Abstract

The effect of aging on the microstructure and shear strength of 62Sn36Pb2Ag/Ni-P/Cu and SnAg/Ni-P/Cu surface mount solder joints was investigated. An intermetallic (IMC) layer of Ni3Sn4 forms at the interface between both solders and the Ni-P barrier layer and it thickens with aging time, with a decrease in the thickness of remaining Ni-P layer. The SnAg solder joint initially has a greater shear force than that of SnPbAg, but it drops dramatically after 250 h aging, and fracture occurs at the Ni-P/Cu interface afterwards, although it initiates in the solder in the initial stage of aging. The fracture in SnAg solder joint may arise from the excessive depletion of Ni characterized by a rapid accumulation of P in the remaining Ni-P layer, which results in a poor adhesion between the Ni-P layer and the Cu substrate. However, for the SnPbAg solder joint, the shear force initially decreases rapidly then asymptotically approaches a minimum, and fracture occurs from inside solder toward the solder/Ni-P interface. SnPbAg solder joint keeps relatively higher shear strength compared to SnAg solder joint after long term aging even though it decreases with aging time.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Electronic Packaging and Soldering Technologies · Intermetallics and Advanced Alloy Properties · 3D IC and TSV technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (19)

Show source-provided references
1. W.J. Tomlinson and A. Fullylove, J. Mater. Sci. 27, 5777 (1992).10.1007/BF01119737 ↗
2. S.K. Kang and A.K. Sarkhel, J. Electron. Mater. 23, 701 (1994).10.1007/BF02651362 ↗
3. J.S. Hwang and R.M. Vorgas, Soldering & Surface Mount Technol. 5, 38 (1990).10.1108/eb037718 ↗
4. D.R. Frear, F.M. Hosking, and P.T. Vianco, Proc. Mater. Devel. in Microelectronic Pkg., ed. P. Singh (Materials Park, OH: ASM, 1991), p. 229.
5. H.N. Keller, IEEE Trans. Comp. Hybrids. Manuf. Technol. 9, 433 (1986).10.1109/TCHMT.1986.1136673 ↗
6. A.H. Graham, R.W. Lindsay, and H.J. Read, J. Electrochem. Soc. 112, 401 (1965).10.1149/1.2423557 ↗
7. K.L. Lin and P.J. Lai, J. Electrochem. Soc. 136, 3803 (1989).10.1149/1.2096552 ↗
8. L.F. Spencer, Metal Finishing 22, 35 (1974).
9. H.G. Schenel and H. Kreye, Plating Surf. Finishing 77, 50 (1990).
10. C.Y. Lee and K.L. Lin, Thin Solid Films 249, 201 (1994).10.1016/0040-6090(94)90761-7 ↗
11. W.J. Tomlinson and H.G. Rhodes, J. Mater. Sci. 22, 1769 (1987).10.1007/BF01132405 ↗
12. C.Y. Lee and K.L. Lin, Thin Solid Films 229, 63 (1993).10.1016/0040-6090(93)90411-H ↗
13. M. Inaba, K. Yamakawa, and N. Iwase, IEEE Trans. Comp. Hybrids. Manuf. Technol. 13, 119 (1990).10.1109/33.52858 ↗
14. G.Y. Li and Y.L. Chan, IEEE Trans. Comp. Hybrids. Manuf. Technol, B21, 398 (1998).
15. Y.Y. Wei and J.G. Duh, J. Mater. Sci. 9, 373 (1998).
16. P.M. Hansen, Constitution of Binary Alloys (New York: McGraw-Hill, 1958), pp. 2, 52.
17. K.N. Tu and R. Rosenberg, Jpn. J. Appl. Phys. Suppl. 2, 633 (1974).
18. G.G. Gawrilov, Chemical (Electroless) Nickel-Plating (England: Portcullis Press, 1979), p. 78.
19. C.D. Young and J.G. Duh, IEEE Trans. Comp. Hybrids. Manuf. Technol. 21, 330 (1998).