Liquid-Phase Separation in the Interdendritic Region After Growth of Primary β-Sn in Undercooled Sn-2.8Ag-0.3Cu Melt
Source abstract
Abstract
An unusual microstructure consisting of both Sn-Ag3Sn and Sn-Cu6Sn5 binary eutectic structures is observed in actual solder balls. In this study, the solidification process of the Sn-Ag3Sn binary eutectic structure after the growth of primary b-Sn in an undercooled Sn-2.8Ag-0.3Cu alloy was investigated by using thermal analysis and interruption tests to understand the formation of the unusual microstructure. First, fine Ag-enriched liquid zones formed around b-Sn after the growth of primary b-Sn. The Ag-enriched zones then gradually enlarged with the accumulation of Ag from the remnant liquid with a decrease in temperature. This indicated that the liquid-phase separation occurred in the remnant liquid after the nucleation of b-Sn. Eventually, when the temperature of the specimen decreased to approximately the binary eutectic temperature, eutectic Ag3Sn nucleated in the Ag-enriched zones. From interruption tests, we determined the precursor of the Sn-Ag3Sn binary eutectic structure before the beginning of Sn-Ag3Sn binary eutectic solidification. This finding corresponds to the precursor of the Sn-Cu6Sn5 binary eutectic structure observed in the Sn-1.0Ag-0.5Cu alloy.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Electronic Packaging and Soldering Technologies · Aluminum Alloy Microstructure Properties · Solidification and crystal growth phenomena
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (14)
Show source-provided references
1. T. Nishimura, Materia Jpn. 43, 651 (2004).10.2320/materia.43.651 ↗
2. A. Nishimura, J. Jpn. Inst. Electron. Packag. 11, 348 (2008).10.5104/jiep.11.348 ↗
3. W.M. Rumball and V. Kondic, The Solidification of Metals (London: The Iron and Steel Institute, 1967), p. 149.
4. W. Kurz and D.J. Fisher, Fundamentals of Solidification (Switzerland: Trans Tech, 1984), p. 99.
5. Y. Miyauchi, H. Esaka, M. Tamura, and K. Shinozuka, J. Jpn. Inst. Met. 72, 804 (2008).10.2320/jinstmet.72.804 ↗
6. Y. Miyauchi, H. Esaka, and K. Shinozuka, J. Jpn. Inst. Met. 73, 732 (2009).10.2320/jinstmet.73.732 ↗
7. Y. Takamatsu, H. Esaka, and K. Shinozuka, J. Jpn. Inst. Met. 74, 101 (2010).10.2320/jinstmet.74.101 ↗
8. Y. Takamatsu, H. Esaka, and K. Shinozuka, Mater. Trans. 52, 189 (2011).10.2320/matertrans.M2010325 ↗
9. Y. Takamatsu, H. Esaka, and K. Shinozuka, J. Jpn. Inst. Met. 74, 551 (2010).10.2320/jinstmet.74.551 ↗
10. Y. Takamatsu, H. Esaka, and K. Shinozuka, Collected Abstracts of the 2011 Spring Meeting of the Japan Inst. Metals(2011), p. 314.
11. L. Snugovsky, P. Snugovsky, D.D. Perovic, T. Sack, and J.W. Rutter, Mater. Sci. Technol. 21, 53 (2005).10.1179/174328405X13994 ↗
12. Y. Takamatsu, H. Esaka, and K. Shinozuka, Mater. Trans. 75, 341 (2011).
13. K. Hashimoto, Bull. Iron Steel Inst. Jpn. 11, 715 (2006).
14. http://www.metallurgy.nist.gov/phase/solder/solder.html