Superconductivity of YBCO Thick Films Prepared by Spark Plasma Sintering
Source abstract
Abstract
YBa2Cu3Ox (YBCO) superconducting thick films have been fabricated on Cu substrates, using a simple screen-printing method from Cu-free powders (Y2O3 and BaCO3). However, such films have poor superconducting properties such as critical current density (Jc) due to the low film density. In this work, we investigate the effect of uniaxial c-axis pressure on the superconducting properties of these YBCO films using a spark plasma sintering (SPS) technique. The film screen-printed on Cu substrates was heat-treated at 850°C for 5 min in vacuum varying the pressure (15, 30, and 45 MPa). To form a superconducting YBCO phase, the film was reheat-treated at 930°C for 30 s in air followed by oxygen annealing at 450°C for 1 h. For heat-treatments performed under pressure, lower film porosity was obtained, and a higher crack density was also observed compared to films prepared without pressure. The densification of the YBCO thick films using the SPS technique was very effective in improving the superconducting properties of the films.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Physics of Superconductivity and Magnetism · Advanced ceramic materials synthesis · Diamond and Carbon-based Materials Research
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (14)
Show source-provided references
1. Y. Matsuoka, E. Ban, H. Ogawa, J. Alloy. Comp. 190, L39 (1993)10.1016/0925-8388(93)90387-3 ↗
2. J. Joo, J.P. Singh, T. Warzynski, A. Grow, R.B. Poeppel, Appl. Supercond. 2, 401 (1994)10.1016/0964-1807(94)90087-6 ↗
3. B. Ravi Sankar, K.A. Padmanabhan, J. Mater. Sci. Lett. 14, 1777 (1995)10.1007/BF00271005 ↗
4. B.R. Hickey, L.M. Dezaneti, D.K. Ross, I.A. Rusakova, J.K. Meen, D. Elthon, Physica C. 341, 437 (2000)10.1016/S0921-4534(00)00531-1 ↗
5. S.I. Cha, K.T. Kim, K.H. Lee, C.B. Mo, S.H. Hong, Scripta Mater. 53, 793 (2005)10.1016/j.scriptamat.2005.06.011 ↗
6. P. Angerer, L.G. Yu, K.A. Khor, G. Korb, I. Zalite, J. Euro. Ceram. Soc. 25, 1919 (2005)10.1016/j.jeurceramsoc.2004.06.008 ↗
7. N. Tamari, I. Kondoh, T. Tanaka, M. Kawahara, M. Tokita, Y. Makino, S. Miyake, J. Jpn. Soc. Powder Powder Metallur. 46, 816 (1999)10.2497/jjspm.46.816 ↗
8. D.S. Perera, M. Tokita, S. Moricca, J. Euro. Ceram. Soc. 18, 401 (1998)10.1016/S0955-2219(97)00139-8 ↗
9. M. Omori, Mater. Sci. Eng. A287, 183 (2000)10.1016/S0921-5093(00)00773-5 ↗
10. Y. Kim, S. Kim, Y.-A. Jeon, Y. Kim, H. Paik, Y. Kim, Y.-H. Han, N.-H. Jeong, S.-C. Han, T.-H. Sung, J.-I. Hong, K. No, J. Electroceram. 17, 1063 (2007)10.1007/s10832-006-7988-3 ↗
11. J. Langhorn, P.J. McGinn, Physica C. 312, 169 (1999)10.1016/S0921-4534(98)00643-1 ↗
12. J.K. Yoon, J.K. Lee, J.Y. Byun, G.H. Kim, Y.H. Paik, J.S. Kim, Surf. Coat. Technol. 160, 29 (2002)10.1016/S0257-8972(02)00379-1 ↗
13. A.H. Lia, M. Ionescua, H.K. Liua, D.L. Shib, X.L. Wanga, X. Pengc, E.W. Collings, Physica C. 426–431, 1408 (2005)
14. H.B. Guo, R. Vaben, D. Stover, Surf. Coat. Technol. 186, 353 (2004)10.1016/j.surfcoat.2004.01.002 ↗