Microstructure, Tensile Mechanical Properties and Electrical Fatigue Mechanism of a Microalloyed Copper Wire
Source abstract
Abstract
In this study, trace quantities of silver, palladium, and gold were added to 5 N pure copper wires to prepare microalloyed copper (MAC) wires. The mechanical properties and electrical fatigue mechanisms of original wires and wire bonding specimens were compared to assess the differences between MAC and Au/Pd-coated copper (CPA) wires. The results indicate that the solid-solution strengthening achieved by the addition of trace alloy elements improved the microhardness and tensile properties of the wires; thus, the overall mechanical properties of the MAC wires were superior to those of a CPA wire. Moreover, after wire bonding, the MAC wires exhibited a higher first bond strength than the CPA wire. In terms of electrical properties, the addition of trace alloying elements increased resistance marginally, which resulted in MAC wires with higher dynamic resistance than the CPA wire in the early stage of electrification. At high currents, CPA wires are affected by Joule heat. The palladium atoms in the coating layer diffuse into the wire matrix, which causes the resistance to increase rapidly and thus results in a decreased fusing current. In a power cycling test, the coefficients of thermal expansion of the coating layers were different from that of the wire; thus, the CPA wire was susceptible to thermal fatigue, which led to its failure. The MAC wires had a higher power cycle life than the CPA wire. Because of their superior mechanical and electrical properties, MAC wires can replace CPA wires in the electronic packaging industry.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Electronic Packaging and Soldering Technologies · 3D IC and TSV technologies · Copper Interconnects and Reliability
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (31)
Show source-provided references
1. G.G. Harman, Wire Bonding in Microelectronics, 3rd ed., (New York: McGraw-Hill, 2010).
2. H.K. Charles, Advanced wire bonding technology: materials, methods, and testing, Materials for Advanced Packaging. ed. D. Lu, and C. Wong (Berlin: Springer, 2017), pp. 131–198.10.1007/978-3-319-45098-8_4 ↗
3. M. Eto, N. Araki, T. Yamada, M. Sugiyama, and S. Fujimoto, Influence of Post-Bonding Heating Process on the Long-term Reliability of Cu/Al Contact. Microelectron Reliab 118, 114058 (2021).10.1016/j.microrel.2021.114058 ↗
4. Y.T. Chiu, T.H. Chiang, Y.F. Chen, P.F. Yang, L. Huang, K.L. Lin, in 64th Electronic Components and Technology Conference (2014), p. 419–424.
5. H. Xu, C. Liu, V.V. Silberschmidtb, S.S. Pramanac, T.J. White, Z. Chen, and V.L. Acoff, Intermetallic Phase Transformations in Au-Al Wire Bonds. Intermetallics 19, 1808–1816 (2011).10.1016/j.intermet.2011.07.003 ↗
6. I. Lum, M. Mayer, and Y. Zhou, Footprint Study of Ultrasonic Wedge-Bonding with Aluminum Wire on Copper Substrate. J. Electron. Mater. 35, 433–442 (2006).10.1007/BF02690530 ↗
7. M.S. Broll, U. Geissler, J. Höfer, S. Schmitz, O. Wittler, and K.D. Lang, Microstructural Evolution of Ultrasonic-Bonded Aluminum Wires. Microelectron Reliab. 55, 961–968 (2015).10.1016/j.microrel.2015.03.002 ↗
8. F.Y. Hung, T.S. Lui, K.M. Chu, and Y.W. Tseng, Aluminium Wires have the Free Air Balls (FABs): Electronic Flame-Off, Fracture Strength, Electrical Properties, and Bonding Characteristics of Nano Zn Film Al–Si Bonding Wires. Metals 7, 152 (2017).10.3390/met7050152 ↗
9. E. Sancaktar, P. Rajput, and A. Khanolkar, Correlation of Silver Migration to the Pull Out Strength of Silver Wire Embedded in an Adhesive Matrix. IEEE Trans. Compon. Packaging Manuf. Technol. 28, 771–780 (2005).10.1109/TCAPT.2005.859752 ↗
10. Y.C. Jang, S. Park, H.D. Kim, Y.C. Ko, K.W. Koo, M.R. Choi, H.G. Kim, N.K. Cho, I.T. Kang, J.H. Yee, S.H. Lim, In IEEE 16th Electronics Packaging Technology Conference (2014), p. 704–708.
11. P. Liu, L. Tong, J. Wang, L. Shi, and H. Tang, Challenges and Developments of Copper Wire Bonding Technology. Microelect Reliab 52, 1092 (2012).10.1016/j.microrel.2011.12.013 ↗
12. P.S. Chauhan, A. Choubey, Z. Zhong, and M.G. Pecht, Copper Wire Bonding (Berlin: Springer, 2014), pp. 39–40.10.1007/978-1-4614-5761-9 ↗
13. C. Lu, in IEEE International Microsystems Packaging Assembly and Circuits Technology Conference (2010), p. 1–4.
14. P. Chauhan, Z.W. Zhong, and M. Pecht, Copper Wire Bonding Concerns and Best Practices. J. Electron. Mater. 42, 2415–2434 (2013).10.1007/s11664-013-2576-1 ↗
15. C.Y. Chang, F.Y. Hung, and T.S. Lui, Mechanical and Electrical Properties of Palladium-Coated Copper Wires with Flash Gold. J. Electron. Mater. 46, 1–8 (2017).10.1007/s11664-017-5355-6 ↗
16. C.S. Lee, T. Tran, D. Boyne, L. Higgins, A. Mawer, in IEEE 64th Electronic Components and Technology Conference (2014), p. 1539–1548.
17. D. Stephan, F.W. Wulff, E. Milke, in 12th Electronics Packaging Technology Conference (2010), p. 343–348.
18. J. Gniewek, J. Pezy, B.G. Baker, and J. O’M. Bockris, The Effect of Noble Metal Additions upon the Corrosion of Copper: An Auger-Spectroscopic Study. J. Electrochem. Soc. 125, 17 (1978).10.1149/1.2131389 ↗
19. J. Li, Y. Li, Z. Wang, H. Bian, Y. Hou, F. Wang, G. Xu, B. Liu, and Y. Liu, Ultrahigh Oxidation Resistance and High Electrical Conductivity in Copper-Silver Powder. Sci. Rep. 6, 1 (2016).10.1038/s41598-016-0001-8 ↗
20. A.B.Y. Lim, W.J. Neo, O. Yauw, B. Chylak, C.L. Gan, and Z. Chen, Evaluation of the Corrosion Performance of Cu–Al Intermetallic Compounds and the Effect of Pd Addition. Microelectron Reliab. 56, 155 (2016).10.1016/j.microrel.2015.10.012 ↗
21. Y. Wu, K.N. Subramanian, S.C. Barton, and A. Lee, Electrochemical Studies of Pd-Doped Cu and Pd-Doped Cu-Al Intermetallics for Understanding Corrosion Behavior in wire-Bonding Packages. Microelect Reliab. 78, 355 (2017).10.1016/j.microrel.2017.09.024 ↗
22. L.N. Ho, H. Nishikawa, N. Natsume, T. Takemoto, K. Miyake, M. Fujita, and K. Ota, Effects of Trace Elements in Copper Fillers on the Electrical Properties of Conductive Adhesives. J. Electron. Mater. 39, 115 (2009).10.1007/s11664-009-0946-5 ↗
23. D.P. Lu, J. Wang, W.J. Zeng, Y. Liu, L. Lu, and B.D. Sun, Study on High-Strength and High-Conductivity Cu–Fe–P Alloys. Mater. Sci. Eng. A 421, 254 (2006).10.1016/j.msea.2006.01.068 ↗
24. P. Żywicki, D.H. Ping, T. Abe, H. Garbacz, Y. Yamabe-Mitarai, and K.J. Kurzydłowski, Effect of Pd Addition on the Microstructure of Ti-30Nb Alloy. Met. Mater. Int. 21, 617 (2015).10.1007/s12540-015-4593-5 ↗
25. W.Y. Zhou, H.Y. Pei, J.Q. Luo, Y.J. Wu, J.L. Chen, F.F. Kang, J.W. Kong, X.Q. Ji, G.X. Yang, and A.H. Yang, Influence of Pd Content on Microstructure and Performance of Au-Coated Ag Alloy Wire. J. Mater. Sci. Mater. Electron. 31, 6241 (2020).10.1007/s10854-020-03178-0 ↗
26. H.W. Hsueh, F.Y. Hung, and T.S. Lui, A study on Electromigration-Inducing Intergranular Fracture of Fine Silver Alloy Wires. Appl. Phys. Lett. 110, 031902 (2017).10.1063/1.4974154 ↗
27. A.Y. Volkov, O.S. Novikova, A.E. Kostina, and B.D. Antonov, Effect of Alloying with Palladium on the Electrical and Mechanical Properties of Copper. Phys. Metals Metallogr. 117, 945 (2016).10.1134/S0031918X16070176 ↗
28. D. Liu, H. Chen, F. Wong, K. Lee, I. Shiu, J. Wu, in IEEE 61st Electronic Components and Technology Conference (2011), p. 1523–1528.
29. F.Y. Hung, Y.T. Wang, L.H. Chen, and T.S. Lui, Recrystallization Effect and Electric Flame-Off Characteristic of Thin Copper Wire. Mater. Trans. 47, 1776 (2006).10.2320/matertrans.47.1776 ↗
30. H. Xu, C. Liu, V.V. Silberschmidt, S.S. Pramana, T.J. White, Z. Chen, and V.L. Acoff, Behavior of Aluminum Oxide, Intermetallics and Voids in Cu-Al Wire Bonds. Acta Mater. 59, 5661 (2011).10.1016/j.actamat.2011.05.041 ↗
31. T.H. Yang, Y.M. Lin, and F.Y. Ouyang, Joule-Heating-Induced Damage in Cu-Al Wedge Bonds Under Current Stressing. J. Electron. Mater. 43, 270–276 (2014).10.1007/s11664-013-2790-x ↗