Effects of Cu, Ag and Sb on the creep-rupture strength of lead-free solder alloys
Source abstract
Abstract
The materials used in the present research are pure Sn metal and Sn-0.5% Cu, Sn-3.5%Ag, Sn-0.3%Sb, and Sn-3.5%Ag-0.5%Cu alloys. Effects of Cu, Ag and Sb on the creep-rupture strength of lead-free solder alloys have been investigated. Creep tests are performed at the stress and temperature range of 3 to 12 MPa and 378 to 403 K, respectively. A 3.5% addition of Ag had the largest contribution to the creep-rupture strength of Sn metal among the single addition of 0.5%Cu, 3.5%Ag, and 0.3%Sb. The combined addition of 3.5%Ag and 0.5%Cu makes the largest creep-rupture strength. The effects of these elements on the microstructure of the lead-free alloys are also investigated with optical microscope (OM) and transmission electron microscope (TEM) observations.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Electronic Packaging and Soldering Technologies · Aluminum Alloys Composites Properties · Aluminum Alloy Microstructure Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (7)
Show source-provided references
1. T. Sawamura, Almit Technical Journal 29, 1 (1996).
2. J. Glazer, J. Electron. Mater. 23, 693 (1994).10.1007/BF02651361 ↗
3. K.L. Murty, F.M. Haggag, and R.K. Mahidhara, J. Electron. Mater. 26, 839 (1997).10.1007/s11664-997-0260-z ↗
4. N. Wade, T. Akuzawa, S. Yamada, D. Sugiyama, I.-S. Kim, and K. Miyahara, J. Electron. Mater. 28, 1286 (1999).10.1007/s11664-999-0169-9 ↗
5. N. Wade, T. Akuzawa, J. Kunii, and K. Miyahara, Key Engineering Mater. 171–174, 663 (2000).
6. Metal Data Book (Jpn. Inst. of Metals, Maruzen, 1984), p. 420.
7. Handbook of Ternary Alloy Phase Diagram (Materials Park, OH: ASM Int., 1995).