Interfacial Reaction and Wetting Behavior Between Pt and Molten Solder
Source abstract
Abstract
Platinum does not oxidize easily, and has slow reaction rates with Sn-based solders. Due to these two positive attributes, a single platinum layer has the potential to replace both the oxidation protection layer and the diffusion barrier layer in the underbump metallurgy of flip-chip devices. To evaluate this potential further, the dissolution rate and the wetting properties of Pt were investigated in this study. It was found that Pt did have a dissolution rate less than half that of Ni, currently the most popular barrier layer material. The wetting properties of Pt were not as good as those of Ni but were nevertheless still acceptable for industrial applications. In short, as far as the dissolution and the wetting characteristics are concerned, Pt is an effective top surface layer for use in underbump metallurgy.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Electronic Packaging and Soldering Technologies · 3D IC and TSV technologies · Silicon and Solar Cell Technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (24)
Show source-provided references
1. W.G. Bader. Weld. J. 48, 551 (1969).
2. B. Meagher, D. Schwarcz, M. Ohring. J. Mater. Sci. 31, 5479 (1996) doi: 10.1007/BF01159320 .10.1007/BF01159320 ↗
3. J.F. Kuhmann, C·H. Chiang, P. Harde, F. Reier, W. Oesterle, I. Urban, and A. Klein, Mater. Sci. Eng. A 242, 22 (1998) doi: 10.1016/S0921-5093(97)00536-4 .10.1016/S0921-5093(97)00536-4 ↗
4. B. Wiens. Z. Metallk. 91, 863 (2000).
5. M. Klein, B. Wiens, M. Hutter, H. Oppermann, R. Aschenbrenner, and H. Reichl, Proc. 50th Electronic Components and Technology Conf. (2000), pp. 40–45.
6. T.H. Kim, Y.H. Kim. JOM 56, 45 (2004) doi: 10.1007/s11837-004-0111-9 .10.1007/s11837-004-0111-9 ↗
7. S.J. Wang, C.Y. Liu. Acta Mater. 55, 3327 (2007) doi: 10.1016/j.actamat.2007.01.031 .10.1016/j.actamat.2007.01.031 ↗
8. S. Bader, W. Gust, H. Hieber. Acta Mater. 43, 329 (1995).
9. D. Gur, M. Bamberger. Acta Mater. 46, 4917 (1998) doi: 10.1016/S1359-6454(98)00192-X .10.1016/S1359-6454(98)00192-X ↗
10. H·K. Kim, H·K. Liou, K·N. Tu. Appl. Phys. Lett. 66, 2337 (1995) doi: 10.1063/1.113975 .10.1063/1.113975 ↗
11. S·K. Kang. Scr. Metall. 14, 421 (1980) doi: 10.1016/0036-9748(80)90338-5 .10.1016/0036-9748(80)90338-5 ↗
12. C.M. Liu (Master’s thesis, National Central University, Taiwan, 2000).
13. W.J. Zhu, J. Wang, H·S. Liu, Z.P. Jin, W·P. Gong. Mater. Sci. Eng. A 456, 109 (2007) doi: 10.1016/j.msea.2006.11.117 .10.1016/j.msea.2006.11.117 ↗
14. C.E. Ho, Y.M. Chen, C.R. Kao. J. Electron. Mater. 28, 1231 (1999) doi: 10.1007/s11664-999-0162-3 .10.1007/s11664-999-0162-3 ↗
15. C.E. Ho, R. Zheng, G.L. Luo, A.H. Lin, C.R. Kao. J. Electron. Mater. 29, 1175 (2000) doi: 10.1007/s11664-000-0010-y .10.1007/s11664-000-0010-y ↗
16. C.E. Ho, S.Y. Tsai, C.R. Kao. IEEE Trans. Adv. Packag. 24, 493 (2001) doi: 10.1109/6040.982835 .10.1109/6040.982835 ↗
17. C·W. Chang, C.E. Ho, S·C. Yang, C.R. Kao. J. Electron. Mater. 35, 1948 (2006) doi: 10.1007/s11664-006-0298-3 .10.1007/s11664-006-0298-3 ↗
18. C·W. Chang, Q.P. Lee, C.E. Ho, C.R. Kao. J. Electron. Mater. 35, 366 (2006) doi: 10.1007/BF02692458 .10.1007/BF02692458 ↗
19. J.Y. Tsai, C·W. Chang, C.E. Ho, Y.L. Lin, C.R. Kao. J. Electron. Mater. 35, 65 (2006) doi: 10.1007/s11664-006-0185-y .10.1007/s11664-006-0185-y ↗
20. J.Y. Tsai, C·W. Chang, Y.C. Shieh, Y.C. Hu, C.R. Kao. J. Electron. Mater. 34, 182 (2005) doi: 10.1007/s11664-005-0231-1 .10.1007/s11664-005-0231-1 ↗
21. Y. Wang, K·N. Tu. Appl. Phys. Lett. 67, 1069 (1995) doi: 10.1063/1.114467 .10.1063/1.114467 ↗
22. H. Baker, ASM Handbook, Vol. 3, Alloy Phase Diagrams (Metals Park, OH: ASM Intl., 1992), p. 2.347.
23. J.I. Lee, S·W. Chen, H.Y. Chang, C.M. Chen. J. Electron. Mater. 32, 117 (2003) doi: 10.1007/s11664-003-0181-4 .10.1007/s11664-003-0181-4 ↗
24. H.Y. Chang, S·W. Chen, D.S·H. Wong, H·F. Hsu. J. Mater. Res. 18, 1420 (2003) doi: 10.1557/JMR.2003.0195 .10.1557/JMR.2003.0195 ↗