).
7. F.T.J. Smith,Met. Trans. 1, 617 (1970).10.1007/BF02811585 ↗
8. S.S. Chern, H.R. Vydyanath, and F.A. Kröger,J. Solid State Chem. 14, 33 (1975).10.1016/0022-4596(75)90359-X ↗
9. M. Wienecke, H. Berger, and M. Schenk,Mater. Sci. Eng. B 16, 219 (1992).10.1016/0921-5107(93)90048-R ↗
10. J. Franc, R. Grill, L. Turjanska, P. Höschl, E. Belas, and P. Moravec,J. App. Phys. 89, 786 (2001).10.1063/1.1321774 ↗
11. T.C. Yu and R.F. Brebrick,J. Phase Equilibria 13, 476 (1992).10.1007/BF02665761 ↗
12. M. Mühlberg, P. Rudolph, M. Laasch, and E. Treser,J. Cryst. Growth 128, 571 (1993).10.1016/S0022-0248(07)80002-9 ↗
13. R.F. Brebrick, C.-H. Su, and P.-K. Liao,Semiconductors and Semimetals, vol. 19, ed. R.K. Willardson and A.C. Beer (New York: Academic Press, 1983), p. 171.10.1016/S0080-8784(08)60276-8 ↗
14. J.P. Gaspard, C. Bergman, C. Bichara, R. Bellissent, P. Chieux and J. Goffart,J. Non-Crystalline Solids 97–98, 1283 (1987).10.1016/0022-3093(87)90307-3 ↗
15. V. Glazov, S. Chizhevskaya, and N. Glagoleva,Liquid Semiconductors (New York: Plenum Press, 1969).10.1007/978-1-4899-6451-9 ↗
16. L. Shcherbak,J. Cryst. Growth 197, 397 (1999).10.1016/S0022-0248(98)00737-4 ↗
17. V. Godlevsky, M. Jain, J. Derby, and J.R. Chelikowsky,Phys. Rev. B 60, 8640 (1999).10.1103/PhysRevB.60.8640 ↗
18. P. Höschl, E. Belas, L. Turjanska, R. Grill, J. Franc, R. Fesh, and P. Moravec,J. Cryst. Growth 220, 440 (2001).
19. R.C. Whelan and D. Shaw,Phys. Stat. Sol. 29, 145 (1968).10.1002/pssb.19680290115 ↗
20. O.A. Matveev, Yu.V. Rud, and V. Sanin,Sov. Phys. Semicond. 3, 779 (1969).
21. K.R. Zanio,Appl. Phys. Lett. 15, 260 (1969).10.1063/1.1652992 ↗
22. O. Panchouk, P. Fochouk, and P. Feichouk,J. Cryst. Growth 161, 144 (1996);J. Solid State Chem. 14, 33 (1975).10.1016/0022-0248(95)00624-9 ↗
23. O. Madelung, editor,Semiconductors—Basic Data, 2nd rev. edition (Berlin: Springer, 1996), p. 267.
24. D. Kranzer,Phys. Stat. Sol. (a) 26, 11 (1974).10.1002/pssa.2210260102 ↗
25. M.A. Berding, M. van Schilfgaarde, and A. Sher,Phys. Rev. B 50, 1519 (1994).10.1103/PhysRevB.50.1519 ↗
26. M.A. Berding, private communication (2000).
27. M.R. Lorenz and B. Segall,Phys. Lett. 7, 18 (1963).10.1016/0031-9163(63)90423-2 ↗
28. P. Emanuelsson, P. Omling, B.K. Meyer, M. Wienecke, and A. Schenk,Phys. Rev. B 47, 15578 (1993).10.1103/PhysRevB.47.15578 ↗
29. B.K. Meyer, P. Omling, E. Wiegel, and G. Mueller-Vogt,Phys. Rev. B 46, 15135 (1992).10.1103/PhysRevB.46.15135 ↗
30. B.K. Meyer and W. Stadler,J. Cryst. Growth 161, 119 (1996).10.1016/0022-0248(95)00620-6 ↗
31. J.V. Rud and K.V. Sanin,Sov. Phys. Semicond. 5, 1385 (1972).
32. H.N.G. Wadley and B.W. Choi,J. Cryst. Growth 172, 323 (1997).10.1016/S0022-0248(96)00497-6 ↗
33. R.F. Brebrick and R. Fang,J. Phys. Chem. Sol. 57, 451 (1996).10.1016/0022-3697(95)00250-2 ↗