Abstract
Biocide free and biocide loaded Zeolite epoxy coatings were formulated and covalently linked to diglycidyl ether bisphenol-A type epoxy resin which acts as a base material. These formulations were applied over the zinc phosphated mild steel specimens by a brushing method to give a thickness of 200 ± 10 μm. The effect of biocide on the corrosion and fouling resistance properties were evaluated by Thermo Gravimetric Analysis (TGA), polarization, electrochemical impedance and antifouling testing. The experimental evidence reveals that the linkage of biocide loaded Nano Zeolite has tremendous potential in resisting corrosion and fouling which is ideally required for marine environments and quite superior to the biocide free Zeolite coating. The purity and the structure of these coatings were examined by an FTIR spectral study.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Marine Biology and Environmental Chemistry · Environmental Chemistry and Analysis · Microplastics and Plastic Pollution
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (28)
Show source-provided references
1. Rittschof D (2001) Natural product antifoulants and coatings development. In: McClintock JB, Baker BJ (eds) Mar Chem Ecol, Chapt. 17. CRC, Boca Raton, FL
2. Bennett RF (1996) Industrial manufacture and applications of tributyltin compounds. In: de Mora SJ (ed) Tributyltin: case study of an environmental contaminant, chapt. 2. Cambridge University Press, New York
3. Ponasik J, Conova S, Kinghorn D, Kinney WA, Rittschof D, Ganem B (1998) Pseudoceratidine, a marine natural product with antifouling activity: synthetic and biological studies. Tetrahedron 54(25):6977–698610.1016/S0040-4020(98)00340-8 ↗
4. Armstrong E, Boyd KG, Pisacane A, Peppiatt CJ, Burgess JG (2000) Marine microbial natural products in antifouling coatings. Biofouling 16(2–4):215–22410.1080/08927010009378446 ↗
5. Rittschof D (2000) Natural product antifoulants: one perspective on the challenge related to coatings development. Biofouling 15(1–3):119–12710.1080/08927010009386303 ↗
6. Alberte RS, Smith R (2006) Transgenic plants incorporating traits of Zostera marina. US Patent 2006053510
7. Alberte RS, Zimmerman RC (2000) Environmentally benign crop protection agents. (Phycogen, USA). PCT Int. Appl. WO 0016632
8. Alexandratos SD (1999) Synthesis and purification of zosteric acid. US Patent 5990336
9. Auby I, Labourg PJ (1996) Seasonal dynamics of Zostera noltii Hornem in the Bay of Arcachon (France). J Sea Res 35:269–27710.1016/S1385-1101(96)90754-6 ↗
10. Barrios CA, Xu QW, Cutright TJ (2005) Incorporating Zosteric acid into silicone coatings to achieve its slow release while reducing fresh water bacterial attachment. Colloids and Surfaces B: Biointerfaces 41:83–9310.1016/j.colsurfb.2004.09.009 ↗
11. Callow ME (1999) Recent advances in marine biotechnology, vol. 3. In: Fingerman M, Nagabhushanam R, Thompson M-F (eds) Biofilms, bioadhesion, corrosion and biofouling, chapter 6. Science, Enfield
12. Premkumar S, Karikalchozhan C, Alagar M (2008) Studies on thermal and morphological behaviour of caprolactum blocked methylene blocked diisocyanate toughened bismaleimide modified epoxy matrices. Eur Polym J 44:2599–260710.1016/j.eurpolymj.2008.05.031 ↗
13. Ananda Kumar S, Balakrishnan T, Alagar M, Denchev Z (2006) Development and characterization of silicone/phosphorus modified epoxy materials and their application as anticorrosion and antifouling coatings. Progr Org Coating 55:207–21710.1016/j.porgcoat.2005.10.001 ↗
14. Chiu Y-C, F-Y Liu et al (2006) Syntheses and characterization of P/Si polysilsequinone/epoxy nanocomposites. Thermochim Acta 473:7–1310.1016/j.tca.2008.03.020 ↗
15. Yam CM, Tong SSY, Kakkar AK (1998) Simple acid-base hydrolytic chemistry approach to molecular self-assembly: thin films of long chain alcohols terminated with alkyl, phenyl, and acetylene groups on inorganic oxides surfaces. Langmuir 14:6941–694710.1021/la9806909 ↗
16. Zhang Newby BM, Cutright T, Barrios CA, Xu Q (2006) Zosteric Acid-An Effective Antifoulant For Reducing FreshWater Bacteria Attachment oncoating. American Coatings Association, Inc. ISSN: 1547–0091
17. Achamlale S, Rezzonico B et al (2009) Evaluation of Zostera detritus as a potential new source of zosteric acid. J Appl Phycol 21:347–35210.1007/s10811-008-9375-8 ↗
18. Zhan B-Z, White MA, Lumsden M (2003) Bonding of organic amino, vinyl, and acryl groups to nanometer-sized NaX Zeolite crystal surfaces. Langmuir 19(10):4205–4210
19. Varsha C, Bajpai SK, Navin C (2009) Investigation of water vapour permeation and antibacterial properties of nano silver loaded cellulose acetate film. Int Food Res J 17:623–639
20. Kumar SA, Sasikumar A (2010) Studies on novel silicone/phosphorus/sulphur containing nano-hybrid epoxy anticorrosive and antifouling coatings. Prog Org Coat 68(3):189–20010.1016/j.porgcoat.2010.02.005 ↗
21. Sundberg DC, Vasishtha N, Zimmerman RC, Smith CM (1997) Selection, design and delivery of environmenally benign antifouling agents. Naval Res Rev 49(4):51–59
22. Quraishi MA, Rafiquee MZA, Saxena N, Khan S (2008) Inhibition of mild steel corrosion in presence of fatty acid imidazolines in hydrochloric acid. 44(1):99–106.
23. Fernandez-Alba AR, Hernando MD, Piedra L, Chisti Y (2002) Toxicity evaluation of single and mixed antifouling biocides measured with acute toxicity bioassays. Anal Chim Acta 456(2):303–31210.1016/S0003-2670(02)00037-5 ↗
24. He Z, Raoa W, Rena T, Liub W, Xue Q (2002) The tribochemical study of some N-containing heterocyclic compounds as lubricating oil additives. Tribol Lett 13:87–9310.1023/A:1020100631716 ↗
25. Vijayan CP, Noel D, Hechler JJ (1986) Alternating current impedance utility in evaluating phosphate coating, phosphorous-chromium rinse and paint performance. ACS 6:59–76
26. Kim J, Nyren-Erickson E et al (2008) Release characteristics of reattached barnacles to non-toxic silicone coatings. Biofouling 24(4):313–31910.1080/08927010802199945 ↗
27. Chen MeiLing QU, YuanYuan YANGLi, Hong GAO (2008) Structures and antifouling properties of low surface energy non-toxic antifouling coatings modified by nano-SiO2 powder. Sci China Ser B-Chem 51(9):848–85210.1007/s11426-008-0069-5 ↗
28. Wiegemann M (2005) Adhesion in blue mussels (Mytilus edulis) and barnacles (Genus Balanus): Mechanisms and technical applications. Aquat Sci 67:166–17610.1007/s00027-005-0758-5 ↗