journal article·2025-06

The reversibility of interlayer ion fixation in the smectite of BCV 2017 bentonite during long-term heating in air at 200 °C, a detailed mineralogical study

Magdaléna Koubová, František Laufek, Irena Hanusová, Marek Szczerba

Publisher page

Abstract

In the context of studies related to the disposal of heat-generating wastes, the aim of this study was to characterize the mineralogical transformations that take place in the BCV 2017 Ca-Mg bentonite (Černý vrch bentonite, Czech Republic) following short (1-day) and long-term (47-month) heating in air at 200 °C. A laboratory procedure involving interlayer cation exchange using the Cu-trien complex with subsequent ethylene glycol solvation and full-profile diffraction pattern modelling was successfully applied for the comparison of the original bentonite and the material heated at 200 °C in air, as well as their subsequent rehydration. In the original bentonite, two smectite-rich mixed layers minerals were modelled, consisting of 10-Å, high- and low-charge smectite layers. The 10-Å layers represented both the illite and also smectite layers with fixed Mg 2+ and Ca 2+ ions in the interlayer. After heating at 200 °C for 47 months, the total cation exchange capacity (CEC) decreased from 58 to 48 meq/100 g, the content of exchangeable Ca 2+ increased from 25 to 27 meq/100 g, and the content of exchangeable Mg 2+ decreased from 47 to 27 meq/100 g. The increase of exchangeable Ca 2+ was caused by liberation of originally fixed Ca 2+ in the interlayer of smectite while decrease of exchangeable Mg 2+ was due to its fixation. The predominance of the fixation of interlayered Mg 2+ over the liberation of Ca 2+ led to the observed decrease of CEC. This decrease was accompanied by increase in the number of both smectite layers with interlayer-fixed Mg 2+ (10-Å layers) from 12 to 19 % (an average value of two smectite-rich MLMs), and low-charged smectite layers from 67 to 76 % in MLMs. A simultaneous decrease in the number of high-charged smectite layers from 22 to 5 % was observed. The BCV 2017 bentonite heated for 1-day reached intermediate values between the original and 47-month heated bentonites. The fixation of the interlayered Mg 2+ was partially reversible, increasing from 27 to 31 meq/100 g after rehydration for 54 days under relative humidity of 97.6 %. The percentage of the 10-Å layers decreased from 19 to 16 % of MLMs and the CEC increased from 48 to 52 meq/100 g. Similar results were obtained when the heated bentonite was saturated with liquid water with 1:100 solid:liquid ratio for the same time period.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Clay minerals and soil interactions · Soil and Unsaturated Flow · Iron oxide chemistry and applications

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (35)

Show source-provided references
1. Influence of mechanical compaction and clay mineral diagenesis on the microfabric and porescale properties of deep-water Gulf of Mexico Mudstones10.1346/CCMN.2006.0540411 ↗
2. Cation migration into empty octahedral sites and surface properties of clays10.1346/CCMN.1971.0190306 ↗
3. Červinka · 2018
4. Effect of heating on swelling and dispersion of different cationic forms of a smectite10.1346/CCMN.1996.0440609 ↗
5. Methods for determination of the layer charge of smectites: a critical assessment of existing approaches10.1007/s42860-023-00234-8 ↗
6. Rehydration of dehydrated-dehydroxylated smectite in a low water vapor environment10.2138/am.2012.3872 ↗
7. Design development of a copper-coated canister for the disposal of spent fuel in a deep geological repository in Opalinus Clay10.1080/1478422X.2017.1292200 ↗
8. Three new, quick CEC methods for determining the amounts of exchangeable calcium cations in calcareous clays10.1346/CCMN.2009.0570306 ↗
9. Interlaboratory CEC and exchangeable cation study of bentonite buffer materials: II. Alternative methods10.1346/CCMN.2012.0600207 ↗
10. XRD measurement of mean crystallite thickness of Illite and Illite/Smectite: reappraisal of the Kubler Index and the Scherrer Equation10.1346/CCMN.1997.0450315 ↗
11. Dehydroxylation behavior of heat-treated and steam-treated homoinic cis-vacant montmorillonites10.1346/CCMN.1999.0470506 ↗
12. Characterization of Bentonites from the in Situ ABM5 Heater Experiment at Äspö Hard Rock Laboratory, Sweden10.3390/min12040471 ↗
13. Chemostratigraphic correlation of sediments containing expandable clay minerals based on ion exchange with Cu(II) triethylenetetramine10.1346/CCMN.2009.0570204 ↗
14. Summary of the research of Czech Bentonites for use in the deep geological repository—up to 2018
15. Eindimensionale fehlordnung in kristallen und ihr einfluss auf die röntgeninterferenzen. I. Berechnung des fehlordnungsgrades aus den röntgenintensitaten10.1107/S0365110X49000552 ↗
16. Charge reduction, octahedral charge, and lithium retention in heated, Li-saturated smectites10.1346/CCMN.1987.0350604 ↗
17. Preparation and characterization of reduced-charge hectorites10.1346/CCMN.1992.0400404 ↗
18. Geochemical, geotechnical, and microbiological changes in Mg/Ca Bentonite after thermal Loading at 150 °C
19. Stability of bentonites in salt solutions II potassium chloride initial step of illitization?10.1016/j.clay.2010.04.009 ↗
20. Effect of extensive drying on the cation exchange capacity of bentonites10.1180/claymin.2010.045.4.441 ↗
21. Termination of swelling capacity of smectites by Cutrien Exchange10.1180/claymin.2011.046.3.411 ↗
22. About the possibility to liberate naturally present fixed cations from dioctahedral smectites by hydrothermal treatment10.1016/j.clay.2023.107115 ↗
23. Komadel, P., Madejová, J., Bujdák, J., 2005. Preparation and properties of reduced-charge smectites - a review. Clay Clay Miner., Vol. 53, No. 4, 313–334. DOl: https://doi.org/10.1346/CCMN.2005.053040l.10.1346/CCMN.2005.0530401 ↗
24. New laboratory procedure for distinguishing smectites with varying permanent layer charge based on the combination of Cu-trien and ethylene glycol solvation methods and X-ray diffraction
25. Mineralogical, geochemical and geotechnical study of BCV 2017 bentonite – the initial state and the state following thermal treatment at 200°C
26. Determination of the cation exchange capacity (CEC) of clay minerals using the complexes of copper(II) ion with triethylenetetranine and tetraethylenepentamine10.1346/CCMN.1999.0470315 ↗
27. An experimental study on thermal relaxation of BCV bentonite
28. Charge reduction and regeneration in K+, Na+, Mg2+, Ni2+ and Co2+-exchanged Wyoming bentonite10.1007/BF00764737 ↗
29. Chemické složení některých bentonitů v severozápadních Čechách
30. Surface area and layer charge of smectite from CEC and EGME/H2O-retention measurements10.1346/CCMN.2008.0560203 ↗
31. New model of ethylene glycol intercalate in smectites for XRD modelling10.1016/j.clay.2017.12.010 ↗
32. Nomographs of sedimentation times for soil particles under gravity or centrifugal acceleration10.2136/sssaj1948.036159950012000C0014x ↗
33. Mineralogy and geochemistry of a bentonite pellets column heated for 10 years10.1007/s42860-023-00238-4 ↗
34. Rietveld structure refinement of Cu-Trien exchanged nontronites10.3389/fchem.2018.00558 ↗
35. Thermal migration behaviour of Na+, Cu2+ and Li+ in montmorillonite