Thermosonic bonding of gold wire onto a copper pad with titanium thin-film deposition
Source abstract
Abstract
A novel thermosonic (TS) bonding process for gold wire bonded onto chips with copper interconnects was successfully developed by depositing a thin, titanium passivation layer on a copper pad. The copper pad oxidizes easily at elevated temperature during TS wire bonding. The bondability and bonding strength of the Au ball onto copper pads are significantly deteriorated if a copper-oxide film exists. To overcome this intrinsic drawback of the copper pad, a titanium thin film was deposited onto the copper pad to improve the bondability and bonding strength. The thickness of the titanium passivation layer is crucial to bondability and bonding strength. An appropriate, titanium film thickness of 3.7 nm is proposed in this work. One hundred percent bondability and high bonding strength was achieved. A thicker titanium film results in poor bond-ability and lower bonding strength, because the thicker titanium film cannot be removed by an appropriate range of ultrasonic power during TS bonding. The protective mechanism of the titanium passivation layer was interpreted by the results of field-emission Auger electron spectroscopy (FEAES) and electron spectroscopy for chemical analysis (ESCA). Titanium dioxide (TiO2), formed during the die-saw and die-mount processes, plays an important role in preventing the copper pad from oxidizing. Reliability of the high-temperature storage (HTS) test for a gold ball bonded on the copper pad with a 3.7-nm titanium passivation layer was verified. The bonding strength did not degrade after prolonged storage at elevated temperature. This novel process could be applied to chips with copper interconnect packaging in the TS wire-bonding process.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Electronic Packaging and Soldering Technologies · 3D IC and TSV technologies · Advanced Welding Techniques Analysis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (20)
Show source-provided references
1. G. Deltoro and N. Sharif, 24th IEEE/CPMT (Piscataway, NJ: IEEE, 1999), pp. 185–188.
2. G.G. Harman, Wire Bonding in Microelectronics (New York: McGraw-Hill, 1997), p. 29.
3. J.N. Aoh, C.L. Chuang, and R.F. Din, Microelectron. Reliab., in revision.
4. J.N. Aoh and C.L. Chuang, J. Electron. Mater. 33, 290 (2004).10.1007/s11664-004-0135-5 ↗
5. T.A. Tran, L. Yong, S. Chen, and A. Chen, IEEE Electronic Components and Technology Conf. (Piscataway, NJ: IEEE, 2000), pp. 1674–1680.
6. J.F. Rohan, G. O’Riordan, and J. Boardman, Appl. Surf. Sci. 185, 289 (2002).10.1016/S0169-4332(01)00982-5 ↗
7. H.S. Chang, J.X. Pon, K.C. Heien, and C.C. Chen, J. Electron. Mater. 30, 1171 (2001).10.1007/s11664-001-0146-4 ↗
8. A. Kumar, H. Bakhru, C. Jin, W.W. Lee, and T.M. Lu, J. Appl. Phys. 81, 3567 (2000).10.1063/1.372381 ↗
9. J. Li, J.W. Mager, and E.G. Colgan, J. Appl. Phys. 70, 2820 (1991).10.1063/1.349344 ↗
10. Y.H. Kim, Y.S. Chaug, N.J. Chou, and J. Kim, J. Vac. Sci. Technol. A 5, 2890 (1987).10.1116/1.574259 ↗
11. EIA/JESD22-B116, Wire Bond Shear Test, EIA/JEDEC STANDARD (Arlington, VA: Electronic Industries Alliance, 1998).
12. MIL-STD 833E, Method No. 2011.7—Bond Strength (Destructive Bond Pull Test), Test Methods Standards for Microcircuits (Philippines: elmBE Research, 1997), semiconfareast.com.
13. G.G. Harman, Wire Bonding in Microelectronics (New York: McGraw-Hill, 1997), p. 23.
14. M. Petzold, L. Berthold, D. Katzer, H. Knoll, D. Memhard, P. Meier, and K.D. Lang, Microelectron. Reliab. 40, 1515 (2000).10.1016/S0026-2714(00)00130-X ↗
15. G.G. Harman, Wire Bonding in Microelectronics (New York: McGraw-Hill, 1997), p. 182.
16. F. Zhang, S. Jin, Y. Mao, Z. Zheng, Y. Chen, and X. Liu, Thin Solid Films 310, 29 (1997).10.1016/S0040-6090(97)00338-6 ↗
17. A.F. Carley, P.R. Chalker, J.C. Riviere, and M.W. Roberts, J. Chem. Soc. Faraday Trans. 83, 351 (1987).10.1039/f19878300351 ↗
18. R. Zanoni, G. Righini, A. Montenero, G. Gnappi, G. Montesperelli, E. Traversa, and G. Gusmano, Surf. Interface Anal. 22, 5645 (1994).10.1002/sia.740220182 ↗
19. J. Pouilleau, D. Devilliers, H. Groult, and P.J. Marcus, Mater. Sci. 32, 5645 (1997).10.1023/A:1018645112465 ↗
20. I. Vaquila, L.I. Vergara, M.C.G. Passeggi, Jr., R.A. Vidal, and J. Ferron, Surf. Coating Technol. 122, 67 (1999).10.1016/S0257-8972(99)00420-X ↗