journal article·2021-10

Dielectric Properties and DC Bias Characteristics of BaTi1-mZrmO3-x mol.% MgO-4.5 mol.% Gd2O3-2 mol.% SiO2 Ceramics

Sea-Fue Wang, Yung-Fu Hsu, Chun-Wei Chang, Yi-Le Liao, Jian-Hua Li, Yuan-Cheng Lai

Journal of Electronic Materials· Volume 50· Issue 10
Publisher page

Abstract

In this study, BaTi1-mZrmO3-4.5 mol.% Gd2O3-2.0 mol.% SiO2 ceramics with different Zr/Ti ratios and MgO contents were prepared via solid-state reaction. The MgO addition decreased the densification temperatures of the ceramics and increased the second phase Ba2GdZrO5.5 content. The temperature coefficient of capacitance curves of the ceramics had an almost linear variation with temperature, with negative temperature coefficients. With the increase of the Zr4+/Ti4+ ratio and MgO content, the temperature coefficient of capacitance rotated counter clockwise due to the lower Tm temperature, and a smaller tan δ and a higher electrical resistance were obtained at room temperature. The Zr4+ ion replacement and MgO addition reduced the $${\text{Ti}}^\prime_{{\text{Ti}}}$$ concentrations, and therefore, lessened the hopping conduction between Ti4+ and Ti3+ ions, while excess MgO produced $${V_O \bullet \bullet }$$ and had an opposing effect. Additionally, larger amounts of MgO led to smaller grain sizes, and thus, more insulating grain boundaries. The change in the dielectric constant with the bias field, a typical nonlinear dielectric behavior, decreased with increasing MgO content and Zr4+/Ti4+ ratio. For BaTi0.70Zr0.30O3 ceramics with additives of 6 mol.% MgO, 4.5 mol.% Gd2O3, and 2 mol.% SiO2, the dielectric constant changed by a minimum value of 0.37% under a bias of 2.5 kV/mm.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Ferroelectric and Piezoelectric Materials · Microwave Dielectric Ceramics Synthesis · Dielectric properties of ceramics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (36)

Show source-provided references
1. K. Hong, T.H. Lee, J.M. Suh, S.H. Yoon, and H.W. Jang, J. Mater. Chem. C 7, 9782 (2019).10.1039/C9TC02921D ↗
2. D. Zhan, Q. Xu, D.P. Huang, H.X. Liu, W. Chen, and F. Zhang, J. Phys. Chem. Solids 114, 220 (2018).10.1016/j.jpcs.2017.10.038 ↗
3. B. Guo, P. Liu, X. Cui, and Y. Song, J. Alloys Compd. 740, 1108 (2018).10.1016/j.jallcom.2018.01.052 ↗
4. D. Zhan, Q. Xu, D.P. Huang, H.X. Liu, W. Chen, and F. Zhang, J. Alloys Compd. 682, 594 (2016).10.1016/j.jallcom.2016.04.317 ↗
5. Q. Luo, X. Li, Z. Yao, L. Zhang, J. Xiea, H. Hao, M. Cao, A. Manan, and H. Liu, Ceram. Int. 44, 5304 (2018).10.1016/j.ceramint.2017.12.146 ↗
6. T. Tsurumi, M. Shono, H. Kakemoto, S. Wada, K. Saito, and H. Chazono, J. Electroceramics 21, 17 (2008).10.1007/s10832-007-9071-0 ↗
7. M. Tamura, S. Takagi, D. Sakurai, S. Aman, Y. Kamada, Dielectric ceramic composition and electronic component. US 8,450,230 B2 (2013).
8. J. Zhao, L. Li, Y. Wang, and Z. Gui, Mater. Sci. Eng. B-Adv. 99, 207 (2003).10.1016/S0921-5107(02)00532-9 ↗
9. D.W. Hahn, J.O. Hong, and Y.H. Han, Jpn. J. Appl. Phys. 47, 5526 (2008).10.1143/JJAP.47.5526 ↗
10. G. Yang, Z. Yue, Z. Gui, and L. Li, J. Appl. Phys. 104, 074115 (2008).10.1063/1.2998906 ↗
11. G. Yang, Z. Yue, J. Zhao, H. Wen, X. Wang, and L. Li, J. Phys. D 39, 3702 (2006).10.1088/0022-3727/39/16/027 ↗
12. Z. Yue, J. Zhao, G. Yang, and L. Li, Ferroelectr. 401, 56 (2010).10.1080/00150191003670424 ↗
13. T. Tsurumi, Y. Yamamoto, H. Kakemoto, and S. Wada, J. Mater. Res. 17, 755 (2002).10.1557/JMR.2002.0110 ↗
14. J.Q. Zhao, L.T. Li, T. Li, Z.L. Gui, and Y.C. Zhang, Key Eng. Mater. 224–226, 59 (2002).10.4028/www.scientific.net/KEM.224-226.59 ↗
15. R. Liang, X.L. Dong, Y. Chen, F. Cao, and Y.L. Wang, Ceram. Int. 33, 957 (2007).10.1016/j.ceramint.2006.02.009 ↗
16. C. Mao, S. Yan, C. Yao, F. Cao, G. Wang, X. Dong, and X. Men, Mater. Res. Express. 4, 016302 (2017).10.1088/2053-1591/aa523a ↗
17. C. Zhu, X. Wang, Q. Zhao, Z. Cai, Z. Cen, and L. Li, J. Eur. Ceram. Soc. 39, 1142 (2019).10.1016/j.jeurceramsoc.2018.11.034 ↗
18. H. Gong, X. Wang, S. Zhang, H. Wen, and L. Li, J. Eur. Ceram. Soc. 34, 1733 (2014).10.1016/j.jeurceramsoc.2013.12.028 ↗
19. D. Zhan, Q. Xu, D. Huang, H.J. Sun, F. Gao, and F. Zhang, J. Electron. Mater. 46, 4503 (2017).10.1007/s11664-017-5435-7 ↗
20. Y. Zhang, Y. Li, H. Zhu, Z. Fu, and Q. Zhang, J. Mater. Sci. Mater. Electron. 27, 9572 (2016).10.1007/s10854-016-5010-7 ↗
21. X. Diez-Betriu, J.E. Garcia, C. Ostos, A.U. Boya, D.A. Ochoa, L. Mestres, and R. Perez, Mater. Chem. Phys. 125, 493 (2011).10.1016/j.matchemphys.2010.10.027 ↗
22. H. Gong, X. Wang, Q. Zhao, and L. Li, J. Mater. Sci. 50, 6898 (2015).10.1007/s10853-015-9228-1 ↗
23. R.D. Shannon, Acta Crystallogr. A A32, 751 (1976).10.1107/S0567739476001551 ↗
24. L. Santos-Gómez, L. León-Reina, J.M. Porras-Vázquez, E.R. Losilla, and D. Marrero-López, Solid State Ion. 239, 1 (2013).10.1016/j.ssi.2013.03.005 ↗
25. F.A. Kröger, and H.J. Vink, Solid State Phys. 3, 307 (1956).10.1016/S0081-1947(08)60135-6 ↗
26. M.A. Alam, L. Zuga, and M.G. Pecht, Ceram. Int. 38, 6091 (2012).10.1016/j.ceramint.2012.05.068 ↗
27. Y. Tsur, A. Hitomi, I. Scrymgeour, and C.A. Ran, Jpn. J. Appl. Phys. 40, 255 (2001).10.1143/JJAP.40.255 ↗
28. Y. Sakabe, Y. Hamaji, H. Sano, and N. Wada, Jpn. J. Appl. Phys. 41, 5668 (2002).10.1143/JJAP.41.5668 ↗
29. S.H. Yoon, M.H. Hong, J.O. Hong, Y.T. Kim, and K.H. Hur, J. Appl. Phys. 102, 054105 (2007).10.1063/1.2777119 ↗
30. L. Li, R. Guo, P. Zhang, J. Zhao, and H. Wang, J. Rare Earths 25, 151 (2007).10.1016/S1002-0721(07)60545-6 ↗
31. S. Wang, S. Zhang, X. Zhou, B. Li, and Z. Chen, Mater. Lett. 59, 2457 (2005).10.1016/j.matlet.2005.03.016 ↗
32. M.A. Gomes, A.S. Lima, K.I.B. Eguiluz, and G.R. Salazar-Banda, J. Mater. Sci. 51, 4709 (2016).10.1007/s10853-016-9789-7 ↗
33. X. Chou, J. Zhai, H. Jiang, and X. Yao, J. Appl. Phys. 182, 084106 (2007).10.1063/1.2799081 ↗
34. J. Jeong, and Y.H. Han, Phys. Chem. Chem Phys. 5, 2264 (2003).10.1039/B300231B ↗
35. H. Kishi, N. Kohzu, J. Sugino, H. Ohsato, Y. Iguchi, and T. Okuda, J. Eur. Ceram. Soc. 19, 1043 (1999).10.1016/S0955-2219(98)00370-7 ↗
36. Electrical Industry Alliance (EIA), World Capacitor Trade Statistics (WCTA), 2002.