Reduction of residual stresses in laser beam welds by means of defocused laser beams
Source abstract
Abstract
Longitudinal residual stresses in beam welds ranging at the value of the local yield strength can diminish the lifespan of components. To extend the service life of welds special methods of welding residual stress reduction were developed earlier which are however not effective for beam welds in complex component geometries. Application of beam welding sources for post-welding heat treatment of components has become a flexible tool for reducing longitudinal stresses in beam welds. Such heat treatment in a specific transversal distance to the weld by a defocused beam results in huge stress reductions depending on the used process parameters. Experimental results for ferritic and austenitic steels reveal weld stress reductions to up to compressive stresses. For different materials and diverse material thicknesses special process parameter regions have to be used in this procedure. At a transmission component this procedure shows a stress reduction by >300 MPa.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Welding Techniques and Residual Stresses · Surface Treatment and Residual Stress · Laser Material Processing Techniques
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
BAM Federal Institute for Materials Research and Testing, Unter den Eichen 87, 12205 Berlin, Germany
References (21)
Show source-provided references
1. Nitschke-Pagel T · Schweißen Schneid. · 2006 · 58 · 466
2. Nitschke-Pagel T · Schweißen Schneid. · 2007 · 59 · 23
3. 10.1002/srin.20020000810.1002/srin.200200008 ↗
4. Brauss ME, Pineault JA, Eckersley JS: ‘Residual stress characterization of welds and post-weld processes using X-ray diffraction techniques’, Proc. SPIE–The International Society for Optical Engineering Process on ‘Control and sensors for manufacturing’, San Antonio, TX, USA, March 1998, SPIE, Vol. 3399, 196–204.10.1117/12.302553 ↗
5. 10.1016/0956-716X(93)90409-L10.1016/0956-716X(93)90409-L ↗
6. 10.1016/j.nucengdes.2006.05.00610.1016/j.nucengdes.2006.05.006 ↗
7. Nitschke-Pagel T · Schweißen Schneid. · 2007 · 59 · 387
8. Gabzdyl J, Johnson A, Williams S, Price D: ‘Laser weld distortion control by cryogenic cooling’, Proc. SPIE–The International Society for Optical Engineering on ‘High-power laser macroprocessing’, Osaka, Japan, March 2003, SPIE, Vol. 4831, 269–274.10.1117/12.486497 ↗
9. Pattee HE, Evans RM, Monroe RE: ‘Flame straightening and its effect on base metal properties’, Battelle Memorial Institute, Columbus, OH, USA, 1969.
10. Connor RJ, Urban MJ, Kaumann EJ: ‘Heat-straightening repair of damaged steel bridge girders: fatigue and fracture performance’, NCHRP Report 604, Transportation Research Board, Washington, DC, USA, 2008.
11. Guan Q · Weld. World · 1994 · 33 · 308
12. 10.1179/13621710422502164310.1179/136217104225021643 ↗
13. Luan G, Li G, Li C, Dong C: ‘DC-LSND friction stir welding’, Proc. 7th Int. Friction Stir Welding Symp., Osaka, Japan, May 2008, TWI, 387–395.
14. Guan Q · Weld. World · 1994 · 33 · 160
15. Guan Q · Paton Weld. J. · 2006 · 12 · 2
16. van der Aa EM, Hermans MJM, Richardson IM: ‘Control of welding residual stress and distortion by addition of a trailing heat sink’, Proc. 8th Int. Conf. on ‘Mathematical modelling of weld phenomena’, 1053–1072; 2007, Graz, Technical University of Graz.
17. 10.1179/174329307X22724710.1179/174329307X227247 ↗
18. 10.1016/j.jmatprotec.2011.07.01910.1016/j.jmatprotec.2011.07.019 ↗
19. Tölle F, Gumenyuk A, Rethmeier M, Backhaus A, Olschok S, Reisgen U: ‘Eigenspannungsreduzierung in Elektronen und Laserstrahlschweißnähten mittels nachlaufender Wärmefelder durch schnelle Strahldefokussierung und ablenkung’, Proc. Int. DVS-Berichte: DVS Congress, Hamburg, Germany, September 2011, DVS, Vol. 275, 465–471.
20. Dull RM, DydoJR, Russell JJ, Shanghvi J: ‘Method of reducing distortion by transient thermal tensioning’, US Patent no. 6861617, 2005.
21. Michaleris P · Weld. J. · 1997 · 76 · 451