Effects of Pulsed Laser Deposition Conditions on the Microstructure of Ca3Co4O9 Thin Films
Source abstract
Abstract
The influence of deposition conditions on the microstructure of Ca3Co4O9 (CCO) thin films fabricated by the pulsed laser deposition technique was investigated. X-ray diffraction revealed that a fast deposition rate resulted in not only low crystallinity but also the existence of the Ca x CoO2 secondary phase. The Ca x CoO2 structure was further confirmed by high-resolution transmission electron microscopy. The CCO thin-film growth was deduced to be a kinetically controlled process, and the quality of the thin films strongly depended on the coalescence process. The formation of Ca x CoO2 was inevitable during the thin-film growth. However, given enough time and supply of oxygen at a lower deposition rate, it was possible to transform the Ca x CoO2 phase into the desired CCO phase during the coalescence process, while with faster deposition, more Ca x CoO2 structure was formed, and the secondary phase could hardly transform into the CCO phase.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: ZnO doping and properties · Electronic and Structural Properties of Oxides · Copper-based nanomaterials and applications
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (18)
Show source-provided references
1. F.J. DiSalvo, Science 285, 703 (1999). doi: 10.1126/science.285.5428.703 .10.1126/science.285.5428.703 ↗
2. I. Terasaki, Y. Sasago, and K. Uchinokura, Phys. Rev. B 56, R12685 (1997). doi: 10.1103/PhysRevB.56.R12685 .10.1103/PhysRevB.56.R12685 ↗
3. A.C. Masset, C. Michel, A. Maignan, M. Hervieu, O. Toulemonde, F. Studer, B. Raveau, and J. Hejtmanek, Phys. Rev. B 62, 166 (2000). doi: 10.1103/PhysRevB.62.166 .10.1103/PhysRevB.62.166 ↗
4. M. Shikano and R. Funahashi, Appl. Phys. Lett. 82, 1851 (2003). doi: 10.1063/1.1562337 .10.1063/1.1562337 ↗
5. L.D. Hicks and M.S. Dresselhaus, Phys. Rev. B 47, 12727 (1993). doi: 10.1103/PhysRevB.47.12727 .10.1103/PhysRevB.47.12727 ↗
6. R. Venkatasubramanian, E. Siivola, T. Colpitts, and B. O’Quinn, Nature 413, 597 (2001). doi: 10.1038/35098012 .10.1038/35098012 ↗
7. T. Terada, Y. Yoshida, M. Ueno, and Y. Takai, J. Ceram. Soc. Jpn. 110, 560 (2002).10.2109/jcersj.110.560 ↗
8. A. Sakai, T. Kanno, S. Yotsuhashi, A. Odagawa, and H. Adachi, Jpn. J. Appl. Phys. 44, L966 (2005). doi: 10.1143/JJAP.44.L966 .10.1143/JJAP.44.L966 ↗
9. Y.F. Hu, W.D. Si, E. Sutter, and Q. Li, Appl. Phys. Lett. 86, 082103 (2005). doi: 10.1063/1.1868873 .10.1063/1.1868873 ↗
10. K. Sugiura, H. Ohta, K. Nomura, M. Hirano, H. Hosono, and K. Koumoto, Appl. Phys. Lett. 89, 032111 (2006). doi: 10.1063/1.2234277 .10.1063/1.2234277 ↗
11. H.U. Habermeier, Mater. Today 10, 34 (2007). doi: 10.1016/S1369-7021(07)70243-2 .10.1016/S1369-7021(07)70243-2 ↗
12. S.R. Gilbert, L.A. Wills, B.W. Wessels, J.L. Schindler, J.A. Thomas, and C.R. Kannewurf, J. Appl. Phys. 80, 969 (1996). doi: 10.1063/1.362909 .10.1063/1.362909 ↗
13. B.L. Cushing and J.B. Wiley, J. Solid State Chem. 141, 385 (1998). doi: 10.1006/jssc.1998.7957 .10.1006/jssc.1998.7957 ↗
14. J.S. Horwitz and J.A. Sprague, Pulsed Laser Deposition of Thin Films, ed. D.B. Chrisey and G.K. Hubler (New York: Wiley, 1994), p. 229.
15. H.W. Eng, W. Prellier, S. Hebert, D. Grebille, L. Mechin, and B. Mercey, J. Appl. Phys. 97, 013706 (2005). doi: 10.1063/1.1823582 .10.1063/1.1823582 ↗
16. Y.F. Hu, E. Sutter, W.D. Si, and Q. Li, Appl. Phys. Lett. 87, 171912 (2005). doi: 10.1063/1.2117615 .10.1063/1.2117615 ↗
17. T. Kanno, S. Yotsuhashi, and H. Adachi, Appl. Phys. Lett. 85, 739 (2004). doi: 10.1063/1.1776310 .10.1063/1.1776310 ↗
18. H. Itahara, W.S. Seo, S. Lee, H. Nozaki, T. Tani, and K. Koumoto, J. Am. Chem. Soc. 127, 6367 (2005). doi: 10.1021/ja0434883 .10.1021/ja0434883 ↗