Effect of the Silver Content of SnAgCu Solder on the Interfacial Reaction and on the Reliability of Angle Joints Fabricated by Laser-Jet Soldering
Source abstract
Abstract
The silver content of lead-free solders affects their microstructure, the interfacial reaction, and the performance of the joints in reliability tests. In this study, Sn3.0Ag0.5Cu (wt.%, SAC305) and Sn1.0Ag0.5Cu (wt.%, SAC105) solder balls of diameter 55 μm were reflowed on gold surface pads by laser-jet soldering. It was found that four types of layered intermetallic compound (IMC) were formed at the interfaces; these were Au5Sn/AuSn, AuSn, AuSn2, and AuSn4 from the pad side to the solder matrix. The Au5Sn/AuSn eutectic region, thickness 400 nm, formed because of the high cooling rate induced by the laser-jet soldering. During high-temperature storage tests, the silver became segregated at the interfaces between the Au–Sn IMC and the solder matrix, resulting in inhibition of IMC growth in SAC305 joints, the shear strengths of which were higher than those of SAC105 joints. In mechanical drop tests, however, percentage failure of the SAC305 joints was twice that of the SAC105 joints.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Electronic Packaging and Soldering Technologies · Adhesion, Friction, and Surface Interactions · Additive Manufacturing Materials and Processes
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (22)
Show source-provided references
1. F. Sun, P. Hochstenbach, W.D. Van Driel, and G.Q. Zhang, Microelectrons Reliab 48, 1167 (2008).10.1016/j.microrel.2008.06.011 ↗
2. R.S. Pandher, B.G. Lewis, R. Vangaveti, and B. Singh, Drop shock reliability of lead-free alloys-effect of micro-additives, in 57th Electronic Components and Technology Conference (ECTC), Reno, Nevada, USA (2007).10.1109/ECTC.2007.373868 ↗
3. C.E. Ho, R. Zheng, G.L. Luo, A.H. Lin, and C.R. Kao, Formation and resettlement of (Au x Ni1−x )Sn4 in solder joints of ball-grid-array packages with the Au/Ni surface finish. J. Electron. Mater. 29, 1175–1181 (2000).10.1007/s11664-000-0010-y ↗
4. J.W. Yoon, W.C. Moon, and S.B. Jung, Interfacial reaction of ENIG/Sn-Ag-Cu/ENIGc sandwich solder joint during isothermal aging. Microelectron. Eng. 83, 2329–2334 (2006).10.1016/j.mee.2006.10.027 ↗
5. R. Zhang, R. Zhao, F. Guo, and Z. Xia, Interfacial reaction between the electroless nickel immersion gold substrate and Sn-based solders. Microelectron. Reliab. 49, 303–309 (2009).10.1016/j.microrel.2008.12.016 ↗
6. A. Dębski, W. G˛asior, Z. Moser, and R. Major, Enthalpy of formation of Au–Sn intermetallic phases Part II. J. Alloy. Compd. 509, 6131–6134 (2011).10.1016/j.jallcom.2011.02.160 ↗
7. C.E. Ho, Y.M. Chen, and C.R. Kao, Reaction kinetics of solder-balls with pads in BGA packages during reflow soldering. J. Electron. Mater. 28, 1231–1237 (1999).10.1007/s11664-999-0162-3 ↗
8. C.E. Ho, S.Y. Tsai, and C.R. Kao, Reaction of solder with Ni/Au metallization for electronic packages during reflow soldering. IEEE Trans. Adv. Pack. 24, 493–498 (2001).10.1109/6040.982835 ↗
9. Z. Mei, P. Johnson, M. Kaufmann, and A. Eslambolchi, Effect of Electroless Ni/immersion Au plating parameters on PBGA solder joint attachment reliability, in 49th Electronic Components and Technology Conference (ECTC), San Diego, CA, USA (1999).
10. C.M. Chuang, P.C. Shin, and K. Lin, The interfacial reaction between Sn-Zn-Ag-Ga-Al solders and metallized Cu substrates. J. Electron. Mater. 33, 7–13 (2004).10.1007/s11664-004-0287-3 ↗
11. M.D. Cheng, S.F. Yen, and T.H. Chuang, Intermetallic compounds formed during the reflow and aging of Sn-3.8Ag-0.7Cu and Sn-20In-2Ag-0.5Cu solder ball grid array packages. J. Electron. Mater. 33, 71–180 (2004).10.1007/s11664-004-0176-9 ↗
12. Q. Xiao, H.J. Bailey, and W.D. Armstrong, Aging effects on microstructure and tensile property of Sn3.9Ag0.6Cu solder alloy. J. Electron. Pack. 126, 208–212 (2004).10.1115/1.1756144 ↗
13. N. Moelans, K.C.H. Kumar, and P. Wollants, Thermodynamic optimization of the lead-free solder system Bi-In-Sn-Zn. J. Alloy. Compd. 360, 98–106 (2003).10.1016/S0925-8388(03)00325-6 ↗
14. L. Yin, A. Chauhan, and T.J. Singler, Reactive wetting inmetal/metal systems: dissolutive versus compound-forming systems. Mater. Sci. Eng. A 495, 80–89 (2008).10.1016/j.msea.2007.11.097 ↗
15. C.P. Lin and C.M. Chen, Solid-state interfacial reactions at the solder joints employing Au/Pd/Ni and Au/Ni as the surface finish metallizations. Microelectron. Reliab. 52, 385–390 (2012).10.1016/j.microrel.2011.03.007 ↗
16. J. Ciulik and M.R. Notis, The Au/Sn phase diagram. J. Alloy. Compd. 191, 71–78 (1993).10.1016/0925-8388(93)90273-P ↗
17. C.F. Yang and S.W. Chen, Interfacial reactions in Au/Sn/Cu sandwich specimens. Intermetallics 18, 672–678 (2010).10.1016/j.intermet.2009.11.003 ↗
18. R. Bali, E. Fleury, S.H. Han, and J.P. Ahn, Interfacial intermetallic phases and nanoeutectic in rapidly quenched Sn-Ag-Cu on Au under bump metallization. J. Alloy. Compd. 457, 113–117 (2008).10.1016/j.jallcom.2007.02.129 ↗
19. M.P. Renavikar, N. Patel, A. Dani, V. Wakharkar, V. Vasudevan, and O. Bchir, et al., Materials technology for environmentally green micro-electronic packaging. Int. Technol. J. 12, 1–16 (2008).10.1535/itj.1201.01 ↗
20. J.H.L. Pang, and F.X. Che, Drop impact analysis of Sn-Ag-Cu solder joints using dynamic high-strain rate plastic strain as the impact damage driving force, in 56th Electronic Components and Technology Conference (ECTC), San Diego, CA, USA (2006).10.1109/ECTC.2006.1645625 ↗
21. T. You, Y. Kim, J. Kim, J. Lee, B. Jung, and J. Moon, et al., Predicting the drop performance of solder joints by evaluating the elastic strain energy from high-speed ball pull tests. J. Electron. Mater. 38, 410–414 (2009).10.1007/s11664-008-0633-y ↗
22. F.X. Che, E.C. Poh, W.H. Zhu, and B.S. Xiong, Ag Content Effect on Mechanical Properties of Sn-xAg-0.5Cu Solders, in 9th Electronics Packaging Technology Conference (EPTC), Singapore (2007).10.1109/EPTC.2007.4469808 ↗