Thermoelectric Properties and Thermal Stability of BiCuSeO
Source abstract
Abstract
Although BiCuSeO has become of interest as a high performance thermoelectric material, it has been reported to be unstable in air above 548 K. However, the details of the thermal degradation of BiCuSeO have not yet been determined. In this study, the time dependence of the thermoelectric properties of BiCuSeO at 550 K was assessed along with the accompanying thermal degradation behavior. Variations in ρ and α over time at 550 K were determined using the direct current four-terminal method and small temperature difference method, respectively. In addition, the crystalline phases of the specimen after thermoelectric measurements were identified by x-ray diffraction (XRD) analysis, and the surface chemical states were analyzed by x-ray photoelectron spectroscopy (XPS). The results of thermoelectric property measurements over time showed that ρ abruptly increased between 135 min and 182 min then decreased from 182 min to 210 min, while the value of α exhibited the opposite trend. XPS and XRD data suggested that BiCuSeO was pyrolyzed upon heating at 550 K for 6 h in air. In contrast, thermogravimetric analysis demonstrated that BiCuSeO was stable below 800 K under inert gas flow, thus the pyrolysis observed at 550 K was the result of reaction with atmospheric oxygen.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced Thermoelectric Materials and Devices · Thermal Radiation and Cooling Technologies · Magnetic and transport properties of perovskites and related materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (13)
Show source-provided references
1. T. Kajikawa, The Handbook of Thermoelectric Engineering (NTS: Tokyo, 2008), p. 19.
2. The Ceramic Society of Japan and The Thermoelectric Society of Japan, Thermoelectric Conversion Material (Tokyo: Nikkan Kogyo Shimbun, 2005).
3. A.M. A.M.Kusainova, P.S. Berdonosov, L.G. Akselrud, L.N. Kholodkovskaya, V.A. Dolgikh, and B.A. Popovkin, J. Solid State Chem. 112, 189 (1994).10.1006/jssc.1994.1285 ↗
4. L.D. Hicks and M.S. Dresselhaus, Phys. Rev. B 47, 12727 (1993).10.1103/PhysRevB.47.12727 ↗
5. Y.-L. Pei, H. Wu, D. Wu, F. Zheng, and J. He, J. Am. Chem. Soc. 136, 13902 (2014).10.1021/ja507945h ↗
6. C. Barreteau, D. Berardan, and N. Dragoe, J. Solid State Chem. 222, 53 (2015).10.1016/j.jssc.2014.11.001 ↗
7. Y. Suge, Thermoelectric Semiconductor (Tokyo: Maki Shoten, 1966), p. 132.
8. K. Uemura and I.A. Nishida, Thermoelectric Semiconductor and Its Applications (Tokyo: The Nikkan Kogyo Shimbun, 1988), p. 186.
9. M. Sakata, Thermoelectric Conversion Engineering—Basics and Applications (Tokyo: Realize, 2001), pp. 297–303.
10. Y. Suge, Thermoelectric Semiconductor (Kyoto: Maki Shoten, 1966), p. 220.
11. K. Uemura and I.A. Nishida, Thermoelectric Semiconductor and Its Applications (Tokyo: The Nikkan Kogyo Shimbun, 1988), p. 183.
12. M. Sakata, Thermoelectric Conversion Engineering—Basics and Applications (Tokyo: Realize, 2001), p. 307.
13. F. Li, T.-R. Wei, F. Kang, and J.-F. Li, J. Alloy. Compd. 614, 394 (2014).10.1016/j.jallcom.2014.06.117 ↗