Abstract

Factors responsible for the failure of the refractory brick lining of pyrometallurgical plants in service at the Svyatogor JSC are considered, of which the major ones are: corrosion due to the attack from high-iron silicon-containing slag, infiltration of molten mass causing fracture during the heat-and-cool thermal cycling, and mechanical impact. Measures that allowed the refractory consumption rate to be reduced to 0.035 tons per ton of blister copper are described.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Material Properties and Applications · Diverse Industrial Engineering Technologies · Industrial Engineering and Technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (5)

Show source-provided references
1. A. P. Snurnikov and S. N. Makarova, "Techniques for cooling the lining of oxyacetylene apparatuses," Tsvetn. Met., No. 8, 35-37 (1989).
2. B. M. Lepinskikh, A. A. Belousov, S. G. Bakhvalov, and A. A. Vostryakov, Transport Properties of Molten Metal and Slag [in Russian], Metallurgiya, Moscow (1995).
3. E. N. Selivanov, "Nickel matte-impregnated magnesite-chromite lining," Ogneupory, No. 6, 28-29 (1995).
4. V. K. Yakushev, I. V. Basina, T. V. Dodis, et al., "Warmup rate and thermal stability of the lining for thermal power units," Kompleks. Ispol'zovanie Mineral. Syr'ya (Comprehensive Raw Mineral Processing), No. 1, 68-70 (1982).
5. V. G. Kozhin, V. V. Belyaev, and N. A. Morozov, "Converter technology in practice at the Svyatogor JSC," Tsvetn. Metallurgiya, No. 6, 17-20 (2002).