Abstract
The reactions between the eutectic PbSn solder and the Au/Ni/Cu tri-layer metallization in advanced microelectronic packages were studied. In this investigation, reflowed packages were subjected to aging at 160°C for times as long as 4000 h. Immediately after the reflow, all the Au had left the Au/Ni/Cu metallization, forming many (Au1−xNix)Sn4 particles distributed throughout the whole solderjoint. In addition, there was a thin layer of Ni3Sn4 (1.4 μm) at the interface. After 500 h of aging, most of the (Au1−xNix)Sn4 particles regrouped at the interface as a continuous (Au0.45Ni0.55)Sn4, layer over the Ni3Sn4 layer. After 2500 h of aging, nearly all the Ni layer had been consumed. A 15 μm layer of (Au0.45Ni0.55) Sn4 and a 20 μm Ni3Sn4 were found over the remaining Ni. At 3000 h, the Cu had started to react with both Ni3Sn4 and (Au1−xNix)Sn4, forming a layer of (Cu1−p−pAupNiq)6Sn5, a layer of (Cu1−r−sAu1Nis)6Sn5, and a layer of Cu3Sn over the Cu layer. A small amount of Cu (2.7–5.7 at.%) was found to dissolve in this Ni3Sn4, forming a ternary compound (Ni1−yCuy)3Sn4. It was revealed that Au diffused up-hill during the reaction. After aging for 4000 h, all the (Au1−xNix)Sn4 had disappeared and Au atoms had diffused into the (Cu1−p−qAupNiq)6Sn5 and (Cu1−r−sAurNis)6Sn5 phases. The practical implications for the above findings were pointed out in this paper.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Electronic Packaging and Soldering Technologies · 3D IC and TSV technologies · Aluminum Alloys Composites Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (10)
Show source-provided references
1. C. E. Ho, R. Zheng, G. L. Luo, A.H. Lin, and C.R. Kao, J. Electron. Mater. 29, 1175 (2000).10.1007/s11664-000-0010-y ↗
2. C. E. Ho, Y. M. Chen, and C. R. Kao, J. Electron. Mater. 28, 1231 (1999).10.1007/s11664-999-0162-3 ↗
3. S. Anhöck, H. Oppermann, C. Kallmayer, R. Aschenbrenner, L. Thomas, and H. Reichl, 1998 IEEE/CPMT Berlin Intl Manufacturing Tech. Symp. Proc. Piscataway, NJ: IEEE, 1998), p. 156.
4. K. Banerji and R. F. Darveaux, Microstructures and Mechanical Properties of Aging Materials, ed. P. K. Liaw et al. (Warrendale, PA: TMS, 1993), p. 431.
5. R. F. Darveaux, K. Banerji, A. Mawer, and G. Dody, Ball Grid Array Technology, ed. J. K. Lau (New York, McGraw-Hill, 1995), p. 379.
6. Z. Mei, M. Kaufmann, A. Eslambolchi, and P. Johnson, 1998 Electron. Comp. Tech. Conf. Proc. Piscataway, NJ: IEEE, 1998), p. 952.
7. A. Zribi, R. R. Chromik, R. Presthus, J. Clum, K. Teed, L. Zavalij, J. DeVita, J. Tova, and E. J. Cotts, Proc, 49th IEEE Electron. Comp. Tech. Conf, (Piscataway, NJ: IEEE, 1999), p. 451.
8. A. Zribi, R. R. Chromik, R. Presthus, K. Teed, L. Zavalij, J. DeVita, J. Tova, E. J. Cotts, J. Clum, R. Erich, A. Primavera, G. Westby, R. J. Coyle, and G. M. Wenger, IEEE Electron. Comp. Technol. 23, 383 (2000).
9. A. M. Minor, and J. W. Morris, Jr., Metall. and Mater. Trans. A 31, 798 (2000).10.1007/s11661-000-0022-5 ↗
10. A. M. Minor, and J. W. Morris, Jr., J. Electron. Mater., 29, 1170 (2000).10.1007/s11664-000-0009-4 ↗