journal article·2009-02

Temperature-Dependent Phase Segregation in Cu/42Sn-58Bi/Cu Reaction Couples under High Current Density

Guangchen Xu, Hongwen He, Fu Guo

Journal of Electronic Materials· Volume 38· Issue 2
Publisher page

Abstract

The effects of current stressing at 10 4 A/cm 2 on Cu/42Sn-58Bi/Cu reaction couples with a one-dimensional structure at 23°C, 50°C, and 114°C were investigated. The microstructural evolution during electromigration was examined using scanning electron microscopy. The temperature dependence of the coarsening of the Bi-rich phase, the dominant migrating entity, and hillock/whisker formation in eutectic Sn-Bi were investigated under high current density. During current stressing at 10 4 A/cm 2 , the average size of the Bi-rich phase remained the same at 23°C, increased at 50°C, and shrank at 140°C. Bi accumulated near the anode side at both high (50°C, 140°C) and low temperature (23°C). At high temperatures, both Sn and Bi diffused towards the anode side, but Bi moved ahead of Sn during current stressing. However, at low temperatures, Sn reversed its direction of migration to the cathode side. Pure Bi hillocks/whiskers and a mixed structure of Sn and Bi hillocks were extruded as a consequence of compressive stress from electromigration-induced mass flow towards the anode side.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Electronic Packaging and Soldering Technologies · Copper Interconnects and Reliability · Electrodeposition and Electroless Coatings

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (19)

Show source-provided references
1. H.B. Huntington, A.R. Grone. J. Phys. Chem. Solids 20, 76 (1961) doi: 10.1016/0022-3697(61)90138-X10.1016/0022-3697(61)90138-X ↗
2. I.A. Blech. J. Appl. Phys. 47, 1203 (1976) doi: 10.1063/1.32284210.1063/1.322842 ↗
3. S.W. Chen, C.M. Chen, W.C. Liu, J. Electron. Mater. 27, 1193 (1998) doi: 10.1007/s11664-998-0068-510.1007/s11664-998-0068-5 ↗
4. A. Lee, W. Liu, C.E. Ho, K.N. Subramanian, J. Appl. Phys. 102, 053507 (2007) doi: 10.1063/1.277712210.1063/1.2777122 ↗
5. S. Brandenburg and S. Yeh, Proceedings of Surface Mount International Conference and Exhibition, SMI98 (San Jose, CA, Aug. 1998), p. 337.
6. T.Y. Lee, K.N. Tu, S.M. Kuo, D.R. Frear, J. Appl. Phys. 89, 3189 (2001) doi: 10.1063/1.134202310.1063/1.1342023 ↗
7. C.Y. Liu, C. Chen, C.N. Liao, K.N. Tu, Appl. Phys. Lett. 75, 58 (1999) doi: 10.1063/1.12427610.1063/1.124276 ↗
8. C. Chen, S.W. Liang, J. Mater. Sci. Mater. Electron. 18, 259 (2007) doi: 10.1007/s10854-006-9020-810.1007/s10854-006-9020-8 ↗
9. C.M. Chen, C.C. Huang, J. Electron. Mater. 36, 760 (2007) doi: 10.1007/s11664-007-0150-410.1007/s11664-007-0150-4 ↗
10. Q.L. Yang, J.K. Shang, J. Electron. Mater. 34, 1363 (2005) doi: 10.1007/s11664-005-0191-510.1007/s11664-005-0191-5 ↗
11. C.M. Chen, C.C. Huang. J. Mater. Res. 23, 1051 (2008) doi: 10.1557/jmr.2008.012810.1557/jmr.2008.0128 ↗
12. L.T. Chen, C.M. Chen, J. Mater. Res. 21, 962–969 (2006) doi: 10.1557/jmr.2006.011310.1557/jmr.2006.0113 ↗
13. C.E. Ho, A. Lee, K.N. Subramanian, J. Mater. Sci. Mater. Electron. 18, 569 (2007) doi: 10.1007/s10854-007-9263-z10.1007/s10854-007-9263-z ↗
14. B. Tao, Y. Wu, H. Ding, Y.L. Xiong, Microelectron. Reliab. 46, 864 (2006) doi: 10.1016/j.microrel.2005.04.01310.1016/j.microrel.2005.04.013 ↗
15. J.G. Lee, F. Guo F, K. N. Subramanian, and J. P. Lucas, Solder. Surf. Mt. Technol. 14, 11 (2002) doi: 10.1108/0954091021042777210.1108/09540910210427772 ↗
16. C.E. Ho, A. Lee, K.N. Subramanian, W. Liu, Appl. Phys. Lett. 91, 021906 (2007) doi: 10.1063/1.275629210.1063/1.2756292 ↗
17. K.N. Tu, Solder Joint Technology: Materials, Properties, and Reliability (Springer, 2007).
18. S.H. Liu, C. Chen, P.C. Liu, T. Chou, J. Appl. Phys. 95, 7742 (2004) doi: 10.1063/1.171201910.1063/1.1712019 ↗
19. M. Shimoji (1977) Liquid Metals: An Introduction to the physics and Chemistry of Metals in the Liquid State. Academic, London