Effects of Second Phase Yb5Sb3 on the Thermoelectric Properties of YbAl3
Source abstract
Abstract
The compound YbAl3 exhibits a very high power factor but also rather a large thermal conductivity, leading to a low figure of merit. The second phase Yb5Sb3 was introduced in the YbAl3 matrix to reduce its thermal conductivity. The composites (YbAl3)1−x(Yb5Sb3)x with x = 0, 0.01, 0.05, 0.10, and 0.20 were synthesized by high frequency induction melting, annealing treatment, and spark plasma sintering. The thermoelectric properties of the composites were evaluated. The composites are of n-type conduction. The pure YbAl3 obtained in this work shows a high power factor of 11,500 μW m−1 K−2 but also a high thermal conductivity of 19.6 W m−1 K−1. However, the existence of Yb5Sb3 compound in the YbAl3 matrix enhances the electrical resistivity and the absolute Seebeck coefficient of the composite, but significantly reduces its thermal conductivity in the temperature range considered, thereby enhancing the figure of merit. The highest ZT value of 0.23 may be obtained in the sample (YbAl3)0.95(Yb5Sb3)0.05 at room temperature, which is apparently higher than that of pure YbAl3.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced Thermoelectric Materials and Devices · Thermodynamic and Structural Properties of Metals and Alloys · Thermal properties of materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (11)
Show source-provided references
1. C. Boulanger, J. Electron. Mater. 39, 1818 (2010).10.1007/s11664-010-1079-6 ↗
2. D.M. Rowe, V.L. Kuznetsov, L.A. Kuznetsova, and G. Min, J. Phys. D Appl. Phys. 35, 2183 (2002).10.1088/0022-3727/35/17/315 ↗
3. G. Zanicchi, P. Riani, D. Mazzone, R. Marazza, D. Rossi, and R. Ferro, J. Alloy. Compd. 215, 181 (1994).10.1016/0925-8388(94)90838-9 ↗
4. S. Katsuyama, M. Suzuki, and T. Tanaka, J. Alloy. Compd. 513, 189 (2012).10.1016/j.jallcom.2011.10.017 ↗
5. T. He, T.G. Calvarese, J.Z. Chen, H.D. Rosenfeld, R.J. Small, J.J. Krajewski, and M.A. Subramanian, 24th International Conference on Thermoelectrics (ICT, 2005), p. 437.
6. G.J. Lehr and D.T. Morelli, Intermetallics 32, 225 (2013).10.1016/j.intermet.2012.08.014 ↗
7. G.J. Lehr and D.T. Morelli, J. Electron. Mater. 42, 1697 (2013).10.1007/s11664-012-2401-2 ↗
8. Y. Chen, B. He, T.J. Zhu, and X.B. Zhao, J. Phys. D Appl. Phys. 45, 1 (2012).
9. J.Q. Li, L.F. Li, S.H. Song, F.S. Liu, and W.Q. Ao, J. Alloy. Compd. 565, 144 (2013).10.1016/j.jallcom.2013.02.149 ↗
10. Y. Gelbstein, B. Dado, O. Ben-Yehuda, Y. Sadia, Z. Dashevsky, and M.P. Dariel, J. Electron. Mater. 39, 2049 (2010).10.1007/s11664-009-1012-z ↗
11. A. Palenzona, J. Less-Common Met. 29, 289 (1972).10.1016/0022-5088(72)90116-6 ↗