journal article·2007-07

Failure Mechanisms and Crack Propagation Paths in Thermally Aged Pb-Free Solder Interconnects

Eduardo Franco De Monlevade, Weiqun Peng

Journal of Electronic Materials· Volume 36· Issue 7
Publisher page

Abstract

Studies were conducted on Pb-free solder interconnects after aging for up to 1,000 h at temperatures of up to 150°C and submitting to drop testing. Cracks were shown to propagate along interphase boundaries (bulk solder/Cu6Sn5, Cu6Sn5/Cu3Sn, Cu3Sn/Cu, and bulk solder/Ag3Sn) and along the bulk solder. Intergranular propagation in the solder was rarely observed, although cross sectioning showed evidence of that particular path. There is a transition in preferred crack propagation with aging time and temperature, from the intermetallic layer to the bulk solder. Sulfur was found in the fracture surfaces and may be a weakening agent in these solders.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Electronic Packaging and Soldering Technologies · 3D IC and TSV technologies · Intermetallics and Advanced Alloy Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (21)

Show source-provided references
1. K.N. Subramanian, J.G. Lee, JOM 55, 26 (2003)10.1007/s11837-003-0242-4 ↗
2. K.K. Hong, J.Y. Huh, J. Electron. Mater. 35, 56 (2006)10.1007/s11664-006-0184-z ↗
3. H.-T. Lee, M.-H. Chen, Mater. Sci. Eng. A 333, 24 (2002)10.1016/S0921-5093(01)01820-2 ↗
4. K.Y. Lee, M. Li, J. Electron. Mater. 32, 906 (2003)10.1007/s11664-003-0208-x ↗
5. W.H. Müller, Microelectron. Reliability 44, 1901 (2004)10.1016/j.microrel.2004.04.020 ↗
6. D.Q. Yu, C.M.L. Wu, C.M.T. Law, J.K.L. Lai, J. Alloys Compd. 392, 192 (2005)10.1016/j.jallcom.2004.09.023 ↗
7. D.Q. Yu, L. Wang, C.M.L. Wu, C.M.T. Law, J. Alloys Compd. 389, 153 (2005)10.1016/j.jallcom.2004.08.017 ↗
8. D. Cavasin, R. Zheng, TMS Lett. 1, 163 (2004)
9. A. Sharif, M.N. Islam, Y.C. Chan, Mater. Sci. Eng. B 113, 184 (2004)10.1016/S0921-5107(04)00406-4 ↗
10. W.C. Luo, C.E. Ho, J.Y. Tsai, Y.L. Lin, C.R. Kao, Mater. Sci. Eng. A 396, 385 (2005)10.1016/j.msea.2005.02.008 ↗
11. L.L. Duan, D.Q. Yu, S.Q. Han, H.T. Ma, L. Wang, J. Alloys Compd. 381, 202 (2004)10.1016/j.jallcom.2004.03.124 ↗
12. K.S. Kim, S.H. Huh, K. Suganuma, J. Alloys Compd. 352, 226 (2003)10.1016/S0925-8388(02)01166-0 ↗
13. D. Li, C. Liu, P.P. Conway, Mater. Sci. Eng. A 391, 95 (2005)10.1016/j.msea.2004.10.007 ↗
14. T.T. Mattila, J.K. Kivilahti, J. Electron. Mater. 34, 969 (2005)10.1007/s11664-005-0084-7 ↗
15. T.T. Mattila, J.K. Kivilahti, J. Electron. Mater. 35, 250 (2005)10.1007/BF02692443 ↗
16. Y.-S. Lai, P.-F. Yang, C.-L. Yeh, Microelectron. Reliability 46, 645 (2006)10.1016/j.microrel.2005.07.005 ↗
17. JEDEC Solid State Technology Association, Standard JESD22B104A, Mechanical Shock, Sept. 1990
18. JEDEC Solid State Technology Association, Standard JESD22B111, Board Level Drop Test Method of Components for Handheld Electronic Products, July 2003
19. H. Fredriksson, M. Hillert, J. Iron Steel Inst. 209, 109 (1971)
20. K.-W. Moon, W.J. Boettinger, U.R. Kattner, F.S. Biancanello, C.A. Handwerker, J. Electron. Mater. 29, 1122 (2000)10.1007/s11664-000-0003-x ↗
21. S.O. Dunford, A. Primavera, and M. Meilunas (Proc. IPC 2002, New Orleans, LA, Nov. 2–3, 2002)