Fabrication of Ni Metal Mask by Electroforming Process Using Wetting Agents
Source abstract
Abstract
We fabricated a Ni metal mask using the electroforming process, in combination with photolithography, and evaluated the effects of adding wetting agents to the electrolyte on the microstructure and mechanical properties. Photo masking, exposure, and development procedures were used to produce additive patterns on the stainless steel substrate. Subsequently, a textured Ni metal mask (30 μm thickness and 100 μm hole size) was formed on the substrate using the electroforming process. We found that the microstructure and mechanical properties varied considerably with the different combinations of the wetting agents added, i.e., the addition of SF-1, SF-2, or both SF-1 and SF-2. The addition of both wetting agents significantly reduced the grain size, resulting in an improved Vickers’s hardness (638 HV) and a reduced surface roughness (11.39 nm). Moreover, the friction coefficient of the Ni mask was reduced to 0.66. The wear resistance of the Ni mask was comparable to that of a commercial stainless steel mask due to the improved hardness and reduced friction coefficient.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Electrodeposition and Electroless Coatings · Advanced Machining and Optimization Techniques · Corrosion Behavior and Inhibition
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (10)
Show source-provided references
1. E. Davis, W. Harding, R. Schwartz, and J. Corning, IBM J. Res. Dev., 8, 102–104 (1964)10.1147/rd.82.0102 ↗
2. J.H. Lau and Y.H. Pao, Solder Joint Reliability of BGA, CSP, Flip Chip, and Fine Pitch SMT Assemblies (New York: McGraw-Hill, 1997)
3. P. Elenius, J. Leal, J. Ney, D. Stepniak, and S. Yeh, Proceedings of IEEE Electronic Comp. and Tech. Conf., 260–265 (1999)
4. K.P. Wong, K.C. Chan, T.M. Yue, Surface Coat. Technol., 115, 132–139, 199910.1016/S0257-8972(99)00165-6 ↗
5. Chao-Min Cheng, Ren-Haw Chen, Microelectr. Eng. 75, 423–432, 200410.1016/j.mee.2004.07.066 ↗
6. C.S. Lin, P.C. Hsu, L. Chang, C.H. Chen, J. Appl. Electrochem. 31, 925–933, 200110.1023/A:1017970417874 ↗
7. ASTM G132, Standard test method for “pin abrasion testing”
8. F.C. Walsh, M.E. Herron, J. Phys. D, 24, 217–225, 199110.1088/0022-3727/24/2/019 ↗
9. J.O. Bockris and G.A. Razumney, Fundamental Aspects of Electrocrystalisation (New York: Plenum, 1967)10.1007/978-1-4684-0697-9 ↗
10. Kollia C., Loizos Z., Spyrellis N., Electrodeposits Surface Coat. Technol., 45, 155–160, 199110.1016/0257-8972(91)90218-L ↗