Effects of Minor Addition of Cu and Ni on the Microstructure, Thermal and Mechanical Properties, and Wettability of Sn-58Bi Solder Alloys

Phairote Sungkhaphaitoon, Suchart Chantaramanee

Journal of Electronic Materials· Volume 54· Issue 5
Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Electronic Packaging and Soldering Technologies · 3D IC and TSV technologies · Advanced Welding Techniques Analysis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (50)

Show source-provided references
1. E. Gouda, I. Faquhi, S. Kariri, M. Qohal, and Y. Kariri, Structure, electrical resistivity, oxidation and corrosion behaviour of tin-lead eutectic alloy. Int. J. Mater. Sci. Appl. 4, 8 (2015).
2. K. Prakash and T. Sritharan, Tensile fracture of tin-lead solder joints in copper. Mater. Sci. Eng. A 379, 277 (2004).10.1016/j.msea.2004.02.049 ↗
3. O.R. Adetunji, R.A. Ashimolowo, P.O. Aiyedun, O.M. Adesusi, H.O. Adeyemi, and O.R. Oloyede, Tensile, hardness and microstructural properties of Sn-Pb solder alloys. Mater. Today Proc. 44, 321 (2021).10.1016/j.matpr.2020.09.656 ↗
4. F.J. Wang, M.O. Keefe, and B. Brinkmeyer, Microstructural evolution and tensile properties of Sn-Ag-Cu mixed with Sn-Pb solder alloys. J. Alloys Compd. 477, 267 (2009).10.1016/j.jallcom.2008.10.141 ↗
5. H.J. Lin and T.H. Chuang, Interfacial microstructure and bonding strength of Sn-3Ag-05Cu and Sn-3Ag-0.5Cu-0.5Ce-xZn solder BGA packages with immersion Ag surface finish. Microelectron. Reliab. 51, 445 (2011).10.1016/j.microrel.2010.07.061 ↗
6. Y. Liu and K.N. Tu, Low melting point solders based on Sn, Bi, and In elements. Mater. Today Adv. 8, 100115 (2020).10.1016/j.mtadv.2020.100115 ↗
7. H.R. Kotadia, P.D. Howes, and S.H. Mannan, A review: on the development of low melting temperature Pb-free solders. Micron. Reliab. 54, 1253 (2014).10.1016/j.microrel.2014.02.025 ↗
8. F. Wang, H. Chen, Y. Huang, L. Liu, and Z. Zhang, Recent progress on the development of Sn-Bi based low-temperature Pb-free solders. J. Mater. Sci. Mater. Electron. 30, 3222 (2019).10.1007/s10854-019-00701-w ↗
9. S.A. Belyakov and C.M. Gourlay, Recommended values for the β-Sn solidus line in Sn-Bi alloys. Thermochim. Acta 654, 65 (2017).10.1016/j.tca.2017.05.009 ↗
10. X. Chen, J. Zhou, F. Xue, and Y. Yao, Mechanical deformation behavior and mechanism of Sn-58Bi solder alloys under different temperatures and strain rates. Mater. Sci. Eng. A 662, 251 (2016).10.1016/j.msea.2016.03.072 ↗
11. I. Abdullah, M.N. Zulkifli, A. Jalar, and R. Ismail, Deformation behaviour of Sn-3.0Ag-0.5Cu (SAC305) solder wire under varied tensile strain rates. Solder. Surf. Mt Technol. 29, 110 (2017).10.1108/SSMT-08-2016-0017 ↗
12. Q.K. Zhang and Z.F. Zhang, In situ observations on shear and creep-fatigue fracture behaviors of SnBi/Cu solder joints. Mater. Sci. Eng. A 528, 2686 (2011).10.1016/j.msea.2010.12.041 ↗
13. F. Wang, D. Li, Z. Zhang, M. Wu, and C. Yan, Improvement on interfacial structure and properties of Sn-58Bi/Cu joint using Sn-3.0Ag-0.5Cu solder as barrier. J. Mater. Sci. Mater. Electron. 28, 19051 (2017).10.1007/s10854-017-7859-5 ↗
14. Z. Mei and J.W. Morris, Characterization of eutectic Sn-Bi solder joints. J. Electron. Mater. 21, 599 (1992).10.1007/BF02655427 ↗
15. L. Shen, P. Septiwerdani, and Z. Chen, Elastic modulus, hardness and creep performance of SnBi alloys using nanoindentation. Mater. Sci. Eng. A 558, 253 (2012).10.1016/j.msea.2012.07.120 ↗
16. O. Mokhtari and H. Nishikawa, Effects of In and Ni addition on microstructure of Sn-58Bi solder joint. J. Electron. Mater. 43, 4158 (2014).10.1007/s11664-014-3359-z ↗
17. P.L. Liu and J.K. Shang, Interfacial embrittlement by bismuth segregation in copper/tin-bismuth Pb-free solder interconnect. J. Mater. Res. 16, 1651 (2001).10.1557/JMR.2001.0229 ↗
18. Q. Zhang, H. Zou, and Z.F. Zhang, Improving tensile and fatigue properties of Sn-58Bi/Cu solder joints through alloying substrate. J. Mater. Res. 25, 303 (2010).10.1557/JMR.2010.0035 ↗
19. P.L. Liu and J.K. Shang, Interfacial embrittlement by bismuth segregation copper/tin-bismuth Pb-free solder interconnect. J. Mater. Res. 16, 1651 (2001).10.1557/JMR.2001.0229 ↗
20. H.F. Zou, Q.K. Zhang, and Z.F. Zhang, Transition of Bi embrittlement of SnBi/Cu joint couples with reflow temperature. J. Mater. Res. 26, 449 (2010).10.1557/jmr.2010.40 ↗
21. H. Kang, S.H. Rajendran, and J.P. Jung, Low melting temperature Sn-Bi Solder: effect of alloying and nanoparticle addition on the microstructural, thermal, interfacial bonding, and mechanical characteristics. Metals 11, 364 (2021).10.3390/met11020364 ↗
22. S. Zhou, C.H. Yang, S.K. Lin, A.N. AlHazaa, O. Mokhtari, X. Liu, and H. Nishikawa, Effects of Ti addition on the microstructure, mechanical properties and electrical resistivity of eutectic Sn58Bi alloy. Mater. Sci. Eng. A 744, 560 (2019).10.1016/j.msea.2018.12.012 ↗
23. A. Torres, L. Hernández, and O. Domínguez, Effect of antimony additions on corrosion and mechanical properties of Sn-Bi eutectic lead-free solder alloy. Mater. Sci. Appl. 3, 355 (2012).
24. Z. Wang, Q.K. Zhang, Y.X. Chen, and Z.L. Song, Influences of Ag and In alloying on Sn-Bi eutectic solder and SnBi/Cu solder joints. J. Mater. Sci. Mater. Electron. 30, 18524 (2019).10.1007/s10854-019-02206-y ↗
25. J. Shen, Y. Pu, H. Yin, D. Luo, and J. Chen, Effects of minor Cu and Zn additions on the thermal, microstructure and tensile properties of Sn-Bi-based solder alloys. J. Alloys Compd. 614, 63 (2014).10.1016/j.jallcom.2014.06.015 ↗
26. G. Xu, F. Guo, X. Wang, Z. Xia, Y. Lei, Y. Shi, and X. Li, Retarding the electromigration effects to the eutectic SnBi solder joints by micro-sized Ni-particles reinforcement approach. J. Alloy. Compd. 509, 878 (2011).10.1016/j.jallcom.2010.09.123 ↗
27. Y. Li and Y.C. Chan, Effect of silver (Ag) nanoparticle size on the microstructure and mechanical properties of Sn58Bi-Ag composite solders. J. Alloy. Compd. 645, 566 (2015).10.1016/j.jallcom.2015.05.023 ↗
28. W.X. Dong, Y.W. Shi, Z.D. Xia, Y.P. Lei, and F. Guo, Effects of trace amounts of rare earth additions on microstructure and properties of Sn-Bi-based solder alloy. J. Electron. Mater. 37, 982 (2008).10.1007/s11664-008-0458-8 ↗
29. W.R. Myung, M.K. Ko, Y. Kim, and S.B. Jung, Effects of Ag content on the reliability of LED package component with Sn-Bi-Ag solder. J. Mater. Sci. Mater. Electron. 26, 8707 (2015).10.1007/s10854-015-3546-6 ↗
30. R.M. Shalaby, Effect of silver and indium addition on mechanical properties and indentation creep behavior of rapidly solidified Bi-Sn based lead-free solder alloys. Mater. Sci. Eng. A 560, 86 (2013).10.1016/j.msea.2012.09.038 ↗
31. Z.M. Lai and D. Ye, Microstructure and properties of Sn-10Bi-xCu solder alloy/joint. J. Electron. Mater. 45, 3702 (2016).10.1007/s11664-016-4561-y ↗
32. O. Mokhtari and H. Nishikawa, Correlation between microstructure and mechanical properties of Sn-Bi-X solders. Mater. Sci. Eng. A 651, 831 (2016).10.1016/j.msea.2015.11.038 ↗
33. K. Kanlayasiri and T. Ariga, Physical properties of Sn58Bi-xNi lead-free solder and its interfacial reaction with copper substrate. Mater. Des. 86, 371 (2015).10.1016/j.matdes.2015.07.108 ↗
34. ASTM Standard ASTM E8/E8M-13a, 1924 (2013), "Standard Test Method for Tension Testing of Metallic Materials," ASTM International, West Conshohocken, PA, 2013, https://doi.org/10.1520/E0008_E0008M-13A10.1520/E0008_E0008M-13A ↗
35. P. Fima, T. Gancarz, J. Pstrus, and A. Sypien, Wetting of Sn-Zn-xIn (x = 0.5, 1.0, 1.5 wt%) alloys on Cu and Ni substrates. J. Mater. Eng. Perform. 21, 595 (2012).10.1007/s11665-012-0124-4 ↗
36. X. Chen, F. Xue, J. Zhou, and Y. Yao, Effect of In on microstructure, thermodynamic characteristic and mechanical properties of Sn-Bi based lead-free solder. J. Alloys Compd. 633, 377 (2015).10.1016/j.jallcom.2015.01.219 ↗
37. H.W. Miao and J.G. Duh, Microstructure evolution in Sn-Bi and Sn-Bi-Cu solder joints under thermal aging. Mater. Chem. Phys. 71, 255 (2001).10.1016/S0254-0584(01)00298-X ↗
38. A.A. El-Daly, Y. Swilem, and A.E. Hammad, Creep properties of Sn-Sb based lead-free solder alloys. J. Alloys Compd. 471, 98 (2009).10.1016/j.jallcom.2008.03.097 ↗
39. J. Chriašteľová and M. Ožvold, Properties of solders with low melting point. J. Alloys Compd. 457, 323 (2008).10.1016/j.jallcom.2007.03.062 ↗
40. K. Moon, W.J. Boettinger, U.R. Kattner, C.A. Handwerker, and D. Lee, The effect of Pb contamination on the solidification behavior of Sn-Bi solders. J. Electron. Mater. 30, 45 (2001).10.1007/s11664-001-0213-x ↗
41. A. Yakymovych and I. Shtablavyi, Effect of nanosized Ni reinforcements on the structure of the Sn-3.0Ag-0.5Cu alloy in liquid and after-eeflow solid states. Metals 13, 1093 (2023).10.3390/met13061093 ↗
42. D.C. Lin, T.S. Srivatsan, G.X. Wang, and R. Kovacevic, Microstructural development in a rapidly cooled eutectic Sn-3.5% Ag solder reinforced with copper powder. Powder Technol. 166, 38 (2006).10.1016/j.powtec.2006.02.009 ↗
43. J. Shen, Y.Y. Pu, H.G. Yin, and Q. Tang, Effects of Cu, Zn on the wettability and shear mechanical properties of Sn-Bi-based lead-free solders. J. Electron. Mater. 44, 532 (2015).10.1007/s11664-014-3460-3 ↗
44. R. Rashidi and H. Naffakh-Moosavy, The influence of chromium addition on the metallurgical, mechanical and fracture aspects of Sn-Cu-Bi/Cu solder joint. J. Mater. Res. Technol. 15, 3321 (2021).10.1016/j.jmrt.2021.10.015 ↗
45. M.J. Rizvi, C. Bailey, Y.C. Chan, M.N. Islam, and H. Lu, Effect of adding 0.3 wt% Ni into the Sn-0.7 wt% Cu solder: Part II Growth of intermetallic layer with Cu during wetting and aging. J. Alloys Compd. 438, 122 (2007).10.1016/j.jallcom.2006.08.071 ↗
46. J.W. Yoon, B.I. Noh, B.K. Kim, C.C. Shur, and S.B. Jung, Wettability and interfacial reactions of Sn-Ag-Cu/Cu and Sn-Ag-Ni/Cu solder joints. J. Alloys Compd. 486, 142 (2009).10.1016/j.jallcom.2009.06.159 ↗
47. C. Yang, F. Song, and S.W. Ricky Lee, Impact of Ni concentration on the intermetallic compound formation and brittle fracture strength of Sn-Cu-Ni (SCN) lead-free solder joints. Microelectron. Reliab. 54, 435 (2014).10.1016/j.microrel.2013.10.005 ↗
48. R. Sayyadi and H. Naffakh-Moosavy, The role of intermetallic compounds in controlling the microstructural, physical and mechanical properties of Cu-[Sn-Ag-Cu-Bi]-Cu solder joints. Sci. Rep. 9, 8389 (2019).10.1038/s41598-019-44758-3 ↗
49. L. Yin, Z. Zhang, Z. Su, H. Zhang, C. Zuo, Z. Yao, G. Wang, L. Zhang, and Y. Zhang, Interfacial microstructure evolution and properties of Sn-0.3Ag-0.7Cu-xSiC solder joints. Mater. Sci. Eng. A 809, 140995 (2021).10.1016/j.msea.2021.140995 ↗
50. L. Zang, Z. Yuan, H. Xu, and B. Xu, Wetting process and interfacial characteristic of Sn-3.0Ag-0.5Cu on different substrates at temperatures ranging from 503 K to 673 K. Appl. Surf. Sci. 257, 4877 (2011).10.1016/j.apsusc.2010.12.131 ↗