journal article·2023-11Open access

Enhancing hydrogen embrittlement resistance of TRIP-rich medium Mn steel by morphology optimization

Yuxuan Liu, Zuoheng Cao, Chengpeng Huang, Chen Hu, Mingxin Huang

Science China Materials· Volume 66· Issue 11

Abstract

相变诱发塑性(TRIP)效应通常可显著提高中锰钢的加工硬化能力, 从而获得出色的强度和塑性组合. 然而, 变形过程中生成的新鲜马氏体极易发生氢脆, 是新型高强中锰钢开发的瓶颈问题. 我们在此提出了一种长带状形貌来减轻新鲜马氏体引起的氢脆. 温轧制备的长带状中锰钢相比传统临界退火制备的等轴晶形貌中锰钢, 不仅具有同等的高加工硬化率, 而且抗氢脆性能更好. 等轴晶形貌中锰钢由于缺乏有效的阻碍机制, 氢裂纹一旦出现便能快速扩展. 相反, 对于长带状形貌中锰钢, 氢裂纹会被晶界和相界所阻碍或偏转. 本形貌设计可以提高其他富TRIP效应的钢和合金的抗氢脆性能.
The source flagged this abstract for review. Check formulas and completeness against the original publication.
Source: expertdata · Quality: needs review · Source record ↗
Source flags: short_text

Research context

OpenAlex topics: Microstructure and Mechanical Properties of Steels · Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (32)

Show source-provided references
1. Huang C, Hu C, Liu Y, et al. Recent developments and perspectives of advanced high-strength medium Mn steel: From material design to failure mechanisms. Mater Futures, 2022, 1: 03200110.1088/2752-5724/ac7fae ↗
2. Sun B, da Silva AK, Wu Y, et al. Physical metallurgy of medium-Mn advanced high-strength steels. Int Mater Rev, 2023, 1–39
3. Suh DW, Kim SJ. Medium Mn transformation-induced plasticity steels: Recent progress and challenges. Scripta Mater, 2017, 126: 63–6710.1016/j.scriptamat.2016.07.013 ↗
4. Huang CP, Wang M, Zhu KY, et al. Carbon-induced negative strain-rate sensitivity in a quenching and partitioning steel. Acta Mater, 2023, 255: 11909910.1016/j.actamat.2023.119099 ↗
5. He BB, Huang MX. Strong and ductile medium Mn steel without transformation-induced plasticity effect. Mater Res Lett, 2018, 6: 365–37110.1080/21663831.2018.1461141 ↗
6. He BB, Luo HW, Huang MX. Experimental investigation on a novel medium Mn steel combining transformation-induced plasticity and twinning-induced plasticity effects. Int J Plast, 2016, 78: 173–18610.1016/j.ijplas.2015.11.004 ↗
7. Hu C, Huang CP, Liu YX, et al. The dual role of TRIP effect on ductility and toughness of a medium Mn steel. Acta Mater, 2023, 245: 11862910.1016/j.actamat.2022.118629 ↗
8. Wan X, Liu G, Ding R, et al. Stabilizing austenite via a core-shell structure in the medium Mn steels. Scripta Mater, 2019, 166: 68–7210.1016/j.scriptamat.2019.03.015 ↗
9. Miller RL. Ultrafine-grained microstructures and mechanical properties of alloy steels. Metall Trans, 1972, 3: 905–91210.1007/BF02647665 ↗
10. Cho L, Kong Y, Speer JG, et al. Hydrogen embrittlement of medium Mn steels. Metals, 2021, 11: 35810.3390/met11020358 ↗
11. Cao Z, Wang Z, Ngiam Y, et al. Hydrogen embrittlement evaluation and prediction in press-hardened steels. Steel Res int, 2023, 94: 220068510.1002/srin.202200685 ↗
12. Sun B, Krieger W, Rohwerder M, et al. Dependence of hydrogen embrittlement mechanisms on microstructure-driven hydrogen distribution in medium Mn steels. Acta Mater, 2020, 183: 313–32810.1016/j.actamat.2019.11.029 ↗
13. Ryu JH, Chun YS, Lee CS, et al. Effect of deformation on hydrogen trapping and effusion in TRIP-assisted steel. Acta Mater, 2012, 60: 4085–409210.1016/j.actamat.2012.04.010 ↗
14. Ding W, Yang K, Gong Y, et al. Improving hydrogen embrittlement resistance of a modified press hardening steel by introducing retained austenite as hydrogen trap. J Iron Steel Res Int, 2022, 29: 1864–187210.1007/s42243-021-00738-4 ↗
15. Du Y, Gao X, Lan L, et al. Hydrogen embrittlement behavior of high strength low carbon medium manganese steel under different heat treatments. Int J Hydrogen Energy, 2019, 44: 32292–3230610.1016/j.ijhydene.2019.10.103 ↗
16. Han J, Nam JH, Lee YK. The mechanism of hydrogen embrittlement in intercritically annealed medium Mn TRIP steel. Acta Mater, 2016, 113: 1–1010.1016/j.actamat.2016.04.038 ↗
17. Zhang Y, Shao C, Wang J, et al. Intercritical annealing temperature dependence of hydrogen embrittlement behavior of cold-rolled Al-containing medium-Mn steel. Int J Hydrogen Energy, 2019, 44: 22355–2236710.1016/j.ijhydene.2019.06.204 ↗
18. Sun B, Lu W, Gault B, et al. Chemical heterogeneity enhances hydrogen resistance in high-strength steels. Nat Mater, 2021, 20: 1629–163410.1038/s41563-021-01050-y ↗
19. Zhang J, Sun B, Yang Z, et al. Enhancing the hydrogen embrittlement resistance of medium Mn steels by designing metastable austenite with a compositional core-shell structure. Acta Metall Sin (Engl Lett), 2023, 36: 1059–107710.1007/s40195-022-01483-7 ↗
20. Huang C, Huang M. Effect of processing parameters on mechanical properties of deformed and partitioned (D&P) medium Mn steels. Metals, 2021, 11: 35610.3390/met11020356 ↗
21. Li ZC, Ding H, Misra RDK, et al. Deformation behavior in cold-rolled medium-manganese TRIP steel and effect of pre-strain on the Lüders bands. Mater Sci Eng-A, 2017, 679: 230–23910.1016/j.msea.2016.10.042 ↗
22. Liu L, Yu Q, Wang Z, et al. Making ultrastrong steel tough by grain-boundary delamination. Science, 2020, 368: 1347–135210.1126/science.aba9413 ↗
23. Steineder K, Krizan D, Schneider R, et al. On the microstructural characteristics influencing the yielding behavior of ultra-fine grained medium-Mn steels. Acta Mater, 2017, 139: 39–5010.1016/j.actamat.2017.07.056 ↗
24. Li X, Ma X, Zhang J, et al. Review of hydrogen embrittlement in metals: Hydrogen diffusion, hydrogen characterization, hydrogen embrittlement mechanism and prevention. Acta Metall Sin (Engl Lett), 2020, 33: 759–77310.1007/s40195-020-01039-7 ↗
25. Pfeil LB. The effect of occluded hydrogen on the tensile strength of iron. Proc R Soc Lond A, 1926, 112: 182–19510.1098/rspa.1926.0103 ↗
26. Fu CL, Painter GS. First principles investigation of hydrogen embrittlement in FeAl. J Mater Res, 1991, 6: 719–72310.1557/JMR.1991.0719 ↗
27. Shao C, Hui W, Zhang Y, et al. Effect of intercritical annealing time on hydrogen embrittlement of warm-rolled medium Mn steel. Mater Sci Eng-A, 2018, 726: 320–33110.1016/j.msea.2018.04.100 ↗
28. Wang Z, Xu J, Li J. Effect of heat treatment processes on hydrogen embrittlement in hot-rolled medium Mn steels. Int J Hydrogen Energy, 2020, 45: 20004–2002010.1016/j.ijhydene.2020.04.241 ↗
29. Fan YH, Zhang B, Yi HL, et al. The role of reversed austenite in hydrogen embrittlement fracture of S41500 martensitic stainless steel. Acta Mater, 2017, 139: 188–19510.1016/j.actamat.2017.08.011 ↗
30. Ngiam Y, Cao ZH, Huang MX. Understanding hydrogen embrittlement in press-hardened steel by coupling phase field and hydrogen diffusion modeling. Mater Sci Eng-A, 2022, 834: 14252310.1016/j.msea.2021.142523 ↗
31. Wang JJ, Hui W, Xie Z, et al. Hydrogen embrittlement of a cold-rolled Al-containing medium-Mn steel: Effect of pre-strain. Int J Hydrogen Energy, 2020, 45: 22080–2209310.1016/j.ijhydene.2020.05.239 ↗
32. Wang Z, Luo ZC, Huang MX. Revealing hydrogen-induced delayed fracture in ferrite-containing quenching and partitioning steels. Materialia, 2018, 4: 260–26710.1016/j.mtla.2018.09.022 ↗