Abstract
We chose Sn−2.8Ag−20In and Sn−10Bi−10In (numbers are in weight percentages unless specified otherwise) as Pb-free solder materials for intermediate-step soldering. We then investigated how the two solders reacted with the under bump metallurgy (UBM) of Au/Ni (Au: 1.5 μm and Ni: 3 μm) at 210°C, 220°C, 230°C, and 240°C for up to 4 min. All, of the Au UBM was dissolved into the solder matrix as soon as the interfacial reaction started. The reaction formed Au(In, Sn)2 in the case of SnAgIn, and it formed Au(Sn, In)4 and Au(In, Sn)2 in the case of SnBiIn. The formation mechanism of the intermetallic phases is explained thermodynamically. The exposed Ni layer reacted with the solder and formed Ni28Sn55In17 in case of SnAgIn, and formed Ni3(Sn, In)4 in case of SnBiIn, at the solder joint interface. Under the same soldering conditions, the Ni3(Sn,In)4 layer in the SnBiIn/UBM is thicker than the Ni28Sn55In17 layer in the SnAgIn/UBM. Because of the thicker intermetallic compound layer, the SnBiIn solder joint has weaker shear strength than the SnAgIn solder joint.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Electronic Packaging and Soldering Technologies · Intermetallics and Advanced Alloy Properties · Advanced Welding Techniques Analysis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (21)
Show source-provided references
1. C.A. Harper, Electronic Packaging and Interconnection Handbook, 3rd ed. (New York: McGraw-Hill, 2000), pp. 7.77–7.91.
2. R.R. Tummala, E.J. Rymaszewski, and A.G. Klopfenstein, Microelectronics Packaging Handbook Part 2: Semiconductor Packaging, 2nd ed. (New York: Chapman & Hall, 1997), pp. 894–907.
3. K. Gilleo, Area Array Packaging Materials (New York: McGraw-Hill, 2002), pp. 25–39.
4. C. Luo and L. Lin, Sens. Actuators, A: Phys. 97–98, 398 (2002).10.1016/S0924-4247(01)00849-4 ↗
5. M. Chiao and L. Lin, Proc. SPIE: Smart Electronics, MEMS, and Nanotechnology, ed. V.K. Varadan (San Diego, CA, 2002), pp. 274–278.10.1117/12.475039 ↗
6. K.S. Dogra, Proc. 4th Annual Int. Electronics Packaging Conf. (IEPS) (Baltimore, MD, 1984), pp. 631–636.
7. H.H. Manko, Solders and Soldering; Materials, Design, Production and Analysis for Reliable Bonding, 3rd ed. (New York: McGraw-Hill, 1992), pp. 1–19.
8. S.-M. Hong, J.-Y. Park, C.-S. Kang, and J.-P. Jung, IEEE Trans. Compon. Packag. Manuf. Technol. 26, 255 (2003).10.1109/TADVP.2002.807622 ↗
9. M.G. Cho, K.W. Paik, H.M. Lee, S.W. Booh, and T.-G. Kim, J. Electron. Mater. 35, 35 (2006).10.1007/s11664-006-0181-2 ↗
10. B. Sundman, B. Jansson, and J.-O. Andersson, CALPHAD 9, 153 (1985).10.1016/0364-5916(85)90021-5 ↗
11. P.G. Kim and K.N. Tu, J. Appl. Phys. 80, 3822 (1996).10.1063/1.363336 ↗
12. L.C. Shiau, C.E. Ho, and C.R. Kao, Soldering. Surf. Mount. Technol. 14, 25 (2002).10.1108/09540910210444692 ↗
13. H. Nowotny and K. Schubert, Z. Metallkd., 37, 23 (1946).
14. S. Kim and D.C. Johnson, J. Alloys Compd. 392, 105 (2005).10.1016/j.jallcom.2004.09.030 ↗
15. H.-M. Wu, F.-C. Wu, and T.-H. Chuang, J. Electron. Mater. 34, 1385 (2005).10.1007/s11664-005-0195-1 ↗
16. T.H. Chuang, K.W. Huang, and W.H. Lin, J. Electron. Mater. 33, 374 (2004).10.1007/s11664-004-0146-2 ↗
17. H.S. Liu, Y. Cui, K. Ishida, and Z.P. Jin, CALPHAD 27, 27 (2003).10.1016/S0364-5916(03)00028-2 ↗
18. I. Ansara and J.-P. Nabot, CALPHAD, 16, 13 (1992).10.1016/0364-5916(92)90032-S ↗
19. H.S. Liu, C.L. Liu, K. Ishida, and Z.P. Jin, J. Electron. Mater. 32, 1290 (2003).10.1007/s11664-003-0025-2 ↗
20. B.-J. Lee, C.-S. Oh, and J.-H. Shim, J. Electron. Mater. 25, 983 (1996).10.1007/BF02666734 ↗
21. D.R. Frear, F.M. Hosking, and P.T. Vianco, Proc. Materials Developments in Microelectronic Packaging Conf. (Materials Park, OH: ASM International, 1991), pp. 229–240.