Effect of Processing of HIPERCO® 50 Alloy Laminates on Their Magnetic Properties
Source abstract
Abstract
Fe-Co-based soft-magnetic materials form an important class of high-induction alloys that are widely used in energy conversion applications in the aerospace industry. In this work, the effect of processing—cut method [stamping and wire-electrical discharge machining (EDM)] and annealing (cut unannealed, cut followed by annealing, and annealing followed by cut)—on the magnetic properties of the HIPERCO® 50 Alloy laminates was investigated. A cold-rolled ∼0.006-in (∼150-μm)-thick strip of HIPERCO® 50 Alloy was cut into ring laminations and final-annealed in dry hydrogen. Scanning electron microscopy (SEM) and x-ray diffraction analysis indicated the presence of extraneous Cu on the cut edge of the wire-EDM cut ring laminates, along with the expected Fe-Co phase for HIPERCO® 50 alloy. SEM micrographs of the cut edge showed the typical sheared surface and irregular surface for stamped and wire-EDM cut ring laminates respectively. The rings that were stamped followed by annealing (STfA) showed superior direct current (DC) and alternating current (AC) magnetic properties. The presence of Cu (diamagnetic) in wire-EDM cut rings adversely affects induction (B) and core loss (P T), compared to the stamped rings for corresponding annealing conditions. The difference in the DC magnetic properties between the ring laminates STfA and annealed followed by stamping (AfST) was significantly large compared to that between the ring laminates that were wire-EDM cut followed by annealing (EDfA) and annealing followed by wire-EDM (AfED). This suggests that, for certain applications where the differences in DC magnetic properties between EDfA and AfED are acceptable, the AfED rings may be put to application/service after the wire-EDM cut operation, i.e. wire-EDM may be performed after ‘final-annealing’. However, the AC properties between EDfA and AfED rings were significantly different, hence for AC applications, the ‘final annealing’, post-cutting, is critical irrespective of the cut method. Wire-EDM incorporates extraneous Cu on the cut edge of the HIPERCO® 50 Alloy laminates and deteriorates its magnetic properties. An intermediate grinding step after wire-EDM, for the removal of Cu, could probably improve the magnetic properties. However, if the extraneous Cu and the accompanied deterioration in magnetic properties is acceptable for certain applications, then the wire-EDM provides the flexibility to have the ‘final-annealing’ of HIPERCO® 50 Alloy laminates either before or after wire-EDM.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced Machining and Optimization Techniques · Electrodeposition and Electroless Coatings · Corrosion Behavior and Inhibition
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (26)
Show source-provided references
1. R.M. Bozorth, Ferromagnetism, 1st ed. (New York: IEEE Press, 1978), pp. 190–209.
2. C.W. Chen, J. Appl. Phys. 32, 348 (1961).10.1063/1.2000465 ↗
3. A.T. English, Trans. Metall. Soc. AIME 236, 14 (1966).
4. D.W. Clegg and R.A. Buckley, Met. Sci. J. 7, 48 (1973).10.1179/030634573790445541 ↗
5. A.W. Smith and R.D. Rawlings, Phys. Status Solidi A 34, 117 (1976).10.1002/pssa.2210340109 ↗
6. M. Rajkovic and R.A. Buckley, Met. Sci. 15, 21 (1981).10.1179/msc.1981.15.1.21 ↗
7. A.I.C. Persiano and R.D. Rawlings, Status Solidi A 103, 574 (1987).
8. CARPENTER Technical Data Sheet—HIPERCO® 50 Alloy, Copyright 2015 CRS Holdings Inc. (a subsidiary of Carpenter Technology Corporation) (1990), http://cartech.ides. com/datasheet.aspx?i=103&e=200&c=TechArt .
9. Q. Zhu, L. Li, M.S. Masteller, and G.J. Del Corso, Appl. Phys. Lett. 69, 25 (1996).10.1063/1.118106 ↗
10. L. Li, J. Appl. Phys. 79, 4578 (1996).10.1063/1.361732 ↗
11. D. Shin, J. Degauque, C. Lebourg, and B. Astie, Journal De Physique IV Colloque C8, C8-545 (1996).
12. Z. Turgut, M.Q. Huang, K. Gallagher, M.E. McHenry, and S.A. Majetich, J. Appl. Phys. 81, 8 (1997).10.1063/1.364887 ↗
13. Y. Ustinovshikov, B. Pushkarev, I. Shabanova, and A. Ulinova, Interface Sci. 10, 311 (2002).10.1023/A:1020837814708 ↗
14. X.M. Cheng, X.K. Zhang, D.Z. Zhang, S.H. Lee, A. Duckham, T.P. Weihs, R.C. Cammarata, J.Q. Xiao, and C.L. Chein, J. Appl. Phys. 93, 7121 (2003).10.1063/1.1557308 ↗
15. B.D. Cullity and C.D. Graham, Introduction to Magnetic Materials, 2nd ed. (Piscataway: IEEE Press, Wiley, 2009), p. 466.
16. E.C. Jameson, Electrical Discharge Machining (Society of Manufacturing Engineers, Dearborn, MI, 2001), p. 12.
17. K.H. Ho and S.T. Newman, Int. J. Mach. Tools Manuf. 43, 1287 (2003).10.1016/S0890-6955(03)00162-7 ↗
18. K.H. Ho, Int. J. Mach. Tools Manuf. 44, 1247 (2004).
19. F. Alpeter and P. Perez, J. Mater. Process. Technol. 149, 147 (2004).10.1016/j.jmatprotec.2003.10.033 ↗
20. K.P. Rajurkar, M.M. Sundaram, and A.P. Malshe, The Seventeenth CIRP Conference on Electro Physical and Chemical Machining (ISEM), Procedia CIRP (2013), vol. 6, p. 13.
21. ASTM A697/A697M Standard test method for alternating current magnetic properties of laminated core specimens using voltmeter-ammeter-wattmeter method, ASTM (2004), http://compass.astm.org/Standards/HISTORICAL/A697A69 7M-03.htm .
22. ASTM A773/A773M Standard test for direct current magnetic properties of low coercivity magnetic materials using hysteresisgraphs, ASTM (2009), http://compass.astm.org/ EDIT/html_annot.cgi?A773+14 .
23. ASTM A927/A927M Standard test method for alternating current magnetic properties of toroidal core specimens using voltmeter-ammeter-wattmeter method, ASTM (2004), http://compass.astm.org/Standards/HISTORICAL/A927A92 7M-04.htm .
24. J.F. Liu and Y.B. Guo, 43rd Proceedings of the North American Manufacturing Research Institution of SME, Procedia Manufacturing (2015), vol. XX, p. 1–11.
25. Y. Sakaki and S. Imagi, IEEE Trans. Magn. 17, 1478 (1981).10.1109/TMAG.1981.1061229 ↗
26. Y. Chen and P. Pillay, Proceedings of IEEE 37th IAS Annual Meeting (Pittsburg, PA, 2002), p. 759.